The invention discloses a preparation method of an interior wall coating. The preparation method comprises the following steps: step 1, preparing the following raw materials: 300-400 parts of cement, 100-250 parts of quartz sand, 2-4 parts of carboxymethyl cellulose, 7-20 parts of an alkali inhibitor and 50-90 parts of poly (ethyl propanol); 2, grinding the raw materials, mixing, and stirring for 2-2.5 hours; 3, 500 parts of deionized water is added, and stirring continues to be conducted for 20-35 min; 4, after stirring is completed, standing is conducted for 30-50 min in the environment of 30-50 DEG C, and a coating finished product is obtained.
本发明公开了一种内墙涂料的制备方法,包括以下步骤:步骤一,准备以下原料:水泥300‑400份、石英砂100‑250份、羧甲基纤维素2‑4份、阻碱剂7‑20份和聚乙丙醇50‑90份;步骤二,将以上原料研磨后混合,搅拌2‑2.5h;步骤三,加入去离子水500份,继续搅拌20‑35min;步骤四,搅拌完成后在30‑50℃环境下静置30‑50min,得到涂料成品。
The invention discloses a preparation method of an interior wall coating. The preparation method comprises the following steps: step 1, preparing the following raw materials: 300-400 parts of cement, 100-250 parts of quartz sand, 2-4 parts of carboxymethyl cellulose, 7-20 parts of an alkali inhibitor and 50-90 parts of poly (ethyl propanol); 2, grinding the raw materials, mixing, and stirring for 2-2.5 hours; 3, 500 parts of deionized water is added, and stirring continues to be conducted for 20-35 min; 4, after stirring is completed, standing is conducted for 30-50 min in the environment of 30-50 DEG C, and a coating finished product is obtained.
本发明公开了一种内墙涂料的制备方法,包括以下步骤:步骤一,准备以下原料:水泥300‑400份、石英砂100‑250份、羧甲基纤维素2‑4份、阻碱剂7‑20份和聚乙丙醇50‑90份;步骤二,将以上原料研磨后混合,搅拌2‑2.5h;步骤三,加入去离子水500份,继续搅拌20‑35min;步骤四,搅拌完成后在30‑50℃环境下静置30‑50min,得到涂料成品。
Preparation method of interior wall coating with higher strength
European Patent Office | 2023
|Housing interior wall decoration coating material and preparation method thereof
European Patent Office | 2015
|Interior wall coating mechanism for building interior decoration
European Patent Office | 2020
|