Preparation process of wear-resistant and anti-pollution ceramic glaze
The wear-resistant and anti-pollution ceramic glaze is prepared from the following raw materials in parts by weight: 40 to 70 parts of silicon dioxide, 15 to 30 parts of kaolin, 15 to 25 parts of wollastonite, 10 to 15 parts of limestone, 25 to 45 parts of amorphous quartz particles, 3 to 12 parts of diatom ooze, 20 to 36 parts of albite, 1 to 3.2 parts of sodium methyl cellulose, 5 to 10 parts of ethylene glycol, 0.3 to 0.8 part of cobalt oxide, 0.1 to 0.3 part of boron nitride, 1.2 to 3.8 parts of solid lubricant, 5 to 10 parts of wear-resistant agent and 10 to 15 parts of thickening agent. The high-boron ceramic tile is prepared from 48-52 parts of quartz powder, 6-9 parts of feldspar powder, 5-7 parts of talcum powder, 9-13 parts of cryolite powder, 8-12 parts of silicoboroaluminite powder, 4-6 parts of aluminum oxide, 3.5-5 parts of zirconyl nitrate, 2.5-4.5 parts of barium oxide, 3-4.5 parts of titanium oxide, 2.5-3.5 parts of scandium oxide and 2-4 parts of high-boron frit. The high-performance environment-friendly wear-resistant glaze has excellent wear resistance and high hardness, can meet the requirements of high-performance environment-friendly wear-resistant glaze and ceramic products thereof, has higher hardness, is non-toxic and healthy to human bodies, and is particularly suitable for daily ceramics such as tableware and household appliances.
本发明公开了一种耐磨抗污染陶瓷釉制备工艺,包括以下重量份的原料:二氧化硅40~70份、高岭土15~30份、硅灰石15~25份、石灰石10~15份、非晶态石英颗粒25~45份、硅藻泥3~12份、钠长石20~36份、甲基纤维素钠1~3.2份、乙二醇5~10份、氧化钴0.3~0.8份、氮化硼0.1~0.3份、固体润滑剂1.2~3.8份、耐磨剂5~10份和增稠剂10~15份,石英粉48~52份、长石粉6~9份、滑石粉5~7份、冰晶石粉9~13份、硅硼铝钙石粉8~12份、三氧化二铝4~6份、硝酸氧锆3.5~5份、氧化钡2.5~4.5份、氧化钛3~4.5份、氧化钪2.5~3.5份、高硼熔块2~4份。本发明具有优良耐磨性能和高硬度,能满足高性能环保耐磨釉及其陶瓷制品的需求,具有更高的硬度,对身体无毒害,健康,尤其适用于餐具、家用器具等日用陶瓷。
Preparation process of wear-resistant and anti-pollution ceramic glaze
The wear-resistant and anti-pollution ceramic glaze is prepared from the following raw materials in parts by weight: 40 to 70 parts of silicon dioxide, 15 to 30 parts of kaolin, 15 to 25 parts of wollastonite, 10 to 15 parts of limestone, 25 to 45 parts of amorphous quartz particles, 3 to 12 parts of diatom ooze, 20 to 36 parts of albite, 1 to 3.2 parts of sodium methyl cellulose, 5 to 10 parts of ethylene glycol, 0.3 to 0.8 part of cobalt oxide, 0.1 to 0.3 part of boron nitride, 1.2 to 3.8 parts of solid lubricant, 5 to 10 parts of wear-resistant agent and 10 to 15 parts of thickening agent. The high-boron ceramic tile is prepared from 48-52 parts of quartz powder, 6-9 parts of feldspar powder, 5-7 parts of talcum powder, 9-13 parts of cryolite powder, 8-12 parts of silicoboroaluminite powder, 4-6 parts of aluminum oxide, 3.5-5 parts of zirconyl nitrate, 2.5-4.5 parts of barium oxide, 3-4.5 parts of titanium oxide, 2.5-3.5 parts of scandium oxide and 2-4 parts of high-boron frit. The high-performance environment-friendly wear-resistant glaze has excellent wear resistance and high hardness, can meet the requirements of high-performance environment-friendly wear-resistant glaze and ceramic products thereof, has higher hardness, is non-toxic and healthy to human bodies, and is particularly suitable for daily ceramics such as tableware and household appliances.
本发明公开了一种耐磨抗污染陶瓷釉制备工艺,包括以下重量份的原料:二氧化硅40~70份、高岭土15~30份、硅灰石15~25份、石灰石10~15份、非晶态石英颗粒25~45份、硅藻泥3~12份、钠长石20~36份、甲基纤维素钠1~3.2份、乙二醇5~10份、氧化钴0.3~0.8份、氮化硼0.1~0.3份、固体润滑剂1.2~3.8份、耐磨剂5~10份和增稠剂10~15份,石英粉48~52份、长石粉6~9份、滑石粉5~7份、冰晶石粉9~13份、硅硼铝钙石粉8~12份、三氧化二铝4~6份、硝酸氧锆3.5~5份、氧化钡2.5~4.5份、氧化钛3~4.5份、氧化钪2.5~3.5份、高硼熔块2~4份。本发明具有优良耐磨性能和高硬度,能满足高性能环保耐磨釉及其陶瓷制品的需求,具有更高的硬度,对身体无毒害,健康,尤其适用于餐具、家用器具等日用陶瓷。
Preparation process of wear-resistant and anti-pollution ceramic glaze
耐磨抗污染陶瓷釉制备工艺
CHEN JIANHONG (author) / CHEN DONGWEN (author) / CHENG LIANGJIA (author)
2023-08-08
Patent
Electronic Resource
Chinese
European Patent Office | 2020
|European Patent Office | 2022
|Wear-resistant antibacterial ceramic glaze and preparation method thereof
European Patent Office | 2024
|