A platform for research: civil engineering, architecture and urbanism
Coal gangue phase change brick capable of autonomously adjusting temperature and preparation method of coal gangue phase change brick
The invention discloses a coal gangue phase change brick capable of automatically adjusting temperature and a preparation method thereof. The coal gangue phase change brick comprises a brick main body and a phase change material layer covering the surface of the brick main body, the phase change material layer is prepared from the following raw materials: coal gangue fine aggregate, cement, a phase change capsule, water, polypropylene fiber, a polycarboxylate superplasticizer and calcium chloride according to the mass ratio of (2.96 to 4.28): (3.29 to 3.78): (0.98 to 1.32): 1: (0 to 0.043): (0 to 0.015): (0.065 to 0.113). Resource recycling of solid waste is achieved, the indoor temperature can be automatically adjusted to range from 20 DEG C to 30 DEG C, and the special effect that the indoor environment is warm in winter and cool in summer is achieved.
本发明公开了一种可自主调温的煤矸石相变砖及其制备方法,包括砖主体和覆盖于砖主体表面的相变材料层;相变材料层的原料比为,煤矸石细集料:水泥:相变胶囊:水:聚丙烯纤维:聚羧酸减水剂:氯化钙组成,按其质量比为2.96‑4.28:3.29‑3.78:0.98‑1.32:1:0‑0.043:0‑0.015:0.065‑0.113。本发明实现了固体废弃物的资源再利用,能自主调节室内温度在20‑30℃之间,使室内达到冬暖夏凉的特效。
Coal gangue phase change brick capable of autonomously adjusting temperature and preparation method of coal gangue phase change brick
The invention discloses a coal gangue phase change brick capable of automatically adjusting temperature and a preparation method thereof. The coal gangue phase change brick comprises a brick main body and a phase change material layer covering the surface of the brick main body, the phase change material layer is prepared from the following raw materials: coal gangue fine aggregate, cement, a phase change capsule, water, polypropylene fiber, a polycarboxylate superplasticizer and calcium chloride according to the mass ratio of (2.96 to 4.28): (3.29 to 3.78): (0.98 to 1.32): 1: (0 to 0.043): (0 to 0.015): (0.065 to 0.113). Resource recycling of solid waste is achieved, the indoor temperature can be automatically adjusted to range from 20 DEG C to 30 DEG C, and the special effect that the indoor environment is warm in winter and cool in summer is achieved.
本发明公开了一种可自主调温的煤矸石相变砖及其制备方法,包括砖主体和覆盖于砖主体表面的相变材料层;相变材料层的原料比为,煤矸石细集料:水泥:相变胶囊:水:聚丙烯纤维:聚羧酸减水剂:氯化钙组成,按其质量比为2.96‑4.28:3.29‑3.78:0.98‑1.32:1:0‑0.043:0‑0.015:0.065‑0.113。本发明实现了固体废弃物的资源再利用,能自主调节室内温度在20‑30℃之间,使室内达到冬暖夏凉的特效。
Coal gangue phase change brick capable of autonomously adjusting temperature and preparation method of coal gangue phase change brick
一种可自主调温的煤矸石相变砖及其制备方法
HUANG ZHUQIANG (author) / ZHANG XIANGCHAO (author) / DENG MIN (author) / DENG MING (author) / WU ZEMIN (author) / CHEN LINKAI (author) / PENG LEKAI (author) / HU SHUAI (author) / TANG HAOYANG (author) / OUYANG JUNJIE (author)
2023-09-19
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
/
E04B
Allgemeine Baukonstruktionen
,
GENERAL BUILDING CONSTRUCTIONS
/
E04C
STRUCTURAL ELEMENTS
,
Bauelemente
/
F28D
Wärmetauscher, soweit in keiner anderen Unterklasse vorgesehen, in denen die Wärmetauschmittel nicht in direkte Berührung miteinander kommen
,
HEAT-EXCHANGE APPARATUS, NOT PROVIDED FOR IN ANOTHER SUBCLASS, IN WHICH THE HEAT-EXCHANGE MEDIA DO NOT COME INTO DIRECT CONTACT