A platform for research: civil engineering, architecture and urbanism
Mining area road repairing method
The invention relates to a mining area road repairing method which comprises the following steps: S1, preparing a repairing material, namely adding 55-65 parts by mass of stone powder, 8-10 parts by mass of slaked lime powder, 6-7 parts by mass of gypsum powder and 4-5 parts by mass of boric acid powder into a solution prepared from 3-4 parts by mass of formaldehyde, 1-2 parts by mass of acetone and 14-16 parts by mass of water, and uniformly stirring to prepare the repairing material; s2, carrying out coarse paving; s3, a land leveler is used for conducting fine scraping on the road surface subjected to coarse paving in the S2; s4, compacting is carried out; and S5, road maintenance is conducted, specifically, water is sprayed to the road surface compacted in the step S4, and a maintenance solution containing calcium chloride and sodium chloride is sprayed 3-5 days later. According to the road repairing method, the road integrity is improved, the road surface breaking degree is reduced, a muddy road surface is not prone to being formed, and the tire slipping phenomenon in the vehicle running process is reduced.
本发明是一种矿区道路修复方法,包括下述步骤:步骤S1:制备修复材料,将以下质量百分数的组分:石粉55‑65份、熟石灰粉8‑10份、石膏粉6‑7份和硼酸粉4‑5份,加入3‑4份甲醛、1‑2份丙酮和14‑16份水制成的溶液拌和均匀,制成修复材料;步骤S2:进行粗铺;步骤S3:使用平地机对S2粗铺后的路面进行精刮;步骤S4:压实;步骤S5:道路养护,对S4中压实后的路面洒水,3‑5天后喷洒含有氯化钙和氯化钠的养护溶液。本发明的道路修复方法使道路整体性提高,路面破碎程度降低,不易形成泥泞路面,降低车辆行驶中轮胎打滑的现象。
Mining area road repairing method
The invention relates to a mining area road repairing method which comprises the following steps: S1, preparing a repairing material, namely adding 55-65 parts by mass of stone powder, 8-10 parts by mass of slaked lime powder, 6-7 parts by mass of gypsum powder and 4-5 parts by mass of boric acid powder into a solution prepared from 3-4 parts by mass of formaldehyde, 1-2 parts by mass of acetone and 14-16 parts by mass of water, and uniformly stirring to prepare the repairing material; s2, carrying out coarse paving; s3, a land leveler is used for conducting fine scraping on the road surface subjected to coarse paving in the S2; s4, compacting is carried out; and S5, road maintenance is conducted, specifically, water is sprayed to the road surface compacted in the step S4, and a maintenance solution containing calcium chloride and sodium chloride is sprayed 3-5 days later. According to the road repairing method, the road integrity is improved, the road surface breaking degree is reduced, a muddy road surface is not prone to being formed, and the tire slipping phenomenon in the vehicle running process is reduced.
本发明是一种矿区道路修复方法,包括下述步骤:步骤S1:制备修复材料,将以下质量百分数的组分:石粉55‑65份、熟石灰粉8‑10份、石膏粉6‑7份和硼酸粉4‑5份,加入3‑4份甲醛、1‑2份丙酮和14‑16份水制成的溶液拌和均匀,制成修复材料;步骤S2:进行粗铺;步骤S3:使用平地机对S2粗铺后的路面进行精刮;步骤S4:压实;步骤S5:道路养护,对S4中压实后的路面洒水,3‑5天后喷洒含有氯化钙和氯化钠的养护溶液。本发明的道路修复方法使道路整体性提高,路面破碎程度降低,不易形成泥泞路面,降低车辆行驶中轮胎打滑的现象。
Mining area road repairing method
一种矿区道路修复方法
HU YANSHU (author) / LIU TIELIANG (author) / LI BAICHUAN (author) / HUANG FEI (author) / WANG LIANHAI (author) / ZHANG BAOHENG (author) / LI SHUYUAN (author) / JIA JUNZHANG (author) / WANG XIAOLONG (author) / WANG QINGBO (author)
2023-09-22
Patent
Electronic Resource
Chinese
Mining area collapse backfill area ecological management and repairing method
European Patent Office | 2020
|RESIN COMPOSITION FOR ROAD REPAIRING AND ROAD REPAIRING METHOD THEREWITH
European Patent Office | 2017
|