A platform for research: civil engineering, architecture and urbanism
Curing agent for waste drilling fluid and use method of curing agent
The invention discloses a curing agent for waste drilling fluid and a use method thereof, and the curing agent comprises the following components in parts by weight: 10-20 parts of silicate, 3-5 parts of ferrous sulfate, 30-45 parts of cement, 5-10 parts of carbide slag, 2-4 parts of sodium chlorate and 5-15 parts of plant ash. The use method comprises the following steps: firstly, adding the cement, the plant ash and the ferrous sulfate into the waste drilling fluid, heating to 50-150 DEG C, stirring for 1-5 hours, cooling to room temperature, adding the carbide slag, stirring for 1-2 hours, then adding the silicate and the chlorate, and uniformly stirring. The curing agent is low in formula cost, simple in use method and good in curing effect.
本发明公开了一种废弃钻井液用固化剂及其使用方法,其成分按重量份数计,包括:硅酸盐10‑20份、硫酸亚铁3‑5份、水泥30‑45份、电石渣5‑10份、氯酸钠2‑4份、草木灰5‑15份。使用方法包括以下步骤:首先向废弃钻井液中,加入水泥、草木灰和硫酸亚铁,加热至50‑150℃,搅拌1‑5h,冷却至室温后,加入电石渣,搅拌1‑2h,再向其中加入硅酸盐和氯酸盐,搅拌均匀,即可。本发明的固化剂配方成本低,使用方法简单,固化效果好。
Curing agent for waste drilling fluid and use method of curing agent
The invention discloses a curing agent for waste drilling fluid and a use method thereof, and the curing agent comprises the following components in parts by weight: 10-20 parts of silicate, 3-5 parts of ferrous sulfate, 30-45 parts of cement, 5-10 parts of carbide slag, 2-4 parts of sodium chlorate and 5-15 parts of plant ash. The use method comprises the following steps: firstly, adding the cement, the plant ash and the ferrous sulfate into the waste drilling fluid, heating to 50-150 DEG C, stirring for 1-5 hours, cooling to room temperature, adding the carbide slag, stirring for 1-2 hours, then adding the silicate and the chlorate, and uniformly stirring. The curing agent is low in formula cost, simple in use method and good in curing effect.
本发明公开了一种废弃钻井液用固化剂及其使用方法,其成分按重量份数计,包括:硅酸盐10‑20份、硫酸亚铁3‑5份、水泥30‑45份、电石渣5‑10份、氯酸钠2‑4份、草木灰5‑15份。使用方法包括以下步骤:首先向废弃钻井液中,加入水泥、草木灰和硫酸亚铁,加热至50‑150℃,搅拌1‑5h,冷却至室温后,加入电石渣,搅拌1‑2h,再向其中加入硅酸盐和氯酸盐,搅拌均匀,即可。本发明的固化剂配方成本低,使用方法简单,固化效果好。
Curing agent for waste drilling fluid and use method of curing agent
一种废弃钻井液用固化剂及其使用方法
GE LIAN (author) / QIAN FAN (author) / WU YI (author) / HE LONG (author) / ZHANG ZHANG (author) / WAN WEI (author) / YUAN YI (author) / TONG FUJIANG (author) / QIAN SIBEI (author) / HU ZONGJIAN (author)
2023-10-24
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Curing agent for fluid stabilized soil and preparation method of curing agent
European Patent Office | 2024
|Curing agent and curing method for phosphogypsum waste residues
European Patent Office | 2020
|Radioactive waste resin curing agent and curing method thereof
European Patent Office | 2024
|