A platform for research: civil engineering, architecture and urbanism
Wrinkle-grain-shaped matte double-layer reaction glaze for art ceramics and preparation method of wrinkle-grain-shaped matte double-layer reaction glaze
The invention discloses wrinkled-grain-shaped matte double-layer reaction glaze for art ceramics and a preparation method of the wrinkled-grain-shaped matte double-layer reaction glaze, and belongs to the technical field of preparation of glaze for art ceramics. The ground glaze comprises the following raw materials in parts by weight: 30-40 parts of potassium feldspar, 4-8 parts of zinc oxide, 5-7 parts of dolomite, 8-11 parts of quartz, 7-10 parts of kaolin, 7-10 parts of calcite powder, 4-5 parts of spodumene, 3-6 parts of talcum powder and 5-7 parts of bentonite; the cover glaze comprises the following raw materials in parts by weight: 7-11 parts of aluminum oxide, 25-35 parts of quartz, 5-10 parts of clay, 4-6 parts of zirconium silicate, 3-7 parts of zinc oxide and 15-20 parts of wollastonite, and the preparation method comprises the following steps: putting the raw materials into a ball mill, adding ballstone and water, carrying out ball milling and sieving to respectively obtain ground glaze slip and cover glaze slip, coating a green body with the ground glaze slip and the cover glaze slip, and firing to obtain a finished product. The artistic ceramic with the wrinkled grain shape and the matte effect is obtained.
本发明公开了一种艺术陶瓷的褶皱纹状哑光双层反应釉及其制备方法,属于艺术陶瓷釉料制备技术领域,本发明的双层反应釉从内向外分为底釉和面釉,底釉包括以下重量份原料:钾长石30‑40份、氧化锌4‑8份、白云石5‑7份、石英8‑11份、高岭土7‑10份、方解石粉7‑10份、锂辉石4‑5份、滑石粉3‑6份、膨润土5‑7份;面釉包括以下重量份原料:氧化铝7‑11份、石英25‑35份、粘土5‑10份、硅酸锆4‑6份、氧化锌3‑7份、硅灰石15‑20份,其制备方法为:将原料放入球磨机中,加入球石和水,球磨过筛,分别得到底釉釉浆和面釉釉浆,涂到坯体上烧制,得到具有褶皱纹状和哑光效果的艺术陶瓷。
Wrinkle-grain-shaped matte double-layer reaction glaze for art ceramics and preparation method of wrinkle-grain-shaped matte double-layer reaction glaze
The invention discloses wrinkled-grain-shaped matte double-layer reaction glaze for art ceramics and a preparation method of the wrinkled-grain-shaped matte double-layer reaction glaze, and belongs to the technical field of preparation of glaze for art ceramics. The ground glaze comprises the following raw materials in parts by weight: 30-40 parts of potassium feldspar, 4-8 parts of zinc oxide, 5-7 parts of dolomite, 8-11 parts of quartz, 7-10 parts of kaolin, 7-10 parts of calcite powder, 4-5 parts of spodumene, 3-6 parts of talcum powder and 5-7 parts of bentonite; the cover glaze comprises the following raw materials in parts by weight: 7-11 parts of aluminum oxide, 25-35 parts of quartz, 5-10 parts of clay, 4-6 parts of zirconium silicate, 3-7 parts of zinc oxide and 15-20 parts of wollastonite, and the preparation method comprises the following steps: putting the raw materials into a ball mill, adding ballstone and water, carrying out ball milling and sieving to respectively obtain ground glaze slip and cover glaze slip, coating a green body with the ground glaze slip and the cover glaze slip, and firing to obtain a finished product. The artistic ceramic with the wrinkled grain shape and the matte effect is obtained.
本发明公开了一种艺术陶瓷的褶皱纹状哑光双层反应釉及其制备方法,属于艺术陶瓷釉料制备技术领域,本发明的双层反应釉从内向外分为底釉和面釉,底釉包括以下重量份原料:钾长石30‑40份、氧化锌4‑8份、白云石5‑7份、石英8‑11份、高岭土7‑10份、方解石粉7‑10份、锂辉石4‑5份、滑石粉3‑6份、膨润土5‑7份;面釉包括以下重量份原料:氧化铝7‑11份、石英25‑35份、粘土5‑10份、硅酸锆4‑6份、氧化锌3‑7份、硅灰石15‑20份,其制备方法为:将原料放入球磨机中,加入球石和水,球磨过筛,分别得到底釉釉浆和面釉釉浆,涂到坯体上烧制,得到具有褶皱纹状和哑光效果的艺术陶瓷。
Wrinkle-grain-shaped matte double-layer reaction glaze for art ceramics and preparation method of wrinkle-grain-shaped matte double-layer reaction glaze
一种艺术陶瓷的褶皱纹状哑光双层反应釉及其制备方法
ZHANG LIANG (author) / WANG DAGU (author)
2023-10-31
Patent
Electronic Resource
Chinese
European Patent Office | 2021
|European Patent Office | 2015
|Black matte glaze for sanitary ware, sanitary ware and preparation method of black matte glaze
European Patent Office | 2024
|Ceramic with frosted matte glaze layer and preparation method thereof
European Patent Office | 2022
|Low-temperature matte reaction glaze and production method thereof
European Patent Office | 2015
|