The invention belongs to the technical field of building materials, and particularly relates to a green high-strength shield soil baking-free brick and a preparation method thereof.The baking-free brick is prepared from 60-80 parts of shield soil, 5-25 parts of waste glass particles, 10-20 parts of sand, 10-20 parts of cement, 1-10 parts of waste diatomite, 1-10 parts of waste glass powder and 5-10 parts of water. In the preparation process, the waste diatomite, the waste glass powder and the cement need to be pre-stirred and then mixed with other materials, meanwhile, water is added in a spraying mode, and finally the mixture is poured into a static pressure brick making machine mold. The shield soil baking-free brick obtained by the method has the characteristics of high strength, environmental protection and high economic benefit on the whole, and has a wide application prospect.
本发明属于建筑材料技术领域,具体涉及一种绿色高强盾构土免烧砖及其制备方法,所述免烧砖包括盾构土60~80份、废玻璃颗粒5~25份、砂子10~20份、水泥10~20份、废弃硅藻土1~10份、废玻璃粉1~10份以及水5~10份。制备过程中,需要将废弃硅藻土、废玻璃粉和水泥预搅拌,再与其他材料混合,同时加水方式采用喷洒,最后将混合料倒入到静压制砖机模具中。该方法获得的盾构土免烧砖整体上具有高强、绿色环保且经济效益高的特点,具有广阔的应用前景。
Green high-strength shield soil baking-free brick and preparation method thereof
The invention belongs to the technical field of building materials, and particularly relates to a green high-strength shield soil baking-free brick and a preparation method thereof.The baking-free brick is prepared from 60-80 parts of shield soil, 5-25 parts of waste glass particles, 10-20 parts of sand, 10-20 parts of cement, 1-10 parts of waste diatomite, 1-10 parts of waste glass powder and 5-10 parts of water. In the preparation process, the waste diatomite, the waste glass powder and the cement need to be pre-stirred and then mixed with other materials, meanwhile, water is added in a spraying mode, and finally the mixture is poured into a static pressure brick making machine mold. The shield soil baking-free brick obtained by the method has the characteristics of high strength, environmental protection and high economic benefit on the whole, and has a wide application prospect.
本发明属于建筑材料技术领域,具体涉及一种绿色高强盾构土免烧砖及其制备方法,所述免烧砖包括盾构土60~80份、废玻璃颗粒5~25份、砂子10~20份、水泥10~20份、废弃硅藻土1~10份、废玻璃粉1~10份以及水5~10份。制备过程中,需要将废弃硅藻土、废玻璃粉和水泥预搅拌,再与其他材料混合,同时加水方式采用喷洒,最后将混合料倒入到静压制砖机模具中。该方法获得的盾构土免烧砖整体上具有高强、绿色环保且经济效益高的特点,具有广阔的应用前景。
Green high-strength shield soil baking-free brick and preparation method thereof
一种绿色高强盾构土免烧砖及其制备方法
ZHANG BAOMING (author) / LIU BO (author) / MA XIAOTAO (author) / YE XIN (author) / SONG QINYUAN (author) / LI CHEN (author) / ZHANG MENGYUAN (author) / CHEN SIYI (author) / YANG XIAOYU (author) / CHEN TIANYU (author)
2023-11-21
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Shield muck biochar-based baking-free brick and preparation method thereof
European Patent Office | 2024
|Mudstone stratum shield muck baking-free brick and preparation method thereof
European Patent Office | 2024
|European Patent Office | 2023
|European Patent Office | 2023
|Residue soil baking-free brick and preparation method thereof
European Patent Office | 2021
|