Low-carbon SMA asphalt mixture
The invention discloses a low-carbon SMA asphalt mixture. The low-carbon SMA asphalt mixture is prepared from the following components in parts by weight: 80-120 parts of emulsified asphalt, 1.2-1.5 parts of a fiber stabilizer, 52-88 parts of cement, 25-46 parts of water, 15-35 parts of mineral powder, 22-36 parts of an epoxy curing agent, 3-17 parts of glass flakes and 0.5-1.5 parts of a toner. Natural minerals are adopted as raw materials, environmental pollution is avoided, emission of harmful substances such as CO2, SOx, NOx, VOC and dust is reduced, damage to the environment and harm to the health of constructors are reduced, meanwhile, the glass flakes are added, good supporting and protecting effects are provided, the waterproof and damp-proof effects are achieved, and moisture permeation is prevented.
本发明公开了一种低碳SMA沥青混合料,所述该低碳SMA沥青混合料的配方如下:乳化沥青80‑120份、纤维稳定剂1.2‑1.5份、水泥52‑88份、水25‑46份、矿粉15‑35份、环氧固化剂22‑36份、玻璃鳞片3‑17份、调色剂0.5‑1.5份。本发明采用天然矿物做原料,不会造成环境污染,同时减少CO2、SOx、NOx、VOC,粉尘等有害物质的排放,从而降低对环境的破坏和对施工人员的健康危害,同时,添加了玻璃鳞片,提供良好的支撑和保护作用同时还具有防水和防潮的作用,以防止水分渗透。
Low-carbon SMA asphalt mixture
The invention discloses a low-carbon SMA asphalt mixture. The low-carbon SMA asphalt mixture is prepared from the following components in parts by weight: 80-120 parts of emulsified asphalt, 1.2-1.5 parts of a fiber stabilizer, 52-88 parts of cement, 25-46 parts of water, 15-35 parts of mineral powder, 22-36 parts of an epoxy curing agent, 3-17 parts of glass flakes and 0.5-1.5 parts of a toner. Natural minerals are adopted as raw materials, environmental pollution is avoided, emission of harmful substances such as CO2, SOx, NOx, VOC and dust is reduced, damage to the environment and harm to the health of constructors are reduced, meanwhile, the glass flakes are added, good supporting and protecting effects are provided, the waterproof and damp-proof effects are achieved, and moisture permeation is prevented.
本发明公开了一种低碳SMA沥青混合料,所述该低碳SMA沥青混合料的配方如下:乳化沥青80‑120份、纤维稳定剂1.2‑1.5份、水泥52‑88份、水25‑46份、矿粉15‑35份、环氧固化剂22‑36份、玻璃鳞片3‑17份、调色剂0.5‑1.5份。本发明采用天然矿物做原料,不会造成环境污染,同时减少CO2、SOx、NOx、VOC,粉尘等有害物质的排放,从而降低对环境的破坏和对施工人员的健康危害,同时,添加了玻璃鳞片,提供良好的支撑和保护作用同时还具有防水和防潮的作用,以防止水分渗透。
Low-carbon SMA asphalt mixture
一种低碳SMA沥青混合料
HOU DESHAO (author) / XU BIN (author) / XU WENMING (author) / YUAN CONG (author) / HAN TIEJUN (author) / WANG HAIYAO (author)
2024-01-26
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
ASPHALT MODIFIER FOR ASPHALT MIXTURE AND ASPHALT MIXTURE COMPRISING SAME
European Patent Office | 2022
|European Patent Office | 2020
|Asphalt modifier, asphalt mixture and preparing methods of asphalt modifier and asphalt mixture
European Patent Office | 2015
|