A platform for research: civil engineering, architecture and urbanism
High-hardness low-energy-consumption artificial colored sand and preparation method thereof
The invention relates to the technical field of artificial colored sand, and discloses high-hardness low-energy-consumption artificial colored sand which comprises the following components: 1000 parts of a coloring base material, 5-15 parts of toner and 25-35 parts of a binder, wherein the binder is prepared from the following components in parts by weight: 40 to 60 parts of acidic silica sol, 30 to 60 parts of methyltrimethoxysilane, 15 to 30 parts of toughening emulsion, 10 to 30 parts of deionized water and 1 to 3 parts of glacial acetic acid. According to the preparation method of the high-hardness low-energy-consumption artificial colored sand, the components of the high-hardness low-energy-consumption artificial colored sand are used for preparing the artificial colored sand. The artificial colored sand has the characteristics of high wear resistance, high aging resistance and high gloss, is resistant to acid, alkali and corrosion, and can well meet the use requirements of colored sand for pavements, and the preparation method can be used for preparing the artificial colored sand at normal temperature, so that the energy consumption can be greatly reduced, the cost can be reduced, and energy conservation and emission reduction can be realized.
本发明涉及人工彩砂技术领域,公开了一种高硬度低能耗人工彩砂,包括如下组分:着色基材1000份,色粉5‑15份,粘结剂25‑35份;其中的粘结剂按重量份数计,包括如下组分:酸性硅溶胶40‑60份,甲基三甲氧基硅烷30‑60份,增韧乳液15‑30份,去离子水10‑30份,冰乙酸1‑3份。一种高硬度低能耗人工彩砂的制备方法,使用上述的高硬度低能耗人工彩砂的组分,用于制备人工彩砂。本发明的人工彩砂具有高耐磨、高耐老化、高光泽的特性,耐酸碱、耐锈蚀,能够较好的满足路面用彩砂的使用要求,且其制备方法能够在常温下制备上述人工彩砂,能够大大降低能耗,降低成本,实现节能减排。
High-hardness low-energy-consumption artificial colored sand and preparation method thereof
The invention relates to the technical field of artificial colored sand, and discloses high-hardness low-energy-consumption artificial colored sand which comprises the following components: 1000 parts of a coloring base material, 5-15 parts of toner and 25-35 parts of a binder, wherein the binder is prepared from the following components in parts by weight: 40 to 60 parts of acidic silica sol, 30 to 60 parts of methyltrimethoxysilane, 15 to 30 parts of toughening emulsion, 10 to 30 parts of deionized water and 1 to 3 parts of glacial acetic acid. According to the preparation method of the high-hardness low-energy-consumption artificial colored sand, the components of the high-hardness low-energy-consumption artificial colored sand are used for preparing the artificial colored sand. The artificial colored sand has the characteristics of high wear resistance, high aging resistance and high gloss, is resistant to acid, alkali and corrosion, and can well meet the use requirements of colored sand for pavements, and the preparation method can be used for preparing the artificial colored sand at normal temperature, so that the energy consumption can be greatly reduced, the cost can be reduced, and energy conservation and emission reduction can be realized.
本发明涉及人工彩砂技术领域,公开了一种高硬度低能耗人工彩砂,包括如下组分:着色基材1000份,色粉5‑15份,粘结剂25‑35份;其中的粘结剂按重量份数计,包括如下组分:酸性硅溶胶40‑60份,甲基三甲氧基硅烷30‑60份,增韧乳液15‑30份,去离子水10‑30份,冰乙酸1‑3份。一种高硬度低能耗人工彩砂的制备方法,使用上述的高硬度低能耗人工彩砂的组分,用于制备人工彩砂。本发明的人工彩砂具有高耐磨、高耐老化、高光泽的特性,耐酸碱、耐锈蚀,能够较好的满足路面用彩砂的使用要求,且其制备方法能够在常温下制备上述人工彩砂,能够大大降低能耗,降低成本,实现节能减排。
High-hardness low-energy-consumption artificial colored sand and preparation method thereof
一种高硬度低能耗人工彩砂及其制备方法
HU ZHONGYUAN (author) / YAO WEI (author) / ZHANG XUTAO (author)