The invention provides a manufacturing method of an environment-friendly brick containing marine wastes such as oyster shells, and the manufacturing method of the environment-friendly brick comprises the following steps: cleaning and cutting biological shells to obtain a first-class material; crushing and grinding the first-class material to obtain a granular second-class material; mixing the first-class material, the second-class material, silica powder, cement and pigment in proportion to form a base material, adding a proper amount of water, and stirring to form a mixture; and pouring the stirred mixture into a mold, discharging bubbles, and curing to form a brick body. Through continuously improved proportion and process design in research, a large amount of marine wastes such as fresh oyster shells and the like are used, and the resource utilization rate is increased. The environment-friendly brick disclosed by the invention has good physical properties and unique appearance, can be widely applied to the fields of buildings, roads, squares and the like, and has relatively high economic values and environment-friendly benefits.
本发明提供了一种包含生蚝壳等海洋废弃物的环保砖制作方法,所述环保砖制作方法包括:将生物外壳,经过清洗、切割处理,得到一类料;将上述一类料进行破碎与研磨,得到颗粒状二类料;将一类料、二类料、硅微粉、水泥和颜料按照比例混合为基料,添加适量水进行搅拌形成混合物;将搅拌后的混合物倒入模具,排出气泡,固化后形成砖体。通过在研究中不断改进的配比和工艺设计,大量使用了生蚝壳等海洋废弃物,提高资源利用率。本发明的环保砖具有良好的物理性能和独特外观,可广泛应用于建筑、道路、广场等领域,具有较高的经济价值和环保效益。
Manufacturing method of environment-friendly brick
The invention provides a manufacturing method of an environment-friendly brick containing marine wastes such as oyster shells, and the manufacturing method of the environment-friendly brick comprises the following steps: cleaning and cutting biological shells to obtain a first-class material; crushing and grinding the first-class material to obtain a granular second-class material; mixing the first-class material, the second-class material, silica powder, cement and pigment in proportion to form a base material, adding a proper amount of water, and stirring to form a mixture; and pouring the stirred mixture into a mold, discharging bubbles, and curing to form a brick body. Through continuously improved proportion and process design in research, a large amount of marine wastes such as fresh oyster shells and the like are used, and the resource utilization rate is increased. The environment-friendly brick disclosed by the invention has good physical properties and unique appearance, can be widely applied to the fields of buildings, roads, squares and the like, and has relatively high economic values and environment-friendly benefits.
本发明提供了一种包含生蚝壳等海洋废弃物的环保砖制作方法,所述环保砖制作方法包括:将生物外壳,经过清洗、切割处理,得到一类料;将上述一类料进行破碎与研磨,得到颗粒状二类料;将一类料、二类料、硅微粉、水泥和颜料按照比例混合为基料,添加适量水进行搅拌形成混合物;将搅拌后的混合物倒入模具,排出气泡,固化后形成砖体。通过在研究中不断改进的配比和工艺设计,大量使用了生蚝壳等海洋废弃物,提高资源利用率。本发明的环保砖具有良好的物理性能和独特外观,可广泛应用于建筑、道路、广场等领域,具有较高的经济价值和环保效益。
Manufacturing method of environment-friendly brick
一种环保砖的制作方法
NIRI EDOARDO (author)
2024-08-13
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
European Patent Office | 2021
|Environment-friendly PC brick and manufacturing method thereof
European Patent Office | 2022
|Environment-friendly brick manufacturing process and mold
European Patent Office | 2021
|