Environment-friendly low-temperature wine bottle glaze and preparation method thereof
The invention discloses environment-friendly low-temperature wine bottle glaze and a preparation method thereof, and belongs to the technical field of wine bottle glaze, and the wine bottle glaze comprises the following raw materials in parts by weight: 5-10 parts of hybrid sol, 3-10 parts of barium carbonate, 35-45 parts of potassium feldspar, 2-4 parts of aluminum oxide, 5-10 parts of lithium chinastone, 35-40 parts of quartz, 3-10 parts of kaolin, 10-15 parts of zirconium silicate, 2-5 parts of low-temperature frit and 1-3 parts of a carbon fiber reinforced component. The carbon fiber reinforced component is graphene oxide coated carbon fiber, the hybrid sol is prepared from Ce doped nano Ti O2, polyvinyl butyral, aluminum nitrate nonahydrate, tetraethyl silicate and absolute ethyl alcohol, and compared with traditional wine bottle glaze, the hybrid sol and the carbon fiber reinforced component are introduced into the wine bottle glaze, so that the obtained wine bottle glaze is good in glossiness, good in elasticity and good in anti-aging performance. The glaze surface is fine and smooth, the strength is high, and the antibacterial wear resistance is good.
本发明公开了一种环保低温酒瓶釉及其制备方法,属于酒瓶釉技术领域,酒瓶釉包括以下重量份原料:杂化溶胶5‑10份、碳酸钡3‑10份、钾长石35‑45份、氧化铝2‑4份、锂瓷石5‑10份、石英35‑40份、高岭土3‑10份、硅酸锆10‑15份、低温熔块2‑5份、碳纤维增强组分1‑3份,所述碳纤维增强组分为氧化石墨烯包覆碳纤维,杂化溶胶由Ce掺杂纳米T i O2、聚乙烯醇缩丁醛、九水合硝酸铝、硅酸四乙酯、无水乙醇组成,相比于传统的酒瓶釉而言,本发明在酒瓶釉中引入了杂化溶胶和碳纤维增强组分,使获得的酒瓶釉面光泽好,釉面细腻、光滑,且强度高、抗菌耐磨性好。
Environment-friendly low-temperature wine bottle glaze and preparation method thereof
The invention discloses environment-friendly low-temperature wine bottle glaze and a preparation method thereof, and belongs to the technical field of wine bottle glaze, and the wine bottle glaze comprises the following raw materials in parts by weight: 5-10 parts of hybrid sol, 3-10 parts of barium carbonate, 35-45 parts of potassium feldspar, 2-4 parts of aluminum oxide, 5-10 parts of lithium chinastone, 35-40 parts of quartz, 3-10 parts of kaolin, 10-15 parts of zirconium silicate, 2-5 parts of low-temperature frit and 1-3 parts of a carbon fiber reinforced component. The carbon fiber reinforced component is graphene oxide coated carbon fiber, the hybrid sol is prepared from Ce doped nano Ti O2, polyvinyl butyral, aluminum nitrate nonahydrate, tetraethyl silicate and absolute ethyl alcohol, and compared with traditional wine bottle glaze, the hybrid sol and the carbon fiber reinforced component are introduced into the wine bottle glaze, so that the obtained wine bottle glaze is good in glossiness, good in elasticity and good in anti-aging performance. The glaze surface is fine and smooth, the strength is high, and the antibacterial wear resistance is good.
本发明公开了一种环保低温酒瓶釉及其制备方法,属于酒瓶釉技术领域,酒瓶釉包括以下重量份原料:杂化溶胶5‑10份、碳酸钡3‑10份、钾长石35‑45份、氧化铝2‑4份、锂瓷石5‑10份、石英35‑40份、高岭土3‑10份、硅酸锆10‑15份、低温熔块2‑5份、碳纤维增强组分1‑3份,所述碳纤维增强组分为氧化石墨烯包覆碳纤维,杂化溶胶由Ce掺杂纳米T i O2、聚乙烯醇缩丁醛、九水合硝酸铝、硅酸四乙酯、无水乙醇组成,相比于传统的酒瓶釉而言,本发明在酒瓶釉中引入了杂化溶胶和碳纤维增强组分,使获得的酒瓶釉面光泽好,釉面细腻、光滑,且强度高、抗菌耐磨性好。
Environment-friendly low-temperature wine bottle glaze and preparation method thereof
一种环保低温酒瓶釉及其制备方法
PAN JUNMING (author) / YI WEI (author) / PAN-XIANG CHUANZI (author) / LU RIGAO (author) / HU JIAN (author) / ZHANG XINQIAO (author) / XU YA (author)
2024-08-23
Patent
Electronic Resource
Chinese
Ceramic wine bottle inner glaze and preparation method thereof
European Patent Office | 2024
|Environment-friendly ceramic glaze and preparation method thereof
European Patent Office | 2021
|Environment-friendly agate glaze and preparation process thereof
European Patent Office | 2021
|Sintering method of colored ceramic glaze for wine bottle production
European Patent Office | 2022
|Manufacturing method of high-strength crackle glaze ceramic wine bottle
European Patent Office | 2021
|