Preparation method of medium-entropy boron carbide ceramic
The invention relates to the technical field of carbide ceramics, in particular to a preparation method of medium-entropy boron carbide ceramics. According to the method, firstly, TiO2 powder, ZrO2 powder, Ta2O5 powder and C powder are subjected to ball milling and mixing and then subjected to two times of vacuum heat treatment to obtain (Ti1/3Zr1/3Ta1/3) C ceramic powder, then the (Ti1/3Zr1/3Ta1/3) C ceramic powder is mixed with B4C and then subjected to a boron heat reaction to prepare the medium-entropy (Ti1/3Zr1/3Ta1/3) ByCz boron carbide ceramic, and # imgabs0 is combined with the high-temperature-resistant characteristic of carbide and the anti-oxidation characteristic of boride, so that the medium-entropy (Ti1/3Zr1/3Ta1/3) ByCz boron carbide ceramic is prepared. The novel medium-entropy (Ti1/3Zr1/3Ta1/3) ByCz boron carbide ceramic with excellent performance is prepared, the operation is simple, rapid and controllable, the cost is low, and the green and energy-saving concept is met.
本发明涉及碳化物陶瓷技术领域,具体涉及一种中熵硼碳化物陶瓷的制备方法。本发明方法首先将TiO2、ZrO2、Ta2O5粉末与C粉球磨混合后经两次真空热处理后得到(Ti1/3Zr1/3Ta1/3)C陶瓷粉体,然后再将其与B4C混合后经硼热反应后制得中熵(Ti1/3Zr1/3Ta1/3)ByCz硼碳化物陶瓷,其中,#imgabs0#本发明方法结合碳化物的耐高温特性和硼化物的抗氧化特性,制备出具有优异性能的新型中熵(Ti1/3Zr1/3Ta1/3)ByCz硼碳化物陶瓷,操作简单快捷可控,成本低廉,符合绿色节能理念。
Preparation method of medium-entropy boron carbide ceramic
The invention relates to the technical field of carbide ceramics, in particular to a preparation method of medium-entropy boron carbide ceramics. According to the method, firstly, TiO2 powder, ZrO2 powder, Ta2O5 powder and C powder are subjected to ball milling and mixing and then subjected to two times of vacuum heat treatment to obtain (Ti1/3Zr1/3Ta1/3) C ceramic powder, then the (Ti1/3Zr1/3Ta1/3) C ceramic powder is mixed with B4C and then subjected to a boron heat reaction to prepare the medium-entropy (Ti1/3Zr1/3Ta1/3) ByCz boron carbide ceramic, and # imgabs0 is combined with the high-temperature-resistant characteristic of carbide and the anti-oxidation characteristic of boride, so that the medium-entropy (Ti1/3Zr1/3Ta1/3) ByCz boron carbide ceramic is prepared. The novel medium-entropy (Ti1/3Zr1/3Ta1/3) ByCz boron carbide ceramic with excellent performance is prepared, the operation is simple, rapid and controllable, the cost is low, and the green and energy-saving concept is met.
本发明涉及碳化物陶瓷技术领域,具体涉及一种中熵硼碳化物陶瓷的制备方法。本发明方法首先将TiO2、ZrO2、Ta2O5粉末与C粉球磨混合后经两次真空热处理后得到(Ti1/3Zr1/3Ta1/3)C陶瓷粉体,然后再将其与B4C混合后经硼热反应后制得中熵(Ti1/3Zr1/3Ta1/3)ByCz硼碳化物陶瓷,其中,#imgabs0#本发明方法结合碳化物的耐高温特性和硼化物的抗氧化特性,制备出具有优异性能的新型中熵(Ti1/3Zr1/3Ta1/3)ByCz硼碳化物陶瓷,操作简单快捷可控,成本低廉,符合绿色节能理念。
Preparation method of medium-entropy boron carbide ceramic
一种中熵硼碳化物陶瓷的制备方法
XIE WEI (author) / ZHANG ZHILUN (author) / WANG HAILONG (author) / LI MINGLIANG (author) / FANG CHENG (author) / LIU WEN (author) / LU HONGXIA (author) / XU HONGLIANG (author)
2024-09-13
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
European Patent Office | 2020
|Layered high-entropy double-boron carbide ceramic powder and preparation method thereof
European Patent Office | 2021
|