Core-shell structure nanowire toughened plasma spraying ZrC-SiC coating and preparation method thereof
The invention discloses a core-shell structure nanowire toughened plasma spraying ZrC-SiC coating and a preparation method thereof. The preparation method comprises the following steps: 1) pretreating a C/C composite material; 2) preparing a SiC-coated SiO2 nanowire layer on the surface of the C/C composite material to obtain a C/C composite material with SiC-coated SiO2 nanowires growing on the surface; 3) coating a PyC layer on the surface of the C/C composite material with the SiC-coated SiO2 nanowires grown on the surface to obtain a C/C composite material with SiC-coated SiO2-coated PyC nanowires grown on the surface; and 4) spraying a ZrC-SiC coating on the surface of the C/C composite material with the SiC (at) SiO2 (at) PyC nanowire growing on the surface to obtain the core-shell structure nanowire toughened plasma spraying ZrC-SiC coating, and the coating and the preparation method thereof can solve the problems of high brittleness of a plasma spraying ceramic coating and poor bonding force of a coating-matrix interface.
本发明公开了一种核壳结构纳米线增韧等离子喷涂ZrC‑SiC涂层及其制备方法,包括以下步骤:1)对C/C复合材料进行预处理;2)在C/C复合材料的表面制备SiC@SiO2纳米线层,得到表面生长有SiC@SiO2纳米线的C/C复合材料;3)在所述表面生长有SiC@SiO2纳米线的C/C复合材料的表面包覆PyC层,得到表面生长有SiC@SiO2@PyC纳米线的C/C复合材料;4)在表面生长有SiC@SiO2@PyC纳米线的C/C复合材料的表面喷涂ZrC‑SiC涂层,得到核壳结构纳米线增韧等离子喷涂ZrC‑SiC涂层,该涂层及其制备方法能够解决等离子喷涂陶瓷涂层脆性大以及涂层‑基体界面结合力差的问题。
Core-shell structure nanowire toughened plasma spraying ZrC-SiC coating and preparation method thereof
The invention discloses a core-shell structure nanowire toughened plasma spraying ZrC-SiC coating and a preparation method thereof. The preparation method comprises the following steps: 1) pretreating a C/C composite material; 2) preparing a SiC-coated SiO2 nanowire layer on the surface of the C/C composite material to obtain a C/C composite material with SiC-coated SiO2 nanowires growing on the surface; 3) coating a PyC layer on the surface of the C/C composite material with the SiC-coated SiO2 nanowires grown on the surface to obtain a C/C composite material with SiC-coated SiO2-coated PyC nanowires grown on the surface; and 4) spraying a ZrC-SiC coating on the surface of the C/C composite material with the SiC (at) SiO2 (at) PyC nanowire growing on the surface to obtain the core-shell structure nanowire toughened plasma spraying ZrC-SiC coating, and the coating and the preparation method thereof can solve the problems of high brittleness of a plasma spraying ceramic coating and poor bonding force of a coating-matrix interface.
本发明公开了一种核壳结构纳米线增韧等离子喷涂ZrC‑SiC涂层及其制备方法,包括以下步骤:1)对C/C复合材料进行预处理;2)在C/C复合材料的表面制备SiC@SiO2纳米线层,得到表面生长有SiC@SiO2纳米线的C/C复合材料;3)在所述表面生长有SiC@SiO2纳米线的C/C复合材料的表面包覆PyC层,得到表面生长有SiC@SiO2@PyC纳米线的C/C复合材料;4)在表面生长有SiC@SiO2@PyC纳米线的C/C复合材料的表面喷涂ZrC‑SiC涂层,得到核壳结构纳米线增韧等离子喷涂ZrC‑SiC涂层,该涂层及其制备方法能够解决等离子喷涂陶瓷涂层脆性大以及涂层‑基体界面结合力差的问题。
Core-shell structure nanowire toughened plasma spraying ZrC-SiC coating and preparation method thereof
一种核壳结构纳米线增韧等离子喷涂ZrC-SiC涂层及其制备方法
LI HEJUN (author) / XU TING (author) / SUN JIA (author) / LIU BING (author) / OU HONGKANG (author) / GUO LINGXIANG (author)
2024-10-25
Patent
Electronic Resource
Chinese
Nanowire toughened ultrahigh-temperature anti-ablation coating and preparation method thereof
European Patent Office | 2024
|European Patent Office | 2024
|European Patent Office | 2024
|European Patent Office | 2021
|Method for preparing whisker toughened composite coating by liquid-phase method spraying process
European Patent Office | 2021
|