Lepidolite particle insulating brick and preparation method thereof
The invention discloses a lepidolite particle insulating brick and a preparation method thereof, the lepidolite particle insulating brick is prepared from the following raw materials in percentage by mass: 40-80% of lepidolite particles and 20-60% of cement, and the lepidolite particles are prepared by taking lepidolite as a raw material through granulation, roasting and leaching. In the invention, the lepidolite particles have the characteristics of low density, high porosity, low heat conductivity coefficient, high strength and the like, and the lepidolite particle insulating brick with light weight, high compressive strength and excellent thermal insulation performance can be formed after the lepidolite particles are compounded with the cement; the adopted lepidolite particles can be directly utilized and do not need to be subjected to pretreatment such as grinding and drying, the preparation process is simpler, operation is more convenient, production energy consumption is lower, the preparation method is suitable for large-scale preparation, industrial application of the lepidolite particle insulating brick is convenient to achieve, the adopted lepidolite particles are large in dosage, and the cost is low. The method can realize large-quantity resource utilization of the lepidolite particles, and can effectively solve the environmental problem of the lepidolite particles.
本发明公开了一种锂云母粒保温砖及其制备方法,该锂云母粒保温砖按照质量百分比计由以下原料制成:40%~80%的锂云母粒和20%~60%的水泥,其中锂云母粒是以锂云母为原料经制粒、焙烧、浸出后制备得到。本发明中,锂云母粒具有密度低、孔隙率高、导热系数低、强度高等特点,与水泥复配后即可形成兼具质轻、抗压强度高、保温性能优异的锂云母粒保温砖;采用的锂云母粒可直接利用,无需对锂云母粒进行粉磨及烘干等预处理,制备工艺更加简单,操作更加方便,生产能耗更低,适合于大规模制备,便于实现锂云母粒保温砖的工业化应用,而且采用的锂云母粒用量大,可实现锂云母粒的大宗量资源化利用,并能有效解决锂云母粒存在环境问题。
Lepidolite particle insulating brick and preparation method thereof
The invention discloses a lepidolite particle insulating brick and a preparation method thereof, the lepidolite particle insulating brick is prepared from the following raw materials in percentage by mass: 40-80% of lepidolite particles and 20-60% of cement, and the lepidolite particles are prepared by taking lepidolite as a raw material through granulation, roasting and leaching. In the invention, the lepidolite particles have the characteristics of low density, high porosity, low heat conductivity coefficient, high strength and the like, and the lepidolite particle insulating brick with light weight, high compressive strength and excellent thermal insulation performance can be formed after the lepidolite particles are compounded with the cement; the adopted lepidolite particles can be directly utilized and do not need to be subjected to pretreatment such as grinding and drying, the preparation process is simpler, operation is more convenient, production energy consumption is lower, the preparation method is suitable for large-scale preparation, industrial application of the lepidolite particle insulating brick is convenient to achieve, the adopted lepidolite particles are large in dosage, and the cost is low. The method can realize large-quantity resource utilization of the lepidolite particles, and can effectively solve the environmental problem of the lepidolite particles.
本发明公开了一种锂云母粒保温砖及其制备方法,该锂云母粒保温砖按照质量百分比计由以下原料制成:40%~80%的锂云母粒和20%~60%的水泥,其中锂云母粒是以锂云母为原料经制粒、焙烧、浸出后制备得到。本发明中,锂云母粒具有密度低、孔隙率高、导热系数低、强度高等特点,与水泥复配后即可形成兼具质轻、抗压强度高、保温性能优异的锂云母粒保温砖;采用的锂云母粒可直接利用,无需对锂云母粒进行粉磨及烘干等预处理,制备工艺更加简单,操作更加方便,生产能耗更低,适合于大规模制备,便于实现锂云母粒保温砖的工业化应用,而且采用的锂云母粒用量大,可实现锂云母粒的大宗量资源化利用,并能有效解决锂云母粒存在环境问题。
Lepidolite particle insulating brick and preparation method thereof
一种锂云母粒保温砖及其制备方法
CHEN YIHENG (author) / ZENG QINGPO (author) / ZHOU KAI (author) / TONG HAOWEN (author) / HUANG BINGJIE (author) / CHEN ZEJIAN (author) / ZHANG QINGYU (author)
2024-11-08
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Honeycomb insulating brick and preparation method thereof
European Patent Office | 2020
|Waterproof insulating brick and preparation method thereof
European Patent Office | 2021
|