1. 5. 7 type basic magnesium sulfate whisker reinforced basic magnesium sulfate cement and preparation method thereof
The invention discloses 1. 5. 7 type basic magnesium sulfate whisker reinforced basic magnesium sulfate cement and a preparation method thereof, and belongs to the technical field of building material preparation. The invention relates to 1. 5. 7 type basic magnesium sulfate whisker reinforced basic magnesium sulfate cement, which is prepared from the following main raw materials: 1. 5. 7 type basic magnesium sulfate whiskers of which the length-diameter ratio is greater than 100 and the average length is 10-40 microns. According to the 1. 5. 7 type basic magnesium sulfate whisker reinforced basic magnesium sulfate cement disclosed by the invention, due to the addition of the 1. 5. 7 type basic magnesium sulfate whisker with the length-diameter ratio of more than 100 and the average length of 10-40 microns, the cement disclosed by the invention has good compression resistance and breaking strength and is short in setting time; according to the preparation method, only the inorganic whiskers are added, other additives are not added, and the method is economical and environment-friendly.
本发明公开了一种1·5·7型碱式硫酸镁晶须增强碱式硫酸镁水泥及其制备方法,属于建筑材料制备技术领域。一种1·5·7型碱式硫酸镁晶须增强碱式硫酸镁水泥,其采用的主要原料为:形貌为长径比>100、平均长度为10‑40μm的1·5·7型碱式硫酸镁晶须。本发明的一种1·5·7型碱式硫酸镁晶须增强碱式硫酸镁水泥,由于长径比>100、平均长度为10‑40μm的1·5·7型碱式硫酸镁晶须的加入,使得本发明的水泥具有良好的抗压、抗折强度,同时凝结时间快;该制备方法只添加无机晶须,不添加其他外加剂,经济环保。
1. 5. 7 type basic magnesium sulfate whisker reinforced basic magnesium sulfate cement and preparation method thereof
The invention discloses 1. 5. 7 type basic magnesium sulfate whisker reinforced basic magnesium sulfate cement and a preparation method thereof, and belongs to the technical field of building material preparation. The invention relates to 1. 5. 7 type basic magnesium sulfate whisker reinforced basic magnesium sulfate cement, which is prepared from the following main raw materials: 1. 5. 7 type basic magnesium sulfate whiskers of which the length-diameter ratio is greater than 100 and the average length is 10-40 microns. According to the 1. 5. 7 type basic magnesium sulfate whisker reinforced basic magnesium sulfate cement disclosed by the invention, due to the addition of the 1. 5. 7 type basic magnesium sulfate whisker with the length-diameter ratio of more than 100 and the average length of 10-40 microns, the cement disclosed by the invention has good compression resistance and breaking strength and is short in setting time; according to the preparation method, only the inorganic whiskers are added, other additives are not added, and the method is economical and environment-friendly.
本发明公开了一种1·5·7型碱式硫酸镁晶须增强碱式硫酸镁水泥及其制备方法,属于建筑材料制备技术领域。一种1·5·7型碱式硫酸镁晶须增强碱式硫酸镁水泥,其采用的主要原料为:形貌为长径比>100、平均长度为10‑40μm的1·5·7型碱式硫酸镁晶须。本发明的一种1·5·7型碱式硫酸镁晶须增强碱式硫酸镁水泥,由于长径比>100、平均长度为10‑40μm的1·5·7型碱式硫酸镁晶须的加入,使得本发明的水泥具有良好的抗压、抗折强度,同时凝结时间快;该制备方法只添加无机晶须,不添加其他外加剂,经济环保。
1. 5. 7 type basic magnesium sulfate whisker reinforced basic magnesium sulfate cement and preparation method thereof
一种1·5·7型碱式硫酸镁晶须增强碱式硫酸镁水泥及其制备方法
XU XUN (author) / SUN YONGTAO (author) / LIN TIANCHENG (author) / ZHU BEI (author) / HU HAILONG (author)
2024-11-12
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Inorganic whisker reinforced basic magnesium sulfate foaming cement and preparation method thereof
European Patent Office | 2021
|Basic magnesium sulfate cement and preparation method thereof
European Patent Office | 2021
|Basic magnesium sulfate cement and preparation method thereof
European Patent Office | 2024
|Basic magnesium sulfate cement concrete and preparation method thereof
European Patent Office | 2022
|Antifatigue basic magnesium sulfate cement and preparation method thereof
European Patent Office | 2015
|