Low-temperature fast-firing slurry containing lithium tailings and ceramic bathroom high-pressure grouting product prepared from low-temperature fast-firing slurry
The invention discloses a lithium-tailing-containing low-temperature fast-firing slurry, which is prepared from the following raw materials in parts by mass: 10 to 20 parts of lithium tailings, 10 to 20 parts of china clay, 10 to 20 parts of chinastone, 10 to 20 parts of kaolin, 10 to 20 parts of sericite clay, 0 to 10 parts of black clay, 0 to 5 parts of wollastonite, 0 to 5 parts of magnesian soil, 0 to 10 parts of potassium-sodium feldspar and 5 to 15 parts of high-temperature sand. The melting temperature of the high-temperature sand ranges from 1250 DEG C to 1300 DEG C. According to the low-temperature fast-firing slurry containing the lithium tailings and the ceramic bathroom high-pressure grouting product thereof provided by the technical scheme, the raw material formula of the slurry is optimized by introducing the lithium tailings, so that low-temperature fast firing of a bathroom ceramic green body is realized, the production cost of the bathroom ceramic product is greatly reduced, and the production efficiency is improved. And meanwhile, the production efficiency of bathroom ceramic products is improved, and the defects in the prior art are overcome.
本发明公开了一种含锂尾矿的低温快烧泥浆,按照质量份数,包括以下原料:锂尾矿10~20份、瓷土10~20份、瓷石10~20份、高岭土10~20份、绢云母泥土料10~20份、黑泥0~10份、硅灰石0~5份、镁质土0~5份、钾钠长石0~10份和高温砂5~15份;所述高温砂的熔融温度为1250~1300°。本技术方案提出的一种含锂尾矿的低温快烧泥浆及其陶瓷卫浴高压注浆制品,通过引入锂尾矿对泥浆的原料配方进行优化,从而实现卫浴陶瓷坯体的低温快烧,极大地降低了卫浴陶瓷制品的生产成本,同时提高了卫浴陶瓷制品的生产效率,以克服现有技术中的不足之处。
Low-temperature fast-firing slurry containing lithium tailings and ceramic bathroom high-pressure grouting product prepared from low-temperature fast-firing slurry
The invention discloses a lithium-tailing-containing low-temperature fast-firing slurry, which is prepared from the following raw materials in parts by mass: 10 to 20 parts of lithium tailings, 10 to 20 parts of china clay, 10 to 20 parts of chinastone, 10 to 20 parts of kaolin, 10 to 20 parts of sericite clay, 0 to 10 parts of black clay, 0 to 5 parts of wollastonite, 0 to 5 parts of magnesian soil, 0 to 10 parts of potassium-sodium feldspar and 5 to 15 parts of high-temperature sand. The melting temperature of the high-temperature sand ranges from 1250 DEG C to 1300 DEG C. According to the low-temperature fast-firing slurry containing the lithium tailings and the ceramic bathroom high-pressure grouting product thereof provided by the technical scheme, the raw material formula of the slurry is optimized by introducing the lithium tailings, so that low-temperature fast firing of a bathroom ceramic green body is realized, the production cost of the bathroom ceramic product is greatly reduced, and the production efficiency is improved. And meanwhile, the production efficiency of bathroom ceramic products is improved, and the defects in the prior art are overcome.
本发明公开了一种含锂尾矿的低温快烧泥浆,按照质量份数,包括以下原料:锂尾矿10~20份、瓷土10~20份、瓷石10~20份、高岭土10~20份、绢云母泥土料10~20份、黑泥0~10份、硅灰石0~5份、镁质土0~5份、钾钠长石0~10份和高温砂5~15份;所述高温砂的熔融温度为1250~1300°。本技术方案提出的一种含锂尾矿的低温快烧泥浆及其陶瓷卫浴高压注浆制品,通过引入锂尾矿对泥浆的原料配方进行优化,从而实现卫浴陶瓷坯体的低温快烧,极大地降低了卫浴陶瓷制品的生产成本,同时提高了卫浴陶瓷制品的生产效率,以克服现有技术中的不足之处。
Low-temperature fast-firing slurry containing lithium tailings and ceramic bathroom high-pressure grouting product prepared from low-temperature fast-firing slurry
一种含锂尾矿的低温快烧泥浆及其陶瓷卫浴高压注浆制品
BAI JINGJING (author) / ZHANG BAOMEI (author) / XUE FUQIN (author) / YANG LIXIN (author)
2024-11-15
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
European Patent Office | 2022
|Low-temperature fast firing method for ceramic production
European Patent Office | 2023
|High-pressure grouting ceramic slurry and preparation method thereof
European Patent Office | 2020
|European Patent Office | 2022
|Low-temperature fast firing blue crystalline glaze composition
European Patent Office | 2015
|