Composite inorganic terrace material
The invention discloses a composite inorganic terrace material, and relates to the technical field of concrete. The composite inorganic terrace material is prepared from the following components in percentage by mass: Portland cement, aggregate, blast furnace iron-smelting slag, anti-crack fibers, glass powder, an activating agent and a micro-expanding agent, the preparation method of the micro-expanding agent comprises the following steps: taking the lithium slag and the red mud, crushing the lithium slag and the red mud, adding water, uniformly stirring, then granulating, forming and sintering, and crushing a sintered product to obtain the micro-expanding agent. The composite inorganic terrace material disclosed by the invention has relatively high compressive strength and tensile strength, the concrete terrace disclosed by the invention has certain micro-expansion performance, and the micro-expansion rate of the terrace in the whole hardening period is relatively gentle. The terrace material disclosed by the invention has relatively good anti-cracking performance due to the conditions.
本发明公开了一种复合无机地坪材料,涉及混凝土技术领域。以质量百分比计,该复合无机地坪材料包括:硅酸盐水泥,集料,高炉冶铁矿渣,抗裂纤维,玻璃粉,激活剂,微膨胀剂;所述微膨胀剂的制备方法包括以下步骤:取锂渣、赤泥,对其粉碎后,加水搅拌均匀,随后对其造粒成型并烧结,对烧结产物进行粉碎即得。本发明的复合无机地坪材料,其具有较高的抗压强度以及较高的抗拉强度,且本发明的混凝土地坪具有一定的微膨胀性能,且在地坪的整个硬化周期内的微膨胀率相对平缓。这些情况使得本发明的地坪材料具有较好的抗裂性能。
Composite inorganic terrace material
The invention discloses a composite inorganic terrace material, and relates to the technical field of concrete. The composite inorganic terrace material is prepared from the following components in percentage by mass: Portland cement, aggregate, blast furnace iron-smelting slag, anti-crack fibers, glass powder, an activating agent and a micro-expanding agent, the preparation method of the micro-expanding agent comprises the following steps: taking the lithium slag and the red mud, crushing the lithium slag and the red mud, adding water, uniformly stirring, then granulating, forming and sintering, and crushing a sintered product to obtain the micro-expanding agent. The composite inorganic terrace material disclosed by the invention has relatively high compressive strength and tensile strength, the concrete terrace disclosed by the invention has certain micro-expansion performance, and the micro-expansion rate of the terrace in the whole hardening period is relatively gentle. The terrace material disclosed by the invention has relatively good anti-cracking performance due to the conditions.
本发明公开了一种复合无机地坪材料,涉及混凝土技术领域。以质量百分比计,该复合无机地坪材料包括:硅酸盐水泥,集料,高炉冶铁矿渣,抗裂纤维,玻璃粉,激活剂,微膨胀剂;所述微膨胀剂的制备方法包括以下步骤:取锂渣、赤泥,对其粉碎后,加水搅拌均匀,随后对其造粒成型并烧结,对烧结产物进行粉碎即得。本发明的复合无机地坪材料,其具有较高的抗压强度以及较高的抗拉强度,且本发明的混凝土地坪具有一定的微膨胀性能,且在地坪的整个硬化周期内的微膨胀率相对平缓。这些情况使得本发明的地坪材料具有较好的抗裂性能。
Composite inorganic terrace material
一种复合无机地坪材料
LI ZIWEN (author) / YANG XINXIN (author) / QIU JIAOCHENG (author) / LEE DONG-WON (author)
2024-12-06
Patent
Electronic Resource
Chinese
IPC:
C04B
Kalk
,
LIME
Composite inorganic terrace material and preparation method thereof
European Patent Office | 2023
|European Patent Office | 2023
|European Patent Office | 2021
|Water-based inorganic mineral composite terrace coating and preparation method thereof
European Patent Office | 2020
|Concrete integral terrace composite material and construction method
European Patent Office | 2021
|