Blast furnace iron runner skimmer suitable for oscillating sintering and preparation method of blast furnace iron runner skimmer
The invention discloses a blast furnace iron runner skimmer suitable for oscillating sintering. The blast furnace iron runner skimmer comprises the following raw materials in percentage by mass: 18-25% of brown fused alumina aggregate with the particle size of 5-8mm; 18%-25% of brown fused alumina aggregate with the particle size of 3-5 mm; 10%-18% of brown fused alumina particles with the particle size of 1-3 mm; 8%-15% of compact corundum particles with the particle size of 0.074-1 mm; 5-9% of dense corundum fine powder with the particle size of less than or equal to 0.074 mm; 6%-12% of silicon carbide particles with the particle size of 0.074-1 mm; 6-12% of silicon carbide fine powder with a particle size of less than or equal to 0.074 mm; 0.5%-3% of spherical asphalt with the particle size of 0.1-0.8 mm; 3%-6% of submicron SiO2 micro powder with the particle size being smaller than or equal to 0.020 mm; 2%-7% of alpha-Al2O3 micro powder with the particle size of less than or equal to 0.020 0.5%-1.0% of boron oxide powder with the particle size being smaller than or equal to 0.044 mm; by redesigning the formula, the raw materials of the blast furnace iron runner skimmer are well matched with oscillation sintering, and the obtained product is good in high-temperature performance, high in volume stability, excellent in erosion resistance, long in service life and low in comprehensive operation and maintenance cost and has remarkable economic and social benefits.
本发明公开了一种适用于振荡烧结的高炉铁沟撇渣器,原料组成按质量百分数计如下:粒径为5~8mm的棕刚玉骨料18%~25%;粒径为3~5mm的棕刚玉骨料18%~25%;粒径为1~3mm的棕刚玉颗粒10%~18%;粒径为0.074~1mm的致密刚玉颗粒8%~15%;粒径为≤0.074mm的致密刚玉细粉5%~9%;粒径为0.074~1mm的碳化硅颗粒6%~12%;粒径为≤0.074mm的碳化硅细粉6%~12%;粒径为0.1~0.8mm的球状沥青0.5%~3%;粒径为≤0.020mm的亚微米SiO2微粉3%~6%;粒径为≤0.020mm的α‑Al2O3微粉2%~7%;粒径为≤0.044mm的氧化硼粉0.5%~1.0%;本发明通过对配方的重新设计使高炉铁沟撇渣器的原料与振荡烧结良好的适配,所得产品高温性能好、体积稳定性高、抗侵蚀性能优异、服役寿命长、综合运行维护成本低,具有显著的经济和社会效益。
Blast furnace iron runner skimmer suitable for oscillating sintering and preparation method of blast furnace iron runner skimmer
The invention discloses a blast furnace iron runner skimmer suitable for oscillating sintering. The blast furnace iron runner skimmer comprises the following raw materials in percentage by mass: 18-25% of brown fused alumina aggregate with the particle size of 5-8mm; 18%-25% of brown fused alumina aggregate with the particle size of 3-5 mm; 10%-18% of brown fused alumina particles with the particle size of 1-3 mm; 8%-15% of compact corundum particles with the particle size of 0.074-1 mm; 5-9% of dense corundum fine powder with the particle size of less than or equal to 0.074 mm; 6%-12% of silicon carbide particles with the particle size of 0.074-1 mm; 6-12% of silicon carbide fine powder with a particle size of less than or equal to 0.074 mm; 0.5%-3% of spherical asphalt with the particle size of 0.1-0.8 mm; 3%-6% of submicron SiO2 micro powder with the particle size being smaller than or equal to 0.020 mm; 2%-7% of alpha-Al2O3 micro powder with the particle size of less than or equal to 0.020 0.5%-1.0% of boron oxide powder with the particle size being smaller than or equal to 0.044 mm; by redesigning the formula, the raw materials of the blast furnace iron runner skimmer are well matched with oscillation sintering, and the obtained product is good in high-temperature performance, high in volume stability, excellent in erosion resistance, long in service life and low in comprehensive operation and maintenance cost and has remarkable economic and social benefits.
本发明公开了一种适用于振荡烧结的高炉铁沟撇渣器,原料组成按质量百分数计如下:粒径为5~8mm的棕刚玉骨料18%~25%;粒径为3~5mm的棕刚玉骨料18%~25%;粒径为1~3mm的棕刚玉颗粒10%~18%;粒径为0.074~1mm的致密刚玉颗粒8%~15%;粒径为≤0.074mm的致密刚玉细粉5%~9%;粒径为0.074~1mm的碳化硅颗粒6%~12%;粒径为≤0.074mm的碳化硅细粉6%~12%;粒径为0.1~0.8mm的球状沥青0.5%~3%;粒径为≤0.020mm的亚微米SiO2微粉3%~6%;粒径为≤0.020mm的α‑Al2O3微粉2%~7%;粒径为≤0.044mm的氧化硼粉0.5%~1.0%;本发明通过对配方的重新设计使高炉铁沟撇渣器的原料与振荡烧结良好的适配,所得产品高温性能好、体积稳定性高、抗侵蚀性能优异、服役寿命长、综合运行维护成本低,具有显著的经济和社会效益。
Blast furnace iron runner skimmer suitable for oscillating sintering and preparation method of blast furnace iron runner skimmer
适用于振荡烧结的高炉铁沟撇渣器及其制备方法
JU MAOQI (author) / CHENG SHUIMING (author) / XIA CHANGYONG (author) / WEI JIANXIU (author) / CAI WEI (author) / CHEN JINFENG (author) / SHAN JIANGBO (author)
2024-12-06
Patent
Electronic Resource
Chinese
Repair mold and repair method for blast furnace main iron runner skimmer
European Patent Office | 2023
|REFRACTORIES FOR RUNNER OF BLAST FURNACE AND RUNNER OF BLAST FURNACE
European Patent Office | 2016
|