A platform for research: civil engineering, architecture and urbanism
Hydrophilic self-cleaning archaized brick and preparation method thereof
The invention discloses a preparation method of a hydrophilic self-cleaning archaized brick. The preparation method comprises the following steps: A, preparing a hydrophilic frit; wherein the hydrophilic frit is prepared from the following raw materials in percentage by mass: 8 to 12 percent of lithium carbonate, 30 to 50 percent of calcined talc, 4 to 8 percent of zinc oxide, 25 to 35 percent of aluminum oxide, 6 to 12 percent of quartz and 3 to 7 percent of silicon carbide; b, preparing hydrophilic self-cleaning glaze; wherein the hydrophilic self-cleaning glaze is prepared from the following raw materials in percentage by mass: 85 to 95 percent of hydrophilic frit, 4 to 12 percent of kaolin and 1 to 3 percent of silicon carbide; and C, applying the hydrophilic self-cleaning glaze to the green body with the concave-convex effect, drying and calcining to obtain the hydrophilic self-cleaning archaized brick. The preparation method of the hydrophilic self-cleaning archaized brick, provided by the invention, is simple and high in operability, and the obtained hydrophilic self-cleaning archaized brick not only has excellent and lasting self-cleaning property, but also is beneficial to reducing the cost.
本发明公开了一种亲水自洁仿古砖的制备方法,包括以下步骤:A、准备亲水熔块;其中,按照质量百分比计算,所述亲水熔块包括以下原料:碳酸锂8~12%、烧滑石30~50%、氧化锌4~8%、三氧化二铝25~35%、石英6~12%和碳化硅3~7%;B、准备亲水自洁釉料;其中,按照质量百分比计算,所述亲水自洁釉料包括以下原料:亲水熔块85~95%、高岭土4~12%和碳化硅1~3%;C、将亲水自洁釉料布施于具有凹凸效果的坯体,干燥并煅烧得到亲水自洁仿古砖。本发明提出的一种亲水自洁仿古砖的制备方法,制备方法简单,操作性强,得到的亲水自洁仿古砖不仅具有优异且持久的自洁性,还有利于降低成本。
Hydrophilic self-cleaning archaized brick and preparation method thereof
The invention discloses a preparation method of a hydrophilic self-cleaning archaized brick. The preparation method comprises the following steps: A, preparing a hydrophilic frit; wherein the hydrophilic frit is prepared from the following raw materials in percentage by mass: 8 to 12 percent of lithium carbonate, 30 to 50 percent of calcined talc, 4 to 8 percent of zinc oxide, 25 to 35 percent of aluminum oxide, 6 to 12 percent of quartz and 3 to 7 percent of silicon carbide; b, preparing hydrophilic self-cleaning glaze; wherein the hydrophilic self-cleaning glaze is prepared from the following raw materials in percentage by mass: 85 to 95 percent of hydrophilic frit, 4 to 12 percent of kaolin and 1 to 3 percent of silicon carbide; and C, applying the hydrophilic self-cleaning glaze to the green body with the concave-convex effect, drying and calcining to obtain the hydrophilic self-cleaning archaized brick. The preparation method of the hydrophilic self-cleaning archaized brick, provided by the invention, is simple and high in operability, and the obtained hydrophilic self-cleaning archaized brick not only has excellent and lasting self-cleaning property, but also is beneficial to reducing the cost.
本发明公开了一种亲水自洁仿古砖的制备方法,包括以下步骤:A、准备亲水熔块;其中,按照质量百分比计算,所述亲水熔块包括以下原料:碳酸锂8~12%、烧滑石30~50%、氧化锌4~8%、三氧化二铝25~35%、石英6~12%和碳化硅3~7%;B、准备亲水自洁釉料;其中,按照质量百分比计算,所述亲水自洁釉料包括以下原料:亲水熔块85~95%、高岭土4~12%和碳化硅1~3%;C、将亲水自洁釉料布施于具有凹凸效果的坯体,干燥并煅烧得到亲水自洁仿古砖。本发明提出的一种亲水自洁仿古砖的制备方法,制备方法简单,操作性强,得到的亲水自洁仿古砖不仅具有优异且持久的自洁性,还有利于降低成本。
Hydrophilic self-cleaning archaized brick and preparation method thereof
一种亲水自洁仿古砖及其制备方法
LI SUBO (author) / LI ZHIHONG (author) / XU YU (author) / ZHONG BAOMIN (author) / LUO QIANG (author) / XIE SUI (author)
2024-12-13
Patent
Electronic Resource
Chinese
European Patent Office | 2024
|Archaized brick prepared from waste ceramic and preparation method of archaized brick
European Patent Office | 2023
|Antiskid antifouling archaized brick and preparation method thereof
European Patent Office | 2024
|