A platform for research: civil engineering, architecture and urbanism
METHOD FOR PRODUCING CALCINED PRODUCT CONTAINING ?-2CAO?SIO2
By preparing a raw material mixture comprising CaO raw material, SiO2 raw material and waste material, and having a content of Al2O3 after heating at 1000°C of 5.0 mass% or less, and calcining at a calcination temperature of 1350°C to 1600°C, it is possible to efficiently use waste materials as a part of raw materials, and to obtain a calcined product that comprises almost an equivalent amount of γ-2CaO·SiO2 as conventional can be obtained.
METHOD FOR PRODUCING CALCINED PRODUCT CONTAINING ?-2CAO?SIO2
By preparing a raw material mixture comprising CaO raw material, SiO2 raw material and waste material, and having a content of Al2O3 after heating at 1000°C of 5.0 mass% or less, and calcining at a calcination temperature of 1350°C to 1600°C, it is possible to efficiently use waste materials as a part of raw materials, and to obtain a calcined product that comprises almost an equivalent amount of γ-2CaO·SiO2 as conventional can be obtained.
METHOD FOR PRODUCING CALCINED PRODUCT CONTAINING ?-2CAO?SIO2
VERFAHREN ZUR HERSTELLUNG EINES KALZINIERTEN PRODUKTS MIT ?-2CAO?SIO2
PROCÉDÉ DE FABRICATION D'OBJET CUIT COMPRENANT UN ???????????
OTA MASAMI (author)
2025-02-19
Patent
Electronic Resource
English
METHOD FOR PRODUCING CALCINED PRODUCT CONTAINING γ-2CAO∙SIO2
European Patent Office | 2023
|METHOD FOR PRODUCING CALCINED PRODUCT CONTAINING γ-2CAO∙SIO2
European Patent Office | 2024
|METHOD FOR PRODUCING CALCINED PRODUCT COMPRISING .GAMMA.-2CAO SIO2
European Patent Office | 2023
|Properties of high-alumina cement containing 2CaO-Al2O3-SiO2
Tema Archive | 1999
|