METHOD FOR PRODUCING CERAMIC COMPOSITE AND CERAMIC COMPOSITE
PROBLEM TO BE SOLVED: To provide a method for producing a ceramic composite capable of suppressing the generation of warpage, peeling, cracking or the like in forming a ceramic composite by sintering each of ceramic parts comprising ceramic compositions having different sintering temperatures, and to provide a ceramic composite.SOLUTION: There is provided a method for producing a ceramic composite by integrally sintering each of ceramic parts comprising ceramic compositions having different sintering temperatures, which comprises: a step of heating a first ceramic part comprising a first ceramic composition to a sintering temperature of the first ceramic composition; and a step of forming a film of a second ceramic composition having a sintering temperature higher than the sintering temperature of the first ceramic composition by a sputtering method to form a second ceramic part on the first ceramic part comprising the first ceramic composition heated to the sintering temperature.SELECTED DRAWING: Figure 1
【課題】焼結温度の異なるセラミック組成物からなる夫々のセラミック部を焼成してセラミック複合体を形成する際に、反りや剥がれ、クラック等が生じることを抑制できるセラミック複合体の製造方法及びセラミック複合体を提供すること。【解決手段】本発明に係るセラミック複合体の製造方法は、焼結温度の異なるセラミック組成物からなる夫々のセラミック部を一括して焼成するセラミック複合体の製造方法であって、第1のセラミック組成物からなる第1のセラミック部を、第1のセラミック組成物の焼結温度まで加熱する工程と、焼結温度まで加熱された第1のセラミック組成物からなる第1のセラミック部上に、スパッタ法により第1のセラミック組成物よりも焼結温度の高い第2のセラミック組成物を成膜して第2のセラミック部を形成する工程と、を有することを特徴とする。【選択図】図1
METHOD FOR PRODUCING CERAMIC COMPOSITE AND CERAMIC COMPOSITE
PROBLEM TO BE SOLVED: To provide a method for producing a ceramic composite capable of suppressing the generation of warpage, peeling, cracking or the like in forming a ceramic composite by sintering each of ceramic parts comprising ceramic compositions having different sintering temperatures, and to provide a ceramic composite.SOLUTION: There is provided a method for producing a ceramic composite by integrally sintering each of ceramic parts comprising ceramic compositions having different sintering temperatures, which comprises: a step of heating a first ceramic part comprising a first ceramic composition to a sintering temperature of the first ceramic composition; and a step of forming a film of a second ceramic composition having a sintering temperature higher than the sintering temperature of the first ceramic composition by a sputtering method to form a second ceramic part on the first ceramic part comprising the first ceramic composition heated to the sintering temperature.SELECTED DRAWING: Figure 1
【課題】焼結温度の異なるセラミック組成物からなる夫々のセラミック部を焼成してセラミック複合体を形成する際に、反りや剥がれ、クラック等が生じることを抑制できるセラミック複合体の製造方法及びセラミック複合体を提供すること。【解決手段】本発明に係るセラミック複合体の製造方法は、焼結温度の異なるセラミック組成物からなる夫々のセラミック部を一括して焼成するセラミック複合体の製造方法であって、第1のセラミック組成物からなる第1のセラミック部を、第1のセラミック組成物の焼結温度まで加熱する工程と、焼結温度まで加熱された第1のセラミック組成物からなる第1のセラミック部上に、スパッタ法により第1のセラミック組成物よりも焼結温度の高い第2のセラミック組成物を成膜して第2のセラミック部を形成する工程と、を有することを特徴とする。【選択図】図1
METHOD FOR PRODUCING CERAMIC COMPOSITE AND CERAMIC COMPOSITE
セラミック複合体の製造方法、セラミック複合体
TAKAO YOSHIYA (author) / MURAMATSU MASAKI (author)
2016-02-01
Patent
Electronic Resource
Japanese
IPC:
C04B
Kalk
,
LIME
METHOD FOR PRODUCING CERAMIC COMPOSITE, AND CERAMIC COMPOSITE
European Patent Office | 2016
|METHOD OF PRODUCING COMPOSITE CERAMIC, METHOD OF REPAIRING CERAMIC, AND COMPOSITE CERAMIC
European Patent Office | 2024
|METHOD FOR PRODUCING CERAMIC MATRIX COMPOSITE AND CERAMIC MATRIX COMPOSITE
European Patent Office | 2020
|CERAMIC MATRIX COMPOSITE AND METHOD FOR PRODUCING CERAMIC MATRIX COMPOSITE
European Patent Office | 2024
|