A platform for research: civil engineering, architecture and urbanism
METHOD FOR BONDING CERAMIC MEMBER AND ALUMINUM MEMBER
PROBLEM TO BE SOLVED: To provide a method for easily bonding a ceramic member and an aluminum member to each other.SOLUTION: A method for bonding a ceramic member and an aluminum member to each other, includes the steps of: (a) preparing a ceramic member containing aluminum and/or silicon and an aluminum member; (b) installing a bonding material on at least one of the ceramic member and the aluminum member, wherein the bonding material comprises a siloxane polymer or a carbon powder-containing silica sol; (c) laminating the ceramic member and the aluminum member with the bonding material interposed therebetween to form an assembly; and (d) heating the assembly at a temperature of 430°C or more and less than 600°C in an inert gas atmosphere or in a vacuum atmosphere.SELECTED DRAWING: Figure 2
【課題】簡便にセラミックス部材とアルミニウム部材を接合する方法を提供する。【解決手段】セラミックス部材とアルミニウム部材とを接合する方法であって、(a)アルミニウムおよび/またはケイ素を含有するセラミックス部材、およびアルミニウム部材を準備するステップと、(b)前記セラミックス部材および前記アルミニウム部材の少なくとも一方に、接合材を設置するステップであって、前記接合材は、シロキサン系ポリマーまたは炭素粉末含有シリカゾルを含むステップと、(c)前記セラミックス部材と前記アルミニウム部材を、前記接合材を介在させた状態で積層し、組立体を構成するステップと、(d)前記組立体を、不活性ガス雰囲気下または真空雰囲気下、430℃以上、600℃未満の温度で加熱するステップと、を有する方法。【選択図】図2
METHOD FOR BONDING CERAMIC MEMBER AND ALUMINUM MEMBER
PROBLEM TO BE SOLVED: To provide a method for easily bonding a ceramic member and an aluminum member to each other.SOLUTION: A method for bonding a ceramic member and an aluminum member to each other, includes the steps of: (a) preparing a ceramic member containing aluminum and/or silicon and an aluminum member; (b) installing a bonding material on at least one of the ceramic member and the aluminum member, wherein the bonding material comprises a siloxane polymer or a carbon powder-containing silica sol; (c) laminating the ceramic member and the aluminum member with the bonding material interposed therebetween to form an assembly; and (d) heating the assembly at a temperature of 430°C or more and less than 600°C in an inert gas atmosphere or in a vacuum atmosphere.SELECTED DRAWING: Figure 2
【課題】簡便にセラミックス部材とアルミニウム部材を接合する方法を提供する。【解決手段】セラミックス部材とアルミニウム部材とを接合する方法であって、(a)アルミニウムおよび/またはケイ素を含有するセラミックス部材、およびアルミニウム部材を準備するステップと、(b)前記セラミックス部材および前記アルミニウム部材の少なくとも一方に、接合材を設置するステップであって、前記接合材は、シロキサン系ポリマーまたは炭素粉末含有シリカゾルを含むステップと、(c)前記セラミックス部材と前記アルミニウム部材を、前記接合材を介在させた状態で積層し、組立体を構成するステップと、(d)前記組立体を、不活性ガス雰囲気下または真空雰囲気下、430℃以上、600℃未満の温度で加熱するステップと、を有する方法。【選択図】図2
METHOD FOR BONDING CERAMIC MEMBER AND ALUMINUM MEMBER
セラミックス部材とアルミニウム部材とを接合する方法
KITA KENICHIRO (author) / KONDO NAOKI (author)
2016-04-14
Patent
Electronic Resource
Japanese
METHOD FOR JOINING CERAMIC MEMBER AND ALUMINUM MEMBER, AND JOINED BODY
European Patent Office | 2018
|MANUFACTURING METHOD FOR CERAMIC MEMBER AND CERAMIC MEMBER
European Patent Office | 2019
|Preparation method of aluminum nitride ceramic structural member
European Patent Office | 2022
|