A platform for research: civil engineering, architecture and urbanism
METHOD FOR FORMING JOINT GROOVE
PROBLEM TO BE SOLVED: To provide a method for forming a joint groove which can secure complexity and diversity of a design while increasing work efficiency and which can appropriately respond to the surface shape of various building frames to be constructed.SOLUTION: A plurality of joint groove forming components 12a are combined and are laid along a joint groove planned part 16a on the surface of a building frame 14, and a solidification material M is installed so as to cover the building frame 14, and the solidification material M is cured. Before the solidification material M is hardened, the plurality of joint groove forming components 12a are removed from the building frame 14, and the solidification material M installed in a non-joint groove planned part 16b which is a site partitioned by the plurality of joint groove forming components 12a is further cured and hardened.SELECTED DRAWING: Figure 1
【課題】作業効率を向上させるとともに、デザインの複雑性・多様性も確保し、また、施工する種々の躯体の表面形状にも適切に対応することができる目地溝の形成方法を提供すること。【解決手段】躯体14の表面に対して、複数の目地溝形成部品12aを組み合わせて目地溝予定部16aに沿って敷設し、躯体14を被覆するように固化材Mを打設し、固化材Mを養生し、 固化材Mの硬化前に、複数の目地溝形成部品12aを躯体14から取外し、複数の目地溝形成部品12aによって区画された部位の非目地溝予定部16bに打設された固化材Mをさらに養生・硬化させる。【選択図】 図1
METHOD FOR FORMING JOINT GROOVE
PROBLEM TO BE SOLVED: To provide a method for forming a joint groove which can secure complexity and diversity of a design while increasing work efficiency and which can appropriately respond to the surface shape of various building frames to be constructed.SOLUTION: A plurality of joint groove forming components 12a are combined and are laid along a joint groove planned part 16a on the surface of a building frame 14, and a solidification material M is installed so as to cover the building frame 14, and the solidification material M is cured. Before the solidification material M is hardened, the plurality of joint groove forming components 12a are removed from the building frame 14, and the solidification material M installed in a non-joint groove planned part 16b which is a site partitioned by the plurality of joint groove forming components 12a is further cured and hardened.SELECTED DRAWING: Figure 1
【課題】作業効率を向上させるとともに、デザインの複雑性・多様性も確保し、また、施工する種々の躯体の表面形状にも適切に対応することができる目地溝の形成方法を提供すること。【解決手段】躯体14の表面に対して、複数の目地溝形成部品12aを組み合わせて目地溝予定部16aに沿って敷設し、躯体14を被覆するように固化材Mを打設し、固化材Mを養生し、 固化材Mの硬化前に、複数の目地溝形成部品12aを躯体14から取外し、複数の目地溝形成部品12aによって区画された部位の非目地溝予定部16bに打設された固化材Mをさらに養生・硬化させる。【選択図】 図1
METHOD FOR FORMING JOINT GROOVE
目地溝の形成方法
MURAYAMA SATORU (author) / DOKI TAKESHI (author)
2016-07-11
Patent
Electronic Resource
Japanese
European Patent Office | 2016
|GROOVE FORMING IMPLEMENT AND ROLLING COMPACTION MACHINE EQUIPPED WITH GROOVE FORMING IMPLEMENT
European Patent Office | 2018
|