MANUFACTURING METHOD OF ROOM TEMPERATURE CONSTRUCTION TYPE ASPHALT MIXTURE AND ROOM TEMPERATURE CONSTRUCTION TYPE ASPHALT MIXTURE
PROBLEM TO BE SOLVED: To increase storage stability of a room temperature construction type asphalt mixture.SOLUTION: A mixing process for mixing an aggregate 2, a fiber material (vegetable fiber 6) and an alkaline powder 7 to form a first mixture body 11, a binder coating process for mixing a binder with the first mixture body 11 to from a second mixture body 12 coated with the binder, an additive coating process for mixing an additive 4a containing spindle oil and dimer acid with the second mixture body 12 to form a third mixture body 13 coated with the additive 4a and a finishing process for adding a hydration reaction material (gypsum 5a or iron steel slag or the like to the third mixture body 13 and mixing them.SELECTED DRAWING: Figure 2
【課題】常温施工型アスファルト合材の貯蔵安定性を高くする。【解決手段】骨材2と繊維質材料(植物繊維6)とアルカリ性粉末7を混合して第一混合体11を形成する混合工程と、第一混合体11にバインダを混合することでバインダが被覆された第二混合体12を形成するバインダ被覆工程と、第二混合体12にスピンドルオイルとダイマー酸を含んだ添加材4aを混合することで添加材4aが被覆された第三混合体13を形成する添加材被覆工程と、第三混合体13に水和反応材(石膏5aまたは鉄鋼スラグなど)を添加して混合する仕上工程と、を備えたことを特徴とする。【選択図】図2
MANUFACTURING METHOD OF ROOM TEMPERATURE CONSTRUCTION TYPE ASPHALT MIXTURE AND ROOM TEMPERATURE CONSTRUCTION TYPE ASPHALT MIXTURE
PROBLEM TO BE SOLVED: To increase storage stability of a room temperature construction type asphalt mixture.SOLUTION: A mixing process for mixing an aggregate 2, a fiber material (vegetable fiber 6) and an alkaline powder 7 to form a first mixture body 11, a binder coating process for mixing a binder with the first mixture body 11 to from a second mixture body 12 coated with the binder, an additive coating process for mixing an additive 4a containing spindle oil and dimer acid with the second mixture body 12 to form a third mixture body 13 coated with the additive 4a and a finishing process for adding a hydration reaction material (gypsum 5a or iron steel slag or the like to the third mixture body 13 and mixing them.SELECTED DRAWING: Figure 2
【課題】常温施工型アスファルト合材の貯蔵安定性を高くする。【解決手段】骨材2と繊維質材料(植物繊維6)とアルカリ性粉末7を混合して第一混合体11を形成する混合工程と、第一混合体11にバインダを混合することでバインダが被覆された第二混合体12を形成するバインダ被覆工程と、第二混合体12にスピンドルオイルとダイマー酸を含んだ添加材4aを混合することで添加材4aが被覆された第三混合体13を形成する添加材被覆工程と、第三混合体13に水和反応材(石膏5aまたは鉄鋼スラグなど)を添加して混合する仕上工程と、を備えたことを特徴とする。【選択図】図2
MANUFACTURING METHOD OF ROOM TEMPERATURE CONSTRUCTION TYPE ASPHALT MIXTURE AND ROOM TEMPERATURE CONSTRUCTION TYPE ASPHALT MIXTURE
常温施工型アスファルト合材の製造方法および常温施工型アスファルト合材
OTOMO NOBUYUKI (author) / KONNO MICHITO (author) / HIURA HIROSHI (author)
2017-04-13
Patent
Electronic Resource
Japanese
IPC:
C08L
COMPOSITIONS OF MACROMOLECULAR COMPOUNDS
,
Massen auf Basis makromolekularer Verbindungen
/
C08J
Verarbeitung
,
WORKING-UP
/
C08K
Verwendung von anorganischen oder nichtmakromolekularen organischen Stoffen als Zusatzstoffe
,
USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES AS COMPOUNDING INGREDIENTS
/
E01C
Bau von Straßen, Sportplätzen oder dgl., Decken dafür
,
CONSTRUCTION OF, OR SURFACES FOR, ROADS, SPORTS GROUNDS, OR THE LIKE
ROOM TEMPERATURE EMULSIFIED ASPHALT MIXTURE, AND METHOD FOR MANUFACTURING SAME
European Patent Office | 2023
|European Patent Office | 2019
|European Patent Office | 2021
|