ROCK WOOL AGGREGATE AND QUALITY EVALUATION METHOD OF ROCK WOOL AGGREGATE FOR ROCK WOOL SPRAYING METHOD
PROBLEM TO BE SOLVED: To provide a technology with improving jamming of rock wool in a hose during a spraying method of the rock wool, a technology with improving cotton waste and a rock wool aggregate less in jamming of the rock wool in the hose during the spraying method of the rock wool and less in cotton waste.MEANS: There is provided a rock wool aggregate having 20% or less of a reduction amount of 1 mm residual rate (R) at predetermined total rotation number (N) of 48000 to 50000 rotations to 1 mm residual rate (R) at predetermined total rotation number (N) of 9500 to 10500 rotations, calculated by a 1 mm residual rate measurement test with an input process, an agitation process, a volatilization process and a classification process. There is provided a quality evaluation method of the rock wool aggregate for rock wool spraying method having a process for selecting the rock wool aggregate having reduction amount of Rto R(selection process) of a specified value or less. The specified value is suitably 20% or less.SELECTED DRAWING: None
【課題】ロックウールの吹付け施工に際してホース内でのロックウールの詰まりが改善された技術、落ち綿が改善された技術を提案すること。ロックウールの吹付け施工に際してホース内でのロックウールの詰まりが少なく、且つ落ち綿が少ないロックウール集合体を提供すること。【手段】投入工程と、攪拌工程と、気化工程と、分級工程とを備える1mm残留率測定試験により求められる、所定の総回転数(NT)が9500〜10500回転のときの1mm残留率(R1)に対する、所定の総回転数(NT)が48000〜50000回転のときの1mm残留率(R2)の減少量が、20%以下であることを特徴とするロックウール集合体。R1に対するR2の減少量が、規定値以下であるロックウール集合体を選定する工程(選定工程)を具備することを特徴とするロックウール吹付け工法用ロックウール集合体の品質評価方法。規定値が20%以下であると好適である。【選択図】なし
ROCK WOOL AGGREGATE AND QUALITY EVALUATION METHOD OF ROCK WOOL AGGREGATE FOR ROCK WOOL SPRAYING METHOD
PROBLEM TO BE SOLVED: To provide a technology with improving jamming of rock wool in a hose during a spraying method of the rock wool, a technology with improving cotton waste and a rock wool aggregate less in jamming of the rock wool in the hose during the spraying method of the rock wool and less in cotton waste.MEANS: There is provided a rock wool aggregate having 20% or less of a reduction amount of 1 mm residual rate (R) at predetermined total rotation number (N) of 48000 to 50000 rotations to 1 mm residual rate (R) at predetermined total rotation number (N) of 9500 to 10500 rotations, calculated by a 1 mm residual rate measurement test with an input process, an agitation process, a volatilization process and a classification process. There is provided a quality evaluation method of the rock wool aggregate for rock wool spraying method having a process for selecting the rock wool aggregate having reduction amount of Rto R(selection process) of a specified value or less. The specified value is suitably 20% or less.SELECTED DRAWING: None
【課題】ロックウールの吹付け施工に際してホース内でのロックウールの詰まりが改善された技術、落ち綿が改善された技術を提案すること。ロックウールの吹付け施工に際してホース内でのロックウールの詰まりが少なく、且つ落ち綿が少ないロックウール集合体を提供すること。【手段】投入工程と、攪拌工程と、気化工程と、分級工程とを備える1mm残留率測定試験により求められる、所定の総回転数(NT)が9500〜10500回転のときの1mm残留率(R1)に対する、所定の総回転数(NT)が48000〜50000回転のときの1mm残留率(R2)の減少量が、20%以下であることを特徴とするロックウール集合体。R1に対するR2の減少量が、規定値以下であるロックウール集合体を選定する工程(選定工程)を具備することを特徴とするロックウール吹付け工法用ロックウール集合体の品質評価方法。規定値が20%以下であると好適である。【選択図】なし
ROCK WOOL AGGREGATE AND QUALITY EVALUATION METHOD OF ROCK WOOL AGGREGATE FOR ROCK WOOL SPRAYING METHOD
ロックウール集合体およびロックウール吹付け工法用ロックウール集合体の品質評価方法
KAMATA RYOTA (author) / TANIBE TORU (author)
2017-10-05
Patent
Electronic Resource
Japanese
European Patent Office | 2016
|METHOD FOR QUALITY EVALUATING OF ROCK WOOL FOR USE IN ROCK WOOL SPRAY AND ROCK WOOL SPRAY METHOD
European Patent Office | 2020
|Rock wool material, rock wool product and preparation method thereof
European Patent Office | 2024
|BINDER FOR ROCK WOOL COMPOSITION, AND ROCK WOOL COMPOSITION
European Patent Office | 2019
|