RECYCLED ORDINARY TEMPERATURE ASPHALT MIXTURE
To provide a recycled ordinary temperature asphalt mixture containing an asphalt recycled aggregate, capable of enhancing both of workability and strength.SOLUTION: A recycled ordinary temperature asphalt mixture contains a novel aggregate, an asphalt recycled aggregate, a molten slag and a binder. The content of the asphalt recycled aggregate is 30 wt.% to 80 w.% based on total weight of the novel aggregate, the asphalt recycled aggregate, and the molten slag. The content of the molten slag is 12.5 wt.% to 33.5 wt.% based on total weight of the novel aggregate, the asphalt recycled aggregate, and the molten slag. The total content of the asphalt recycled aggregate and the molten slag is 63.5 wt.% to 92.5 wt.% based on total weight of the novel aggregate, the asphalt recycled aggregate, and the molten slag.SELECTED DRAWING: None
【課題】アスファルト再生骨材を含む再生常温アスファルト混合物において、作業性及び強度の両方を向上させることができる再生常温アスファルト混合物を提供する。【解決手段】実施形態に係る再生常温アスファルト混合物は、新規骨材、アスファルト再生骨材、溶融スラグ及びバインダを含有する。アスファルト再生骨材の含有量は、新規骨材、アスファルト再生骨材及び溶融スラグの合計重量に対して30重量%以上80重量%以下である。溶融スラグの含有量は、新規骨材、アスファルト再生骨材及び溶融スラグの合計重量に対して12.5重量%以上33.5重量%以下である。アスファルト再生骨材及び溶融スラグの合計含有量は、新規骨材、アスファルト再生骨材及び溶融スラグの合計重量に対して63.5重量%以上92.5重量%以下である。【選択図】なし
RECYCLED ORDINARY TEMPERATURE ASPHALT MIXTURE
To provide a recycled ordinary temperature asphalt mixture containing an asphalt recycled aggregate, capable of enhancing both of workability and strength.SOLUTION: A recycled ordinary temperature asphalt mixture contains a novel aggregate, an asphalt recycled aggregate, a molten slag and a binder. The content of the asphalt recycled aggregate is 30 wt.% to 80 w.% based on total weight of the novel aggregate, the asphalt recycled aggregate, and the molten slag. The content of the molten slag is 12.5 wt.% to 33.5 wt.% based on total weight of the novel aggregate, the asphalt recycled aggregate, and the molten slag. The total content of the asphalt recycled aggregate and the molten slag is 63.5 wt.% to 92.5 wt.% based on total weight of the novel aggregate, the asphalt recycled aggregate, and the molten slag.SELECTED DRAWING: None
【課題】アスファルト再生骨材を含む再生常温アスファルト混合物において、作業性及び強度の両方を向上させることができる再生常温アスファルト混合物を提供する。【解決手段】実施形態に係る再生常温アスファルト混合物は、新規骨材、アスファルト再生骨材、溶融スラグ及びバインダを含有する。アスファルト再生骨材の含有量は、新規骨材、アスファルト再生骨材及び溶融スラグの合計重量に対して30重量%以上80重量%以下である。溶融スラグの含有量は、新規骨材、アスファルト再生骨材及び溶融スラグの合計重量に対して12.5重量%以上33.5重量%以下である。アスファルト再生骨材及び溶融スラグの合計含有量は、新規骨材、アスファルト再生骨材及び溶融スラグの合計重量に対して63.5重量%以上92.5重量%以下である。【選択図】なし
RECYCLED ORDINARY TEMPERATURE ASPHALT MIXTURE
再生常温アスファルト混合物
CHINOKAN EMI (author) / GENTO TSUTOMU (author) / KOSHIBA TOMOHIRO (author)
2019-02-21
Patent
Electronic Resource
Japanese
European Patent Office | 2019
|European Patent Office | 2024
|RECYCLED ASPHALT MIXTURE MANUFACTURING METHOD AND RECYCLED ASPHALT MIXTURE
European Patent Office | 2020
|