GROUND IMPROVER COMPOSITION AND USE THEREOF
To provide a ground improver composition capable of providing excellent ground durability while suppressing corrosion of a metal structure, and to provide a use thereof.SOLUTION: The ground improver composition contains (A) a metal (meth)acrylate, (B) a polyvalent metal salt compound other than the metal (meth)acrylate, (C) an α-hydroxy acid or a salt thereof, (D) a basic compound, (E) a polymerization initiator, and (F) water. The total amount of the component (A) and the component (B) is 2.0-15 mass%. The molar ratio of the component (C) to a central metal of the component (B) is 0.1-1.0. The ground improver composition has a pH of 4.0-9.0. Preferably, the component (B) is an aluminum salt compound, and the component (C) is a C2-8 α-hydroxy acid or a salt thereof.SELECTED DRAWING: None
【課題】金属製構造物の腐食を抑制しつつ優れた地盤耐久性を提供できる地盤改良剤組成物及びその利用を提供する。【解決手段】(A)(メタ)アクリル酸金属塩と、(B)前記(メタ)アクリル酸金属塩以外の多価金属塩化合物と、(C)αヒドロキシ酸又はその塩と、(D)塩基性化合物と、(E)重合開始剤と、(F)水と、を含み、前記(A)及び前記(B)成分の総量が2.0〜15質量%であり、前記(B)成分の中心金属に対する前記(C)成分のモル比が0.1〜1.0であり、pHが4.0〜9.0とする地盤改良剤組成物。好ましくは、(B)成分がアルミニウム塩化合物であり、(C)成分が炭素数2〜8のα−ヒドロキシ酸又はその塩である、地盤改良剤組成物。【選択図】なし
GROUND IMPROVER COMPOSITION AND USE THEREOF
To provide a ground improver composition capable of providing excellent ground durability while suppressing corrosion of a metal structure, and to provide a use thereof.SOLUTION: The ground improver composition contains (A) a metal (meth)acrylate, (B) a polyvalent metal salt compound other than the metal (meth)acrylate, (C) an α-hydroxy acid or a salt thereof, (D) a basic compound, (E) a polymerization initiator, and (F) water. The total amount of the component (A) and the component (B) is 2.0-15 mass%. The molar ratio of the component (C) to a central metal of the component (B) is 0.1-1.0. The ground improver composition has a pH of 4.0-9.0. Preferably, the component (B) is an aluminum salt compound, and the component (C) is a C2-8 α-hydroxy acid or a salt thereof.SELECTED DRAWING: None
【課題】金属製構造物の腐食を抑制しつつ優れた地盤耐久性を提供できる地盤改良剤組成物及びその利用を提供する。【解決手段】(A)(メタ)アクリル酸金属塩と、(B)前記(メタ)アクリル酸金属塩以外の多価金属塩化合物と、(C)αヒドロキシ酸又はその塩と、(D)塩基性化合物と、(E)重合開始剤と、(F)水と、を含み、前記(A)及び前記(B)成分の総量が2.0〜15質量%であり、前記(B)成分の中心金属に対する前記(C)成分のモル比が0.1〜1.0であり、pHが4.0〜9.0とする地盤改良剤組成物。好ましくは、(B)成分がアルミニウム塩化合物であり、(C)成分が炭素数2〜8のα−ヒドロキシ酸又はその塩である、地盤改良剤組成物。【選択図】なし
GROUND IMPROVER COMPOSITION AND USE THEREOF
地盤改良剤組成物及びその利用