COATING LIQUID COMPOSITION FOR DEPOSITING PIEZOELECTRIC FILM, METHOD FOR MANUFACTURING THE SAME, ORIENTED PIEZOELECTRIC FILM AND LIQUID EJECTION HEAD
To provide a coating liquid composition capable of obtaining a NNBT film preferentially oriented on a specific crystal plane and having high liquid stability.SOLUTION: Used is a sodium niobate-barium titanate based coating liquid composition comprising (a) a sol-gel raw material including (i) a niobium component, such as niobium alkoxide, (ii) a sodium component, such as sodium alkoxide, (iii) a titanium component, such as titanium alkoxide and (iv) a barium component, such as barium alkoxide and (b) a compound including at least one kind selected from a group consisting of a β-ketoester compound and a β-diketone compound.SELECTED DRAWING: Figure 1
【課題】特定の結晶面に優先配向したNNBT膜が得られ、かつ液安定性が高い塗工液組成物を提供する。【解決手段】(a)(i)ニオブアルコキシド等のニオブ成分と、(ii)ナトリウムアルコキシド等のナトリウム成分と、(iii)チタンアルコキシド等のチタン成分と、(iv)バリウムアルコキシド等のバリウム成分と、を含むゾル−ゲル原料、および(b)β−ケトエステル化合物およびβ−ジケトン化合物からなる群より選択される少なくとも1種を含む化合物、を含むことを特徴とする、ニオブ酸ナトリウム−チタン酸バリウム系塗工液組成物を用いる。【選択図】図1
COATING LIQUID COMPOSITION FOR DEPOSITING PIEZOELECTRIC FILM, METHOD FOR MANUFACTURING THE SAME, ORIENTED PIEZOELECTRIC FILM AND LIQUID EJECTION HEAD
To provide a coating liquid composition capable of obtaining a NNBT film preferentially oriented on a specific crystal plane and having high liquid stability.SOLUTION: Used is a sodium niobate-barium titanate based coating liquid composition comprising (a) a sol-gel raw material including (i) a niobium component, such as niobium alkoxide, (ii) a sodium component, such as sodium alkoxide, (iii) a titanium component, such as titanium alkoxide and (iv) a barium component, such as barium alkoxide and (b) a compound including at least one kind selected from a group consisting of a β-ketoester compound and a β-diketone compound.SELECTED DRAWING: Figure 1
【課題】特定の結晶面に優先配向したNNBT膜が得られ、かつ液安定性が高い塗工液組成物を提供する。【解決手段】(a)(i)ニオブアルコキシド等のニオブ成分と、(ii)ナトリウムアルコキシド等のナトリウム成分と、(iii)チタンアルコキシド等のチタン成分と、(iv)バリウムアルコキシド等のバリウム成分と、を含むゾル−ゲル原料、および(b)β−ケトエステル化合物およびβ−ジケトン化合物からなる群より選択される少なくとも1種を含む化合物、を含むことを特徴とする、ニオブ酸ナトリウム−チタン酸バリウム系塗工液組成物を用いる。【選択図】図1
COATING LIQUID COMPOSITION FOR DEPOSITING PIEZOELECTRIC FILM, METHOD FOR MANUFACTURING THE SAME, ORIENTED PIEZOELECTRIC FILM AND LIQUID EJECTION HEAD
圧電体膜形成用塗工液組成物、その製造方法、配向性圧電体膜、並びに、液体吐出ヘッド
KOTANI YOSHINORI (author) / KOBAYASHI MOTOKAZU (author) / OHASHI RYOTA (author) / NAKASU MINAKO (author)
2020-04-09
Patent
Electronic Resource
Japanese
European Patent Office | 2022
|ORIENTED PIEZOELECTRIC FILM, METHOD OF MANUFACTURING THE SAME, AND LIQUID EJECTION HEAD
European Patent Office | 2019
|European Patent Office | 2019
|European Patent Office | 2019
|European Patent Office | 2020
|