CURABLE COMPOSITION
To provide a method for producing a curable composition that can give a cured body of high strength at a high curing rate.SOLUTION: A curable composition contains a cyclic carbonate having a hydroxy group, calcium hydroxide, and aggregate. Within 1.5 hours just after mixing the cyclic carbonate with the calcium hydroxide, the compression strength of the curable composition becomes 30 N/mm2 or more.SELECTED DRAWING: None
【課題】硬化速度が大きく、かつ高強度の硬化体を得ることができる硬化性組成物を提供すること。【解決手段】ヒドロキシ基を有する環状カーボネートと、水酸化カルシウムと、骨材とを含む硬化性組成物であって、前記環状カーボネートと前記水酸化カルシウムとを混合した直後から1.5時間以内に、前記硬化性組成物の圧縮強度が30N/mm2以上となる、硬化性組成物。【選択図】なし
CURABLE COMPOSITION
To provide a method for producing a curable composition that can give a cured body of high strength at a high curing rate.SOLUTION: A curable composition contains a cyclic carbonate having a hydroxy group, calcium hydroxide, and aggregate. Within 1.5 hours just after mixing the cyclic carbonate with the calcium hydroxide, the compression strength of the curable composition becomes 30 N/mm2 or more.SELECTED DRAWING: None
【課題】硬化速度が大きく、かつ高強度の硬化体を得ることができる硬化性組成物を提供すること。【解決手段】ヒドロキシ基を有する環状カーボネートと、水酸化カルシウムと、骨材とを含む硬化性組成物であって、前記環状カーボネートと前記水酸化カルシウムとを混合した直後から1.5時間以内に、前記硬化性組成物の圧縮強度が30N/mm2以上となる、硬化性組成物。【選択図】なし
CURABLE COMPOSITION
硬化性組成物
TASAKA YUKIO (author) / MIURA DAISUKE (author) / FUKUSHIMA YUTA (author)
2022-10-03
Patent
Electronic Resource
Japanese
IPC:
C04B
Kalk
,
LIME