FIREPROOF COATING REPAIR MATERIAL
To provide a water-kneading repair material for a sprayed rock wool fireproof coating material, wherein the water-kneading fireproof coating repair material has excellent adhesion and workability, and also excellent fireproof coating property.SOLUTION: A water-kneading fireproof coating repair material includes 55-65 pts.mass of rock wool, 35-45 pts.mass of cement, 0.2-2.2 pts.mass of an anionic surfactant, and 0.1-3 pts.mass of a thickener.SELECTED DRAWING: None
【課題】吹付けロックウール耐火被覆材に対する水練り補修材であって、付着性、作業性に優れ、かつ耐火被覆性にも優れる水練り耐火被覆補修材を提供すること。【解決手段】ロックウール55~65質量部、セメント35~45質量部、アニオン性界面活性剤0.2~2.2質量部及び増粘剤0.1~3質量部を含有する水練り耐火被覆補修材。【選択図】なし
FIREPROOF COATING REPAIR MATERIAL
To provide a water-kneading repair material for a sprayed rock wool fireproof coating material, wherein the water-kneading fireproof coating repair material has excellent adhesion and workability, and also excellent fireproof coating property.SOLUTION: A water-kneading fireproof coating repair material includes 55-65 pts.mass of rock wool, 35-45 pts.mass of cement, 0.2-2.2 pts.mass of an anionic surfactant, and 0.1-3 pts.mass of a thickener.SELECTED DRAWING: None
【課題】吹付けロックウール耐火被覆材に対する水練り補修材であって、付着性、作業性に優れ、かつ耐火被覆性にも優れる水練り耐火被覆補修材を提供すること。【解決手段】ロックウール55~65質量部、セメント35~45質量部、アニオン性界面活性剤0.2~2.2質量部及び増粘剤0.1~3質量部を含有する水練り耐火被覆補修材。【選択図】なし
FIREPROOF COATING REPAIR MATERIAL
耐火被覆補修材
FUJI MASAFUMI (author) / YAMAMOTO CHINATSU (author) / SHINAGAWA HAJIME (author) / SAKUMA TOMOHIRO (author)
2022-10-13
Patent
Electronic Resource
Japanese
FIREPROOF COATING METHOD, STEEL BEAM, AND FIREPROOF COATING MATERIAL
European Patent Office | 2022
|FIREPROOF COATING MATERIAL SPRAYING METHOD AND FIREPROOF COATING MATERIAL SPRAYING SYSTEM
European Patent Office | 2021
|FIREPROOF COATING MATERIAL AND ANTIOXIDATION COATING MATERIAL
European Patent Office | 2021
|FIREPROOF MEMBER AND FIREPROOF COATING MATERIAL INCLUDING SAME
European Patent Office | 2024
|European Patent Office | 2021
|