MANUFACTURING METHOD OF COMPOSITE OPTICAL CERAMICS ELEMENT
To provide a method of manufacturing a composite optical ceramic element in which degradation of the optical properties may be suppressed.SOLUTION: A manufacturing method includes a first step of preparing a first powder P1 for a first ceramics part 10 and a second powder P2 for a second ceramics part 20, containing a first transition element, a second step of arranging the first powder P1 in a first region R1 and the second powder P2 in a second region R2 to make contact between the first powder P1 and the second powder P2 to form a contact state, and a third step of forming the first ceramics part 10 and the second ceramics part 20 from each of the first and second powders P1 and P2 to form a composite PB by sintering the first and second powders P1 and P2 while maintaining the contact state.SELECTED DRAWING: Figure 4
【課題】光学特性の劣化を抑制可能な複合光学セラミックス素子の製造方法を提供する。【解決手段】この製造方法は、第1遷移元素を含み、第1セラミックス部10のための第1粉末P1と、第2セラミックス部20のための第2粉末P2と、を用意する第1工程と、第1領域R1に第1粉末P1を配置すると共に第2領域R2に第2粉末P2を配置し、第1粉末P1と第2粉末P2とを接触させて接触状態を形成する第2工程と、接触状態を維持しつつ第1粉末P1及び第2粉末P2を焼結することにより、第1粉末P1及び第2粉末P2のそれぞれから第1セラミックス部10及び第2セラミックス部20のそれぞれを形成し、複合体PBを形成する第3工程と、を備える。【選択図】図4
MANUFACTURING METHOD OF COMPOSITE OPTICAL CERAMICS ELEMENT
To provide a method of manufacturing a composite optical ceramic element in which degradation of the optical properties may be suppressed.SOLUTION: A manufacturing method includes a first step of preparing a first powder P1 for a first ceramics part 10 and a second powder P2 for a second ceramics part 20, containing a first transition element, a second step of arranging the first powder P1 in a first region R1 and the second powder P2 in a second region R2 to make contact between the first powder P1 and the second powder P2 to form a contact state, and a third step of forming the first ceramics part 10 and the second ceramics part 20 from each of the first and second powders P1 and P2 to form a composite PB by sintering the first and second powders P1 and P2 while maintaining the contact state.SELECTED DRAWING: Figure 4
【課題】光学特性の劣化を抑制可能な複合光学セラミックス素子の製造方法を提供する。【解決手段】この製造方法は、第1遷移元素を含み、第1セラミックス部10のための第1粉末P1と、第2セラミックス部20のための第2粉末P2と、を用意する第1工程と、第1領域R1に第1粉末P1を配置すると共に第2領域R2に第2粉末P2を配置し、第1粉末P1と第2粉末P2とを接触させて接触状態を形成する第2工程と、接触状態を維持しつつ第1粉末P1及び第2粉末P2を焼結することにより、第1粉末P1及び第2粉末P2のそれぞれから第1セラミックス部10及び第2セラミックス部20のそれぞれを形成し、複合体PBを形成する第3工程と、を備える。【選択図】図4
MANUFACTURING METHOD OF COMPOSITE OPTICAL CERAMICS ELEMENT
複合光学セラミックス素子の製造方法
SO JUSEI (author) / KATO YOSHINORI (author) / FUJITA TAKAYOSHI (author) / KIMURA HIROTO (author)
2023-05-19
Patent
Electronic Resource
Japanese
Method for manufacturing composite optical ceramic element
European Patent Office | 2024
|European Patent Office | 2017
|European Patent Office | 2017
European Patent Office | 2020
|METHOD FOR MANUFACTURING OPTICAL ELEMENT AND OPTICAL ELEMENT
European Patent Office | 2023
|