A platform for research: civil engineering, architecture and urbanism
Warm modified asphalts and warm modified asphaltconcretes
The present invention provides warm modified asphalt, which comprises: 100 wt% of an asphalt mixture comprising 60 to 95 wt% of asphalt for road pavement, 4.8 to 35 wt% of an unhardened rubber powder and 0.2 to 5 wt% of polyphosphoric acid; 0.5 to 15 wt% of one or at least two selected from a group consisting of styrene butadiene styrene (SBS), styrene butadiene rubber (SBR) and styrene ethylene butadiene styrene (SEBS) having a butadiene content of 30 wt% or more; 0.05 to 5 wt% of a coupling agent; 2 to 15 wt% of semi-drying or drying oil having an iodine value of 100 or more; and 0.05 to 2 wt% of a solidifying agent. The warm modified asphalt and the warm modified asphalt concrete according to the present invention can reduce harmful gas discharged during production and construction, thereby reducing the discomfort of workers and passengers.
본 발명은 도로포장용 아스팔트 60 ~ 95 중량%, 탈경화 고무분말 4.8 ~ 35 중량%, 폴리인산 0.2 ~ 5 중량%가 혼합된 아스팔트 혼합물 100 중량부; 부타디엔 함량이 30 중량% 이상인 스티렌부타디엔스트렌(SBS), 스티렌뷰타디엔고무(SBR) 및 스티렌에틸렌뷰타디엔스티렌(SEBS) 중에서 선택되는 어느 하나 또는 2종 이상의 혼합된 고탄성 고분자 0.5 ~ 15 중량부; 커플링제 0.05 ~ 5 중량부; 100 이상의 아이오딘 가(Iodine value)를 갖는 반건성유 또는 건성유 2 ~ 15 중량부; 고화제 0.05 ~ 2 중량부;를 포함하는 것을 특징으로 하는 중온 개질 아스팔트를 제공한다.
Warm modified asphalts and warm modified asphaltconcretes
The present invention provides warm modified asphalt, which comprises: 100 wt% of an asphalt mixture comprising 60 to 95 wt% of asphalt for road pavement, 4.8 to 35 wt% of an unhardened rubber powder and 0.2 to 5 wt% of polyphosphoric acid; 0.5 to 15 wt% of one or at least two selected from a group consisting of styrene butadiene styrene (SBS), styrene butadiene rubber (SBR) and styrene ethylene butadiene styrene (SEBS) having a butadiene content of 30 wt% or more; 0.05 to 5 wt% of a coupling agent; 2 to 15 wt% of semi-drying or drying oil having an iodine value of 100 or more; and 0.05 to 2 wt% of a solidifying agent. The warm modified asphalt and the warm modified asphalt concrete according to the present invention can reduce harmful gas discharged during production and construction, thereby reducing the discomfort of workers and passengers.
본 발명은 도로포장용 아스팔트 60 ~ 95 중량%, 탈경화 고무분말 4.8 ~ 35 중량%, 폴리인산 0.2 ~ 5 중량%가 혼합된 아스팔트 혼합물 100 중량부; 부타디엔 함량이 30 중량% 이상인 스티렌부타디엔스트렌(SBS), 스티렌뷰타디엔고무(SBR) 및 스티렌에틸렌뷰타디엔스티렌(SEBS) 중에서 선택되는 어느 하나 또는 2종 이상의 혼합된 고탄성 고분자 0.5 ~ 15 중량부; 커플링제 0.05 ~ 5 중량부; 100 이상의 아이오딘 가(Iodine value)를 갖는 반건성유 또는 건성유 2 ~ 15 중량부; 고화제 0.05 ~ 2 중량부;를 포함하는 것을 특징으로 하는 중온 개질 아스팔트를 제공한다.
Warm modified asphalts and warm modified asphaltconcretes
중온 개질 아스팔트 및 중온 개질 아스팔트 콘크리트