The present invention relates to an ascon composition with an improved low noise function, and an ascon construction method using the same. The ascon composition with an improved low noise function of the present invention comprises: a bottom layer part (10) including a composition of 75 to 80 wt% of an aggregate having 20 to 25 mm of a particle diameter, 15 to 21 wt% of an aggregate having 10 to 15 mm of a particle diameter, 2 to 5 wt% of limestone powder, and 1 to 3 wt% of a mineral fiber filler; a first middle layer part (20); a second middle layer part (30); and a top layer part (40) including a composition of 50 to 56 wt% of an aggregate having 3 to 6 mm of a particle diameter, 7 to 14 wt% of an aggregate having 1 to 1.5 mm of a particle diameter, 21 to 24 wt% of asphalt, 1 to 3 wt% of an asphalt modifier, 3 to 6 wt% of an anti-stripping agent, 2 to 5 wt% of a high elastic resin, and 1 to 3 wt% of a middle temperature additive.
본 발명은 저소음 기능이 향상된 아스콘 조성물 및 그 조성물을 이용한 아스콘 시공방법에 관한 것으로 아스콘을 형성하는 두께층을 최소화하면서도 저소음 기능이 향상되도록 하기 위하여, 입경 20∼25㎜의 골재 75∼80중량%, 입경 10∼15㎜의 골재 15∼21중량%, 석회석 분말 2∼5중량%, 미네랄섬유 충진제 1∼3중량%의 조성물로 된 하단층부(10); 입경 12∼17㎜의 골재 73∼81중량%, 입경 8∼10㎜의 골재 10∼15중량%, 석회석 분말 2∼5중량%, 미네랄섬유 충진제 1∼3중량%, 아스팔트 3∼5중량%, 아스팔트 개질제 0.5∼1중량%, 중온 첨가제 1∼3중량%의 조성물로 된 제1중단층부(20); 고탄성수지 78∼83중량%, 플라스틱 공중합체 11∼15중량%, 미네랄섬유 충진제 2∼5중량%, 박리 방지제 2∼5중량%, 분산제 1∼3중량%의 조성물로 된 제2중단층부(30); 입경 3∼6㎜의 골재 50∼56중량%, 입경 1∼1.5㎜의 골재 7∼14중량%, 아스팔트 21∼24중량%, 아스팔트 개질제 1∼3중량%, 박리 방지제 3∼6중량%, 고탄성수지 2∼5중량%, 중온 첨가제 1∼3중량%의 조성물로 된 상단층부(40);를 포함하여 이루어지며, 상기 제2중단층부(30)에서 플라스틱 공중합체는 폴리에틸렌, 폴리부텐 중 선택되는 적어도 하나 이상과, 폴리에틸렌이민, 폴리페닐렌 설파이드, 폴리벤지미다졸 중 선택되는 적어도 하나 이상이 공중합된 공중합체로 형성되고, 상기 하단층부(10), 제1중단층부(20), 제2중단층부(30), 상단층부(40)는 5:1.5:2:1.5의 두께 비율로 적층 형성되며, 상기 상단층부(40) 100중량부에 대해 고무칩 1∼3중량부가 더 포함되고, 상기 하단층부(10) 100중량부에 대해 규산칼륨 0.5∼1.5중량%가 더 포함되어 구성되는 것을 특징으로 한다.
Constructing method of ascon using ascon mixture
The present invention relates to an ascon composition with an improved low noise function, and an ascon construction method using the same. The ascon composition with an improved low noise function of the present invention comprises: a bottom layer part (10) including a composition of 75 to 80 wt% of an aggregate having 20 to 25 mm of a particle diameter, 15 to 21 wt% of an aggregate having 10 to 15 mm of a particle diameter, 2 to 5 wt% of limestone powder, and 1 to 3 wt% of a mineral fiber filler; a first middle layer part (20); a second middle layer part (30); and a top layer part (40) including a composition of 50 to 56 wt% of an aggregate having 3 to 6 mm of a particle diameter, 7 to 14 wt% of an aggregate having 1 to 1.5 mm of a particle diameter, 21 to 24 wt% of asphalt, 1 to 3 wt% of an asphalt modifier, 3 to 6 wt% of an anti-stripping agent, 2 to 5 wt% of a high elastic resin, and 1 to 3 wt% of a middle temperature additive.
본 발명은 저소음 기능이 향상된 아스콘 조성물 및 그 조성물을 이용한 아스콘 시공방법에 관한 것으로 아스콘을 형성하는 두께층을 최소화하면서도 저소음 기능이 향상되도록 하기 위하여, 입경 20∼25㎜의 골재 75∼80중량%, 입경 10∼15㎜의 골재 15∼21중량%, 석회석 분말 2∼5중량%, 미네랄섬유 충진제 1∼3중량%의 조성물로 된 하단층부(10); 입경 12∼17㎜의 골재 73∼81중량%, 입경 8∼10㎜의 골재 10∼15중량%, 석회석 분말 2∼5중량%, 미네랄섬유 충진제 1∼3중량%, 아스팔트 3∼5중량%, 아스팔트 개질제 0.5∼1중량%, 중온 첨가제 1∼3중량%의 조성물로 된 제1중단층부(20); 고탄성수지 78∼83중량%, 플라스틱 공중합체 11∼15중량%, 미네랄섬유 충진제 2∼5중량%, 박리 방지제 2∼5중량%, 분산제 1∼3중량%의 조성물로 된 제2중단층부(30); 입경 3∼6㎜의 골재 50∼56중량%, 입경 1∼1.5㎜의 골재 7∼14중량%, 아스팔트 21∼24중량%, 아스팔트 개질제 1∼3중량%, 박리 방지제 3∼6중량%, 고탄성수지 2∼5중량%, 중온 첨가제 1∼3중량%의 조성물로 된 상단층부(40);를 포함하여 이루어지며, 상기 제2중단층부(30)에서 플라스틱 공중합체는 폴리에틸렌, 폴리부텐 중 선택되는 적어도 하나 이상과, 폴리에틸렌이민, 폴리페닐렌 설파이드, 폴리벤지미다졸 중 선택되는 적어도 하나 이상이 공중합된 공중합체로 형성되고, 상기 하단층부(10), 제1중단층부(20), 제2중단층부(30), 상단층부(40)는 5:1.5:2:1.5의 두께 비율로 적층 형성되며, 상기 상단층부(40) 100중량부에 대해 고무칩 1∼3중량부가 더 포함되고, 상기 하단층부(10) 100중량부에 대해 규산칼륨 0.5∼1.5중량%가 더 포함되어 구성되는 것을 특징으로 한다.
Constructing method of ascon using ascon mixture
저소음 기능이 향상된 아스콘 조성물 및 그 조성물을 이용한 아스콘 시공방법