A platform for research: civil engineering, architecture and urbanism
Concrete reinforcement materials including adhesives for wet face and early hardening section repair mortar and concrete repair and reinforcement method
The present invention relates to a concrete repair/reinforcement material composition including an adhesive for a wet surface and an early hardening section repair mortar, and a concrete repair/reinforcement method using the concrete repair/reinforcement material composition, capable of ensuring stability of a worker and improving economic efficiency. According to the present invention, the concrete repair/reinforcement material composition including the adhesive for the wet surface and the early hardening section repair mortar includes: an adhesive composition including a water-soluble acryl polymer, a surfactant, a stabilizer, an antifoaming agent, a moisturizing agent, a film forming agent, and water; and a section repair mortar composition including a cement mixture, a fast hardening material, gypsum, an inorganic expanding material, a metal-based expanding material, hydrophilic nylon-based microfibers, an organic/inorganic composite waterproofing agent, a fluidizing agent, an air-entraining agent, a thixotropic agent, a curing agent, a retarder, and silica sand.
본 발명의 콘크리트 보수보강재료 조성물은, 습윤면용 접착제와 조기경화성 단면보수 모르타르를 구비하는 콘크리트 보수보강재료 조성물 34.0 ~ 45.0중량부, 계면활성제 0.1 ~ 0.2 중량부, 안정제 7.0 ~ 9.3 중량부, 소포제 0.03 ~ 0.06 중량부, 보습제 1.8 ~ 2.7 중량부, 조막제 3.07 ~ 4.74 중량부, 물은 38 ~ 54 중량부로 이루어지는 접착제 조성물; 및 시멘트 혼합물 19 ~ 24 중량부, 속경재 5 ~ 10 중량부, 석고 3 ~ 6.3 중량부, 무기팽창재 1 ~ 3중량부, 금속계 팽창재 0.02 ~ 0.05중량부, 친수성 나일론계 마이크로 섬유 0.1 ~ 0.2 중량부, 유무기 복합 방수제 3.2 ~ 6 중량부, 유동화제 0.1 ~ 0.4 중량부, 공기연행제 0.004 ~ 0.01 중량부, 요변제 0.44 ~ 1.54 중량부, 경화제 0.09 ~ 0.2 중량부, 지연제 0.046 ~ 0.3 중량부, 규사 48 ~ 68중량부로 이루어지는 단면보수몰탈 조성물을 포함하고, 상기 접착제 조성물을 콘크리트 단면에 도포하고, 상기 단면보수몰탈 조성물을 시공하여 콘크리트 보수보강이 이루어지는 것을 특징으로 한다.또한, 본 발명의 콘크리트 보수보강 공법은, (a) 콘크리트 구조물을 따라 흐르는 유체를 우회시켜 콘크리트 구조물 내부에 유체가 흐르지 않도록 차단하는 단계; (b) 콘크리트 구조물에 발생된 파손 부위, 철근이 부식되어 박리된 부위, 또는 중성화가 이루어져 강도를 상실한 부위에 치핑작업을 진행하여 이물질을 제거하고 세척수를 분사하는 단계; (c) 세척수가 분사된 콘크리트 구조물에 접착제 조성물을 도포하는 단계; (d) 상기 접착제 조성물이 도포된 콘크리트 구조물에 섬유 메시 보강재를 설치 고정하는 단계: (e) 상기 섬유 메시 보강재가 설치된 콘크리트 구조물에 단면보수몰탈 조성물을 도포하여 경화시키는 단계; (f) 상기 단면보수몰탈이 도포된 콘크리트 구조물에 수용성 에폭시계 프라이머를 도포하는 단계; 및 (g) 상기 수용성 에폭시계 프라이머가 도포된 콘크리트 구조물에 수용성 변성에폭시계 표면보호제를 도포하는 단계를 포함하고, 상기 섬유 메시 보강재는, 내알칼리성, 유연성, 인장강도, 탄성계수가 우수한 탄소섬유, 유리섬유, 아라미드 섬유, 바잘트 섬유로 이루어진 메시 구조로 이루어지고, 이중에서 선택되어진 하나 또는 둘 이상의 섬유 메시 보강재를 보강이 필요한 콘크리트 단면에 설치 고정하여 콘크리트의 휨강도를 증진시키고, 지하 구조물 상부에서 또는 하부에서 발생되는 진동을 흡수하는 내진성이 우수한 콘크리트 보강재를 이루며, 규격은 60~300g/㎡ 및 메시 크기가 10~50mm 인 크로스 스티치 타입의 보강재를 사용하는 특징이 있다.
Concrete reinforcement materials including adhesives for wet face and early hardening section repair mortar and concrete repair and reinforcement method
The present invention relates to a concrete repair/reinforcement material composition including an adhesive for a wet surface and an early hardening section repair mortar, and a concrete repair/reinforcement method using the concrete repair/reinforcement material composition, capable of ensuring stability of a worker and improving economic efficiency. According to the present invention, the concrete repair/reinforcement material composition including the adhesive for the wet surface and the early hardening section repair mortar includes: an adhesive composition including a water-soluble acryl polymer, a surfactant, a stabilizer, an antifoaming agent, a moisturizing agent, a film forming agent, and water; and a section repair mortar composition including a cement mixture, a fast hardening material, gypsum, an inorganic expanding material, a metal-based expanding material, hydrophilic nylon-based microfibers, an organic/inorganic composite waterproofing agent, a fluidizing agent, an air-entraining agent, a thixotropic agent, a curing agent, a retarder, and silica sand.
본 발명의 콘크리트 보수보강재료 조성물은, 습윤면용 접착제와 조기경화성 단면보수 모르타르를 구비하는 콘크리트 보수보강재료 조성물 34.0 ~ 45.0중량부, 계면활성제 0.1 ~ 0.2 중량부, 안정제 7.0 ~ 9.3 중량부, 소포제 0.03 ~ 0.06 중량부, 보습제 1.8 ~ 2.7 중량부, 조막제 3.07 ~ 4.74 중량부, 물은 38 ~ 54 중량부로 이루어지는 접착제 조성물; 및 시멘트 혼합물 19 ~ 24 중량부, 속경재 5 ~ 10 중량부, 석고 3 ~ 6.3 중량부, 무기팽창재 1 ~ 3중량부, 금속계 팽창재 0.02 ~ 0.05중량부, 친수성 나일론계 마이크로 섬유 0.1 ~ 0.2 중량부, 유무기 복합 방수제 3.2 ~ 6 중량부, 유동화제 0.1 ~ 0.4 중량부, 공기연행제 0.004 ~ 0.01 중량부, 요변제 0.44 ~ 1.54 중량부, 경화제 0.09 ~ 0.2 중량부, 지연제 0.046 ~ 0.3 중량부, 규사 48 ~ 68중량부로 이루어지는 단면보수몰탈 조성물을 포함하고, 상기 접착제 조성물을 콘크리트 단면에 도포하고, 상기 단면보수몰탈 조성물을 시공하여 콘크리트 보수보강이 이루어지는 것을 특징으로 한다.또한, 본 발명의 콘크리트 보수보강 공법은, (a) 콘크리트 구조물을 따라 흐르는 유체를 우회시켜 콘크리트 구조물 내부에 유체가 흐르지 않도록 차단하는 단계; (b) 콘크리트 구조물에 발생된 파손 부위, 철근이 부식되어 박리된 부위, 또는 중성화가 이루어져 강도를 상실한 부위에 치핑작업을 진행하여 이물질을 제거하고 세척수를 분사하는 단계; (c) 세척수가 분사된 콘크리트 구조물에 접착제 조성물을 도포하는 단계; (d) 상기 접착제 조성물이 도포된 콘크리트 구조물에 섬유 메시 보강재를 설치 고정하는 단계: (e) 상기 섬유 메시 보강재가 설치된 콘크리트 구조물에 단면보수몰탈 조성물을 도포하여 경화시키는 단계; (f) 상기 단면보수몰탈이 도포된 콘크리트 구조물에 수용성 에폭시계 프라이머를 도포하는 단계; 및 (g) 상기 수용성 에폭시계 프라이머가 도포된 콘크리트 구조물에 수용성 변성에폭시계 표면보호제를 도포하는 단계를 포함하고, 상기 섬유 메시 보강재는, 내알칼리성, 유연성, 인장강도, 탄성계수가 우수한 탄소섬유, 유리섬유, 아라미드 섬유, 바잘트 섬유로 이루어진 메시 구조로 이루어지고, 이중에서 선택되어진 하나 또는 둘 이상의 섬유 메시 보강재를 보강이 필요한 콘크리트 단면에 설치 고정하여 콘크리트의 휨강도를 증진시키고, 지하 구조물 상부에서 또는 하부에서 발생되는 진동을 흡수하는 내진성이 우수한 콘크리트 보강재를 이루며, 규격은 60~300g/㎡ 및 메시 크기가 10~50mm 인 크로스 스티치 타입의 보강재를 사용하는 특징이 있다.
Concrete reinforcement materials including adhesives for wet face and early hardening section repair mortar and concrete repair and reinforcement method
습윤면용 접착제와 조기경화성 단면보수 모르타르를 구비하는 콘크리트 보수보강재료 조성물 및 이를 이용하는 콘크리트 보수보강 공법
KIM HEUM (author) / HAN SANG HEON (author)
2020-10-19
Patent
Electronic Resource
Korean
European Patent Office | 2023
|Concrete Section Repair And Reinforcement Method Using Polymer Mortar
European Patent Office | 2023
|Repair-reinforcement mortar of concrete structure and repair-reinforcement method using thereof
European Patent Office | 2020
|