PROTEINIC FOAM-PRODUCING AGENT AND METHOD FOR ITS PRODUCTION
FIELD: construction.SUBSTANCE: proteinic foam-producing agent for the production of porous construction materials includes, wt %: proteinaceous substance of microbiological synthesis - waste biomass of Aspergillus niger fungus of citric acid production 16, alkaline agent - mixture of slaked lime 2-4 and dust of electric filters formed during purification of exhaust gases of burning kilns of cement production, 0-2, stabilising additive in the form of 15% solution of metal salt solution, water - the rest. Method for producing the above mentioned proteinic foam-producing agent comprises mixing of protein-containing agent of microbiological synthesis, alkaline reagent, previously suspended in water, hydrolysis in the microwave field with frequency of 2450 Hz and power of 700 W during 20 minutes, cooling of mixture up to the room temperature, filtering, diluting of the obtained hydrolyzate up to the required foam-producing activity and stabilisation by the metal salt solution.EFFECT: reduction of duration of the alkaline hydrolysis, waste utilisation.2 cl, 2 tbl
Изобретение относится к области производства пористых строительных материалов, в частности к пенообразователям, полученным на основе органических материалов и неорганических промышленных отходов. Белковый пенообразователь для производства пористых строительных материалов включает, мас.%: протеинсодержащее вещество микробиологического синтеза - отработанную биомассу гриба Aspergillus niger производства лимонной кислоты 16, щелочной реагент - смесь извести гашеной 2-4 и пыли электрофильтров, образующейся при очистке отходящих газов обжиговых печей цементного производства, 0-2, стабилизирующую добавку в виде 15%-ного раствора соли металла, воду - остальное. Способ получения указанного выше белкового пенообразователя включает смешение протеинсодержащего вещества микробиологического синтеза, щелочного реагента, предварительно суспензированного в воде, гидролиз в СВЧ-поле с частотой 2450 Гц и мощностью 700 Вт в течение 20 минут, охлаждение смеси до комнатной температуры, фильтрование, разбавление полученного гидролизата до необходимой пенообразующей активности и стабилизацию раствором соли металла. Технический результат - сокращение длительности щелочного гидролиза, утилизация отходов. 2 н.п. ф-лы, 2 табл.
PROTEINIC FOAM-PRODUCING AGENT AND METHOD FOR ITS PRODUCTION
FIELD: construction.SUBSTANCE: proteinic foam-producing agent for the production of porous construction materials includes, wt %: proteinaceous substance of microbiological synthesis - waste biomass of Aspergillus niger fungus of citric acid production 16, alkaline agent - mixture of slaked lime 2-4 and dust of electric filters formed during purification of exhaust gases of burning kilns of cement production, 0-2, stabilising additive in the form of 15% solution of metal salt solution, water - the rest. Method for producing the above mentioned proteinic foam-producing agent comprises mixing of protein-containing agent of microbiological synthesis, alkaline reagent, previously suspended in water, hydrolysis in the microwave field with frequency of 2450 Hz and power of 700 W during 20 minutes, cooling of mixture up to the room temperature, filtering, diluting of the obtained hydrolyzate up to the required foam-producing activity and stabilisation by the metal salt solution.EFFECT: reduction of duration of the alkaline hydrolysis, waste utilisation.2 cl, 2 tbl
Изобретение относится к области производства пористых строительных материалов, в частности к пенообразователям, полученным на основе органических материалов и неорганических промышленных отходов. Белковый пенообразователь для производства пористых строительных материалов включает, мас.%: протеинсодержащее вещество микробиологического синтеза - отработанную биомассу гриба Aspergillus niger производства лимонной кислоты 16, щелочной реагент - смесь извести гашеной 2-4 и пыли электрофильтров, образующейся при очистке отходящих газов обжиговых печей цементного производства, 0-2, стабилизирующую добавку в виде 15%-ного раствора соли металла, воду - остальное. Способ получения указанного выше белкового пенообразователя включает смешение протеинсодержащего вещества микробиологического синтеза, щелочного реагента, предварительно суспензированного в воде, гидролиз в СВЧ-поле с частотой 2450 Гц и мощностью 700 Вт в течение 20 минут, охлаждение смеси до комнатной температуры, фильтрование, разбавление полученного гидролизата до необходимой пенообразующей активности и стабилизацию раствором соли металла. Технический результат - сокращение длительности щелочного гидролиза, утилизация отходов. 2 н.п. ф-лы, 2 табл.
PROTEINIC FOAM-PRODUCING AGENT AND METHOD FOR ITS PRODUCTION
БЕЛКОВЫЙ ПЕНООБРАЗОВАТЕЛЬ И СПОСОБ ЕГО ПОЛУЧЕНИЯ
STAROSTINA IRINA VIKTOROVNA (author) / OVCHAROVA IRINA VLADIMIROVNA (author) / PENDJURIN EVGENIJ ALEKSANDROVICH (author) / KUZINA ELENA MIKHAJLOVNA (author) / BESEDINA IRINA NIKOLAEVNA (author)
2015-06-10
Patent
Electronic Resource
Russian
IPC:
C04B
Kalk
,
LIME
Water capillary absorption of cellular clayed concrete obtained by proteinic foaming
British Library Conference Proceedings | 2002
|British Library Online Contents | 2012
|British Library Online Contents | 2017
|British Library Conference Proceedings | 2005
|Nano foaming agent composition for producing foam concrete and preparation method thereof
European Patent Office | 2023
|