CLINKER-FREE BINDER
FIELD: construction.SUBSTANCE: invention relates to construction materials, particularly, to binders and can be used for production of dry construction mixes, mortars and concretes as well as other construction materials. This binder comprises the following components: annealed at 800-900°C mix of magnesium-bearing carbonates and clays, magnesium sulphate and mineral additive, i.e. zeolite-bearing carbonate-silicic rock, plasticising agent SP-1 and gardening promoter, i.e. sodium sulphate, at the following ratio of said components, wt %: said mix - 58-85, magnesium sulphate - 3-6, zeolite-bearing carbonate-silicic rock - 10-30, plasticising agent SP-1 - 1-2, sodium sulphate - 1-4. Note here that magnesium-bearing carbonate rock-to-clay ratio makes (2.7-10):1.EFFECT: higher strength under normal conditions.2 cl, 2 tbl
Изобретение относится к области строительных материалов, в частности к вяжущим, и может найти применение в строительной отрасли для изготовления сухих строительных смесей, строительных растворов и бетонов, а также других строительных материалов. Технический результат изобретения - повышение прочности в нормальных условиях. Вяжущее включает обожженную при температуре 800-900°C смесь магнийсодержащих карбонатных пород и глины, сульфат магния и минеральную добавку - цеолитсодержащую карбонатно-кремнеземистую породу, пластификатор СП-1 и ускоритель твердения - сульфат натрия при следующем содержании ингредиентов в масс. %: указанная смесь 58-85, сульфат магния 3-6, цеолитсодержащая карбонатно-кремнеземистая порода 10-30, пластификатор СП-1 1-2, сульфат натрия 1-4. Причем соотношение магнийсодержащих карбонатных пород и глины составляет (2,7-10): 1. 1 з.п. ф-лы, 2 табл.
CLINKER-FREE BINDER
FIELD: construction.SUBSTANCE: invention relates to construction materials, particularly, to binders and can be used for production of dry construction mixes, mortars and concretes as well as other construction materials. This binder comprises the following components: annealed at 800-900°C mix of magnesium-bearing carbonates and clays, magnesium sulphate and mineral additive, i.e. zeolite-bearing carbonate-silicic rock, plasticising agent SP-1 and gardening promoter, i.e. sodium sulphate, at the following ratio of said components, wt %: said mix - 58-85, magnesium sulphate - 3-6, zeolite-bearing carbonate-silicic rock - 10-30, plasticising agent SP-1 - 1-2, sodium sulphate - 1-4. Note here that magnesium-bearing carbonate rock-to-clay ratio makes (2.7-10):1.EFFECT: higher strength under normal conditions.2 cl, 2 tbl
Изобретение относится к области строительных материалов, в частности к вяжущим, и может найти применение в строительной отрасли для изготовления сухих строительных смесей, строительных растворов и бетонов, а также других строительных материалов. Технический результат изобретения - повышение прочности в нормальных условиях. Вяжущее включает обожженную при температуре 800-900°C смесь магнийсодержащих карбонатных пород и глины, сульфат магния и минеральную добавку - цеолитсодержащую карбонатно-кремнеземистую породу, пластификатор СП-1 и ускоритель твердения - сульфат натрия при следующем содержании ингредиентов в масс. %: указанная смесь 58-85, сульфат магния 3-6, цеолитсодержащая карбонатно-кремнеземистая порода 10-30, пластификатор СП-1 1-2, сульфат натрия 1-4. Причем соотношение магнийсодержащих карбонатных пород и глины составляет (2,7-10): 1. 1 з.п. ф-лы, 2 табл.
CLINKER-FREE BINDER
БЕСКЛИНКЕРНОЕ ВЯЖУЩЕЕ
SHELIKHOV NIKOLAJ SERGEEVICH (author) / SAGDIEV RUSLAN RUSTEMOVICH (author) / RAKHIMOV RAVIL ZUFAROVICH (author)
2015-06-20
Patent
Electronic Resource
Russian
IPC:
C04B
Kalk
,
LIME
COMPOSITION OF SELF-HEALING CONCRETE USING CLINKER BINDER AND CLINKER AGGREGATE
European Patent Office | 2021
COMPOSITION OF SELF-HEALING CONCRETE USING CLINKER BINDER AND CLINKER AGGREGATE
European Patent Office | 2022