HYDRAULIC BINDER WITH LOW CLINKER CONTENT
FIELD: technological processes.SUBSTANCE: present invention relates to hydraulic binder involving the parts by weight: (a) from 20 to 60 parts of portland cement clinker; (b) 20 to 40 parts of slag; and (c) from 5 to 60 parts of inorganic material different from the clinker and slag; wherein sum of (a), (b) and (c) equals 100 parts; while binder additionally contains slag activator including on 100 parts of the sum of (a) and (b): from 1.4 to 6.55 parts of alkali metal salt in an equivalent of NaO; and from 1.1 to 11.0 parts of calcium sulphate in an equivalent of SO. Invention also relates to hydraulic composition and method of its production, to shaped product and use of the hydraulic composition. Invention is developed in subclaims.EFFECT: strength increase during 24 hours after preparation and reduced carbon dioxide emission after 28 days.1 cl, 2 tbl
Настоящее изобретение относится к гидравлическому вяжущему, включающему в частях по массе: (a) от 20 до 60 частей портландцементного клинкера; (b) от 20 до 40 частей шлака; и (c) от 5 до 60 частей неорганического материала, отличного от клинкера и шлака; причем сумма (a), (b) и (c) равна 100 частям; где вяжущее дополнительно включает активатор шлака, включающий на 100 частей суммы (a) и (b): от 1,4 до 6,55 частей соли щелочного металла в выражении на эквивалент NaO; и от 1,1 до 11,0 частей сульфата кальция в выражении на SO. Изобретение также относится к гидравлической композиции и способу её получения, к профилированному изделию и к применению гидравлической композиции. Изобретение развито в зависимых пунктах формулы изобретения. Технический результат - повышение прочности через 24 часа после приготовления и через 28 суток, снижение выделения углекислого газа. 2 табл.
HYDRAULIC BINDER WITH LOW CLINKER CONTENT
FIELD: technological processes.SUBSTANCE: present invention relates to hydraulic binder involving the parts by weight: (a) from 20 to 60 parts of portland cement clinker; (b) 20 to 40 parts of slag; and (c) from 5 to 60 parts of inorganic material different from the clinker and slag; wherein sum of (a), (b) and (c) equals 100 parts; while binder additionally contains slag activator including on 100 parts of the sum of (a) and (b): from 1.4 to 6.55 parts of alkali metal salt in an equivalent of NaO; and from 1.1 to 11.0 parts of calcium sulphate in an equivalent of SO. Invention also relates to hydraulic composition and method of its production, to shaped product and use of the hydraulic composition. Invention is developed in subclaims.EFFECT: strength increase during 24 hours after preparation and reduced carbon dioxide emission after 28 days.1 cl, 2 tbl
Настоящее изобретение относится к гидравлическому вяжущему, включающему в частях по массе: (a) от 20 до 60 частей портландцементного клинкера; (b) от 20 до 40 частей шлака; и (c) от 5 до 60 частей неорганического материала, отличного от клинкера и шлака; причем сумма (a), (b) и (c) равна 100 частям; где вяжущее дополнительно включает активатор шлака, включающий на 100 частей суммы (a) и (b): от 1,4 до 6,55 частей соли щелочного металла в выражении на эквивалент NaO; и от 1,1 до 11,0 частей сульфата кальция в выражении на SO. Изобретение также относится к гидравлической композиции и способу её получения, к профилированному изделию и к применению гидравлической композиции. Изобретение развито в зависимых пунктах формулы изобретения. Технический результат - повышение прочности через 24 часа после приготовления и через 28 суток, снижение выделения углекислого газа. 2 табл.
HYDRAULIC BINDER WITH LOW CLINKER CONTENT
ГИДРАВЛИЧЕСКОЕ ВЯЖУЩЕЕ С НИЗКИМ СОДЕРЖАНИЕМ КЛИНКЕРА
SHVARTSENTRUBER ARNO (author) / MARTEN MILEN (author) / PURSEL FABRIS (author)
2016-11-10
Patent
Electronic Resource
Russian
IPC:
C04B
Kalk
,
LIME
FLUIDIZER FOR A HYDRAULIC BINDER COMPRISING A SULFOALUMINOUS CLINKER
European Patent Office | 2016
|