A platform for research: civil engineering, architecture and urbanism
METHOD OF PRODUCING PLASTICISING ADDITIVE FOR CONCRETE AND ADDITIVE OBTAINED USING SAID METHOD
FIELD: chemistry.SUBSTANCE: method includes static copolycondensation of sulphanilic acid with formaldehyde by mixing components while heating over a calculated period of time, followed by alkaline neutralisation of the end product, wherein static copolycondensation of sulphanilic acid with formaldehyde is carried out in conjunction with phenol and/or derivatives from the phenol series: alkylphenol, ethoxylated alkylphenol, ethoxylated phenol, with the following content of components, wt %: sulphanilic acid 10-20, phenol 10-20, derivatives from the phenol series 1-10, formaldehyde 5-15, water - the balance up to 100%, wherein the copolycondensation process is carried out at temperature of the mixture of 80-120°C, the calculated period of time is 20-720 minutes, and neutralisation of the copolycondensation product - water-soluble polymer - is carried out with 10-20% alkali solution and the product is cooled to 20-30°C. The superplasticiser obtained using the present method is a water-soluble polymer and contains, wt %: polymer 20-45, water - the balance up to 100%.EFFECT: obtaining an additive having both hydrophilic and hydrophobic properties, longer mobility retention period.2 cl, 3 tbl
Изобретение направлено на получения пластифицирующей добавки для бетона, обладающей свойствами суперпластификатора, более технологичной и экономически выгодной в производстве. Способ включает статическую сополиконденсацию сульфаниловой кислоты с формальдегидом путем перемешивания компонентов при нагревании в расчетный период времени с последующей щелочной нейтрализацией конечного продукта, при этом статическую сополиконденсацию сульфаниловой кислоты с формальдегидом ведут совместно с фенолом и/или с производными из ряда фенолов: алкилфенолом, этоксилированным алкилфенолом, этоксилированным фенолом при следующем содержании компонентов, мас.%: сульфаниловая кислота 10-20, фенол 10-20, производные из ряда фенола 1-10, формальдегид 5-15, вода остальное до 100%, при этом процесс сополиконденсации осуществляют при температуре смеси 80-120°C, расчетный период времени составляет 20-720 мин, а нейтрализацию продукта сополиконденсации - водорастворимый полимер проводят 10-20%-ным раствором щелочи и охлаждают продукт до температуры 20-30°C. Полученный по указанному способу суперпластификатор является водорастворимым полимером и содержит в мас.%: полимер 20-45, остальное - вода до 100%. Технический результат - получение добавки, обладающей как гидрофильными, так и гидрофобными свойствами, увеличение сроков сохранения подвижности. 2 н.п. ф-лы, 3 табл.
METHOD OF PRODUCING PLASTICISING ADDITIVE FOR CONCRETE AND ADDITIVE OBTAINED USING SAID METHOD
FIELD: chemistry.SUBSTANCE: method includes static copolycondensation of sulphanilic acid with formaldehyde by mixing components while heating over a calculated period of time, followed by alkaline neutralisation of the end product, wherein static copolycondensation of sulphanilic acid with formaldehyde is carried out in conjunction with phenol and/or derivatives from the phenol series: alkylphenol, ethoxylated alkylphenol, ethoxylated phenol, with the following content of components, wt %: sulphanilic acid 10-20, phenol 10-20, derivatives from the phenol series 1-10, formaldehyde 5-15, water - the balance up to 100%, wherein the copolycondensation process is carried out at temperature of the mixture of 80-120°C, the calculated period of time is 20-720 minutes, and neutralisation of the copolycondensation product - water-soluble polymer - is carried out with 10-20% alkali solution and the product is cooled to 20-30°C. The superplasticiser obtained using the present method is a water-soluble polymer and contains, wt %: polymer 20-45, water - the balance up to 100%.EFFECT: obtaining an additive having both hydrophilic and hydrophobic properties, longer mobility retention period.2 cl, 3 tbl
Изобретение направлено на получения пластифицирующей добавки для бетона, обладающей свойствами суперпластификатора, более технологичной и экономически выгодной в производстве. Способ включает статическую сополиконденсацию сульфаниловой кислоты с формальдегидом путем перемешивания компонентов при нагревании в расчетный период времени с последующей щелочной нейтрализацией конечного продукта, при этом статическую сополиконденсацию сульфаниловой кислоты с формальдегидом ведут совместно с фенолом и/или с производными из ряда фенолов: алкилфенолом, этоксилированным алкилфенолом, этоксилированным фенолом при следующем содержании компонентов, мас.%: сульфаниловая кислота 10-20, фенол 10-20, производные из ряда фенола 1-10, формальдегид 5-15, вода остальное до 100%, при этом процесс сополиконденсации осуществляют при температуре смеси 80-120°C, расчетный период времени составляет 20-720 мин, а нейтрализацию продукта сополиконденсации - водорастворимый полимер проводят 10-20%-ным раствором щелочи и охлаждают продукт до температуры 20-30°C. Полученный по указанному способу суперпластификатор является водорастворимым полимером и содержит в мас.%: полимер 20-45, остальное - вода до 100%. Технический результат - получение добавки, обладающей как гидрофильными, так и гидрофобными свойствами, увеличение сроков сохранения подвижности. 2 н.п. ф-лы, 3 табл.
METHOD OF PRODUCING PLASTICISING ADDITIVE FOR CONCRETE AND ADDITIVE OBTAINED USING SAID METHOD
СПОСОБ ПОЛУЧЕНИЯ ПЛАСТИФИЦИРУЮЩЕЙ ДОБАВКИ ДЛЯ БЕТОНА И ДОБАВКА, ПОЛУЧЕННАЯ УКАЗАННЫМ СПОСОБОМ
CHAGAROVSKIJ ALEKSEJ OLEGOVICH (author)
2015-06-20
Patent
Electronic Resource
Russian
IPC:
C04B
Kalk
,
LIME
ADDITIVE FOR CONCRETE AND METHOD FOR PRODUCING ADDITIVE FOR CONCRETE
European Patent Office | 2019
|ADDITIVE FOR CONCRETE AND METHOD FOR PRODUCING ADDITIVE FOR CONCRETE
European Patent Office | 2019
|