A platform for research: civil engineering, architecture and urbanism
METHOD OF PRODUCING BINDER FOR MAKING CARBON MATERIALS AND ARTICLES THEREFROM
FIELD: metallurgy.SUBSTANCE: invention relates to metallurgy, in particular to methods for producing and preparing electrode pitch intended for production of anode mass, coal and graphitised products, carbon structural materials, and can be used in coke-chemical or petroleum refining industry. Method for preparing a binder for production of carbon materials and products made of them comprises mixing coal tar and petroleum refining liquid product having a density at 20 °C is not less than 1.02 g/cm; viscosity at 100 °C is not more than 20 cSt; coking ability of not less than 5 %; stripping fraction boiling below 300 °C, no more than 5 %, in a ratio of 85:15 to 50:50 wt%, heat treating resultant mixture at 410-430 °C in liquid phase with separation of distillate fractions and undistillable distillate residue and air oxidation of undistillable distillation residue at 325-360 °C and air supply rate of 20-54 l/kg of pitch.EFFECT: proposed method allows to obtain binder pitch suitable for production of anode mass.1 cl, 5 tbl, 12 ex
Изобретение относится к области металлургии, в частности к способам получения и подготовки электродного пека, предназначенного для производства анодной массы, угольной и графитированной продукции, конструкционных углеграфитовых материалов, и может найти применение в коксохимической или нефтеперерабатывающей промышленности. Способ получения связующего для изготовления углеродных материалов и изделий из них включает смешение каменноугольной смолы и жидкого продукта нефтепереработки, обладающего плотностью при 20°C не менее 1,02 г/см; вязкостью при 100°C не более 20 сСт; коксуемостью не менее 5%; отгоном фракции, выкипающей до 300°C, не более 5%, в соотношении от 85:15 до 50:50 мас.%, термообработку полученной смеси при 410-430°C в жидкой фазе с отделением дистиллятных фракций и неперегоняемого остатка дистилляции и окисление воздухом неперегоняемого остатка дистилляции при 325-360°C и при подаче воздуха из расчета 20-54 л/кг пека. Предлагаемый способ позволяет получать связующий пек, пригодный для изготовления анодной массы. 5 табл., 12 пр.
METHOD OF PRODUCING BINDER FOR MAKING CARBON MATERIALS AND ARTICLES THEREFROM
FIELD: metallurgy.SUBSTANCE: invention relates to metallurgy, in particular to methods for producing and preparing electrode pitch intended for production of anode mass, coal and graphitised products, carbon structural materials, and can be used in coke-chemical or petroleum refining industry. Method for preparing a binder for production of carbon materials and products made of them comprises mixing coal tar and petroleum refining liquid product having a density at 20 °C is not less than 1.02 g/cm; viscosity at 100 °C is not more than 20 cSt; coking ability of not less than 5 %; stripping fraction boiling below 300 °C, no more than 5 %, in a ratio of 85:15 to 50:50 wt%, heat treating resultant mixture at 410-430 °C in liquid phase with separation of distillate fractions and undistillable distillate residue and air oxidation of undistillable distillation residue at 325-360 °C and air supply rate of 20-54 l/kg of pitch.EFFECT: proposed method allows to obtain binder pitch suitable for production of anode mass.1 cl, 5 tbl, 12 ex
Изобретение относится к области металлургии, в частности к способам получения и подготовки электродного пека, предназначенного для производства анодной массы, угольной и графитированной продукции, конструкционных углеграфитовых материалов, и может найти применение в коксохимической или нефтеперерабатывающей промышленности. Способ получения связующего для изготовления углеродных материалов и изделий из них включает смешение каменноугольной смолы и жидкого продукта нефтепереработки, обладающего плотностью при 20°C не менее 1,02 г/см; вязкостью при 100°C не более 20 сСт; коксуемостью не менее 5%; отгоном фракции, выкипающей до 300°C, не более 5%, в соотношении от 85:15 до 50:50 мас.%, термообработку полученной смеси при 410-430°C в жидкой фазе с отделением дистиллятных фракций и неперегоняемого остатка дистилляции и окисление воздухом неперегоняемого остатка дистилляции при 325-360°C и при подаче воздуха из расчета 20-54 л/кг пека. Предлагаемый способ позволяет получать связующий пек, пригодный для изготовления анодной массы. 5 табл., 12 пр.
METHOD OF PRODUCING BINDER FOR MAKING CARBON MATERIALS AND ARTICLES THEREFROM
СПОСОБ ПОЛУЧЕНИЯ СВЯЗУЮЩЕГО ДЛЯ ИЗГОТОВЛЕНИЯ УГЛЕРОДНЫХ МАТЕРИАЛОВ И ИЗДЕЛИЙ ИЗ НИХ
FRIZORGER VLADIMIR KONSTANTINOVICH (author) / MARAKUSHINA ELENA NIKOLAEVNA (author) / PINGIN VITALIJ VALEREVICH (author) / KRAK MIKHAIL IVANOVICH (author)
2016-04-27
Patent
Electronic Resource
Russian
CARBON-CARBON COMPOSITE MATERIAL AND METHOD OF MAKING ARTICLES THEREFROM
European Patent Office | 2015
|European Patent Office | 2024
|CARBON-CARBON COMPOSITE MATERIAL AND METHOD FOR MANUFACTURING ARTICLES THEREFROM
European Patent Office | 2018
|BINDER COMPOSITION COMPRISING FLY ASH AND HIGH-STRENGTH BINDER PREPARED THEREFROM
European Patent Office | 2020
|