METHOD FOR OBTAINING SYNTHETIC LIGHT CERAMIC SAND AND ITS APPLICATION
FIELD: construction materials.SUBSTANCE: group of inventions relates to a method for producing light ceramic sand and using it as a building material, and also as light sand used in hydraulic fracturing for shale gas extraction. The method for producing light ceramic sand includes dry spraying of fly ash in an amount from 5 to 50 wt. %, in wet bauxite residue in an amount from 50 to 95 wt. %, with simultaneous rotation of the rotor and the pallet, optional addition of bentonite in an amount from 0 to 5 wt. %, or fine silica from 0 to 10 wt. %, to fly ash or to wet bauxite residue, formation of granules using a high-intensity agitator providing high shear stresses, drying of granules at temperatures from 150 to 300°C in a fluidized bed to obtain dried granules, high-temperature sintering of dried granules at a temperature from 1015 to 1275°C to obtain light ceramic sand. Light ceramic sand is obtained by the above method. Light ceramic sand is used for the production of light mortars and concrete. The group of inventions is developed in dependent points of the formula.EFFECT: creation of a simple and economical method for obtaining light ceramic sand, the disposal of industrial waste.8 cl, 1 dwg, 1 tbl
Группа изобретений относится к способу получения легкого керамического песка и применению его в качестве строительного материала, а также в качестве легкого песка, используемого при гидроразрыве пласта для добычи сланцевого газа. Способ получения легкого керамического песка включает сухое распыление золы-уноса в количестве от 5 до 50 мас.% во влажный бокситовый остаток в количестве от 50 до 95 мас.% при одновременном вращении ротора и поддона, необязательное добавление бентонита в количестве от 0 до 5 мас.% или мелкодисперсного кремнезема от 0 до 10 мас.% к золе-уноса или к влажному бокситовому остатку, формирование гранул с использованием высокоинтенсивной мешалки, обеспечивающей высокие напряжения сдвига, сушку гранул при температуре от 150 до 300°С в псевдоожиженном слое с получением высушенных гранул, высокотемпературное спекание высушенных гранул при температуре от 1015 до 1275°С с получением легкого керамического песка. Легкий керамический песок, полученный указанным выше способом. Применение легкого керамического песка для производства легких строительных растворов и бетона. Группа изобретений развита в зависимых пунктах формулы. Технический результат – создание простого и экономичного способа получения легкого керамического песка, утилизация промышленных отходов. 3 н. и 5 з.п. ф-лы, 1 ил., 1 табл.
METHOD FOR OBTAINING SYNTHETIC LIGHT CERAMIC SAND AND ITS APPLICATION
FIELD: construction materials.SUBSTANCE: group of inventions relates to a method for producing light ceramic sand and using it as a building material, and also as light sand used in hydraulic fracturing for shale gas extraction. The method for producing light ceramic sand includes dry spraying of fly ash in an amount from 5 to 50 wt. %, in wet bauxite residue in an amount from 50 to 95 wt. %, with simultaneous rotation of the rotor and the pallet, optional addition of bentonite in an amount from 0 to 5 wt. %, or fine silica from 0 to 10 wt. %, to fly ash or to wet bauxite residue, formation of granules using a high-intensity agitator providing high shear stresses, drying of granules at temperatures from 150 to 300°C in a fluidized bed to obtain dried granules, high-temperature sintering of dried granules at a temperature from 1015 to 1275°C to obtain light ceramic sand. Light ceramic sand is obtained by the above method. Light ceramic sand is used for the production of light mortars and concrete. The group of inventions is developed in dependent points of the formula.EFFECT: creation of a simple and economical method for obtaining light ceramic sand, the disposal of industrial waste.8 cl, 1 dwg, 1 tbl
Группа изобретений относится к способу получения легкого керамического песка и применению его в качестве строительного материала, а также в качестве легкого песка, используемого при гидроразрыве пласта для добычи сланцевого газа. Способ получения легкого керамического песка включает сухое распыление золы-уноса в количестве от 5 до 50 мас.% во влажный бокситовый остаток в количестве от 50 до 95 мас.% при одновременном вращении ротора и поддона, необязательное добавление бентонита в количестве от 0 до 5 мас.% или мелкодисперсного кремнезема от 0 до 10 мас.% к золе-уноса или к влажному бокситовому остатку, формирование гранул с использованием высокоинтенсивной мешалки, обеспечивающей высокие напряжения сдвига, сушку гранул при температуре от 150 до 300°С в псевдоожиженном слое с получением высушенных гранул, высокотемпературное спекание высушенных гранул при температуре от 1015 до 1275°С с получением легкого керамического песка. Легкий керамический песок, полученный указанным выше способом. Применение легкого керамического песка для производства легких строительных растворов и бетона. Группа изобретений развита в зависимых пунктах формулы. Технический результат – создание простого и экономичного способа получения легкого керамического песка, утилизация промышленных отходов. 3 н. и 5 з.п. ф-лы, 1 ил., 1 табл.
METHOD FOR OBTAINING SYNTHETIC LIGHT CERAMIC SAND AND ITS APPLICATION
СПОСОБ ПОЛУЧЕНИЯ СИНТЕТИЧЕСКОГО ЛЕГКОГО КЕРАМИЧЕСКОГО ПЕСКА И ЕГО ПРИМЕНЕНИЕ
ABBAS MOHAMMAD KHAN (author)
2022-01-25
Patent
Electronic Resource
Russian
IPC:
C04B
Kalk
,
LIME
European Patent Office | 2018
|A NOVEL METHOD OF PRODUCING SYNTHETIC LIGHTWEIGHT CERAMIC SAND AND USES THEREOF
European Patent Office | 2020
|A novel method of producing synthetic lightweight ceramic sand and uses thereof
European Patent Office | 2023
|A NOVEL METHOD OF PRODUCING SYNTHETIC LIGHTWEIGHT CERAMIC SAND AND USES THEREOF
European Patent Office | 2021
|