PRODUCTION METHOD FOR FORSTERITE FINE PARTICLES
A method for producing forsterite microparticles having a primary particle size of 1 to 200 nm, as determined through electron microscopy, characterized in that the method includes spray-drying, at 50° C. or higher and lower than 300° C., a solution containing a water-soluble magnesium salt and colloidal silica at a mole ratio of magnesium atoms to silicon atoms (Mg/Si) of 2; and subsequently, firing the spray-dried product in air at 800 to 1,000° C.
PRODUCTION METHOD FOR FORSTERITE FINE PARTICLES
A method for producing forsterite microparticles having a primary particle size of 1 to 200 nm, as determined through electron microscopy, characterized in that the method includes spray-drying, at 50° C. or higher and lower than 300° C., a solution containing a water-soluble magnesium salt and colloidal silica at a mole ratio of magnesium atoms to silicon atoms (Mg/Si) of 2; and subsequently, firing the spray-dried product in air at 800 to 1,000° C.
PRODUCTION METHOD FOR FORSTERITE FINE PARTICLES
ISAJI TADAYUKI (author) / OGIHARA TAKASHI (author) / KODERA TAKAYUKI (author)
2016-11-17
Patent
Electronic Resource
English