ASPHALT CONCRETE WITH AGGREGATES AND WASTE DERIVED FROM RECYCLED WASTE GLASS AND WASTE PLASTICS AND MANUFACTURING PROCESS
The invention describes the compositions and the process of obtaining an asphaltic concrete for a single base and binder course (layer) of the road structure, composed of a bituminous mixture, containing aggregates derived from crushed and sorted recycled glass 0/4 and 4/8 mm and shredded plastic 0/10 mm. The new material is made up in two recipes: with total or partial replacement of conventional mineral aggregates: sand, rock aggregates and filler. The recipe partially replacing, but at least 20%, the conventional mineral aggregates, meets all the requirements according to AND IND 605-2018, required for the roads of technical class 3, 4 and 5.The process of obtaining the new asphalt mixture material is characterized by the fact that the glass is mixed together with the aggregates and the filler at 160-180° C., bitumen heated to 180° C. is added and, after mixing the mixture for 30-35 sec., the shredded plastic constituent is added and further mixed for 10-15 sec., resulting in a polymerized asphalt mixture.
ASPHALT CONCRETE WITH AGGREGATES AND WASTE DERIVED FROM RECYCLED WASTE GLASS AND WASTE PLASTICS AND MANUFACTURING PROCESS
The invention describes the compositions and the process of obtaining an asphaltic concrete for a single base and binder course (layer) of the road structure, composed of a bituminous mixture, containing aggregates derived from crushed and sorted recycled glass 0/4 and 4/8 mm and shredded plastic 0/10 mm. The new material is made up in two recipes: with total or partial replacement of conventional mineral aggregates: sand, rock aggregates and filler. The recipe partially replacing, but at least 20%, the conventional mineral aggregates, meets all the requirements according to AND IND 605-2018, required for the roads of technical class 3, 4 and 5.The process of obtaining the new asphalt mixture material is characterized by the fact that the glass is mixed together with the aggregates and the filler at 160-180° C., bitumen heated to 180° C. is added and, after mixing the mixture for 30-35 sec., the shredded plastic constituent is added and further mixed for 10-15 sec., resulting in a polymerized asphalt mixture.
ASPHALT CONCRETE WITH AGGREGATES AND WASTE DERIVED FROM RECYCLED WASTE GLASS AND WASTE PLASTICS AND MANUFACTURING PROCESS
DEBIE DENNIS (author) / ZAPCIU MIRON (author) / TUDOSE SEBASTIAN (author) / CLADOVEANU FLAVIUS-VALERIU (author) / ENE NICOLETA-MARIANA (author) / DIMA CATALIN (author) / IONESCU NICOLETA-ADACIZA (author) / COSTEI MONICA (author)
2024-03-28
Patent
Electronic Resource
English
IPC:
C08L
COMPOSITIONS OF MACROMOLECULAR COMPOUNDS
,
Massen auf Basis makromolekularer Verbindungen
/
C08K
Verwendung von anorganischen oder nichtmakromolekularen organischen Stoffen als Zusatzstoffe
,
USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES AS COMPOUNDING INGREDIENTS
/
E01C
Bau von Straßen, Sportplätzen oder dgl., Decken dafür
,
CONSTRUCTION OF, OR SURFACES FOR, ROADS, SPORTS GROUNDS, OR THE LIKE
European Patent Office | 2015
|APPARATUS OF MANUFACTURING RECYCLED AGGREGATES DERIVED FROM CONSTRUCTION WASTE
European Patent Office | 2021
|Stone Matrix Asphalt Using Aggregates Modified with Waste Plastics
British Library Conference Proceedings | 2014
|