Solvent based slurry compositions for making environmental barrier coatings and environmental barrier coatings comprising the same
Organic solvent based slurry compositions for making an environmental barrier coating including from about 6.8 wt % to about 96.1 wt % solvent; from about 3.9 wt % to about 93.2 wt % primary material; and from about 0.01 wt % to about 20 wt % slurry sintering aid.
Solvent based slurry compositions for making environmental barrier coatings and environmental barrier coatings comprising the same
Organic solvent based slurry compositions for making an environmental barrier coating including from about 6.8 wt % to about 96.1 wt % solvent; from about 3.9 wt % to about 93.2 wt % primary material; and from about 0.01 wt % to about 20 wt % slurry sintering aid.
Solvent based slurry compositions for making environmental barrier coatings and environmental barrier coatings comprising the same
KIRBY GLEN HAROLD (author) / BOUTWELL BRETT ALLEN (author)
2015-06-23
Patent
Electronic Resource
English
European Patent Office | 2018
|European Patent Office | 2019
|European Patent Office | 2018
|European Patent Office | 2015
|Solvent based slurry compositions for making environmental barrier coatings
European Patent Office | 2015
|