Slurry compositions for making environmental barrier coatings and environmental barrier coatings comprising the same
Slurry compositions for making an environmental barrier coating including from about 9 wt % to about 81 wt % water; from about 3 wt % to about 72 wt % primary material; and from about 0.1 wt % to about 18 wt % slurry sintering aid, and environmental barrier coatings including such compositions.
Slurry compositions for making environmental barrier coatings and environmental barrier coatings comprising the same
Slurry compositions for making an environmental barrier coating including from about 9 wt % to about 81 wt % water; from about 3 wt % to about 72 wt % primary material; and from about 0.1 wt % to about 18 wt % slurry sintering aid, and environmental barrier coatings including such compositions.
Slurry compositions for making environmental barrier coatings and environmental barrier coatings comprising the same
KIRBY GLEN HAROLD (author) / BOUTWELL BRETT ALLEN (author)
2015-07-07
Patent
Electronic Resource
English
European Patent Office | 2018
|European Patent Office | 2018
|European Patent Office | 2015
|European Patent Office | 2019
|Solvent based slurry compositions for making environmental barrier coatings
European Patent Office | 2015
|