A platform for research: civil engineering, architecture and urbanism
Method of manufacturing transparent sesquioxide sintered body, and transparent sesquioxide sintered body manufactured by the method
Provided is a method of manufacturing a transparent sesquioxide sintered body by which a transparent M2O3 type sesquioxide sintered body can be manufactured. A powder including particles of an oxide of at least one rare earth element selected from Y, Sc or lanthanide elements and Zr oxide particles is prepared as a raw material powder, wherein in the particle size distribution of the rare earth element oxide particles, or in the particle size distribution of secondary particles in the case where the rare earth element oxide particles are agglomerated to form the secondary particles, the particle diameter D2.5 value at which the cumulative particle amount from the minimum particle size side is 2.5% based on the total particle amount is in the range from 180 nm to 2000 nm, inclusive. The raw material powder is press molded into a predetermined shape, followed by sintering.
Method of manufacturing transparent sesquioxide sintered body, and transparent sesquioxide sintered body manufactured by the method
Provided is a method of manufacturing a transparent sesquioxide sintered body by which a transparent M2O3 type sesquioxide sintered body can be manufactured. A powder including particles of an oxide of at least one rare earth element selected from Y, Sc or lanthanide elements and Zr oxide particles is prepared as a raw material powder, wherein in the particle size distribution of the rare earth element oxide particles, or in the particle size distribution of secondary particles in the case where the rare earth element oxide particles are agglomerated to form the secondary particles, the particle diameter D2.5 value at which the cumulative particle amount from the minimum particle size side is 2.5% based on the total particle amount is in the range from 180 nm to 2000 nm, inclusive. The raw material powder is press molded into a predetermined shape, followed by sintering.
Method of manufacturing transparent sesquioxide sintered body, and transparent sesquioxide sintered body manufactured by the method
IKARI MASANORI (author) / NOJIMA YOSHIHIRO (author) / MAKIKAWA SHINJI (author) / IKESUE AKIO (author)
2015-07-28
Patent
Electronic Resource
English
IPC:
C04B
Kalk
,
LIME
/
C09K
Materialien für Anwendungen, soweit nicht anderweitig vorgesehen
,
MATERIALS FOR APPLICATIONS NOT OTHERWISE PROVIDED FOR
/
H01J
Elektrische Entladungsröhren oder Entladungslampen
,
ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS
/
H01S
Vorrichtungen, die stimulierte Emission verwenden
,
DEVICES USING STIMULATED EMISSION
European Patent Office | 2020
Ho ion doped sesquioxide transparent ceramic and preparation method thereof
European Patent Office | 2022
|European Patent Office | 2021
|European Patent Office | 2020
|European Patent Office | 2023
|