POWDER WATERPROOFING ADMIXTURE, METHOD FOR PREPARING SAME, AND CONSTRUCTION METHOD USING SAME
A powder waterproofing admixture of the present invention contains 100 parts by weight of zinc stearate, 10-20 parts by weight of silica fume, 10-15 parts by weight of active silica, 30-40 parts by weight of diatomite, 1-2 parts by weight of sodium lauryl sulfate, 1-2 parts by weight of sodium benzoate, 1-3 parts by weight of hydrogel particles and 1-2 parts by weight of a surfactant. Further, the powder waterproofing admixture of the present invention may further contain pyrobitumen particles, wherein the amount of added pyrobitumen particles is preferably 0.5-1 wt% for the entire powder waterproofing admixture.
La présente invention concerne un hydrofuge en poudre contenant 100 parties en poids de stéarate de zinc, 10 à 20 parties en poids de fumées de silice, 10 à 15 parties en poids de silice active, 30 à 40 parties en poids de diatomite, 1 à 2 parties en poids de laurylsulfate de sodium, 1 à 2 parties en poids de benzoate de sodium, 1 à 3 parties en poids de particules d'hydrogel et 1 à 2 parties en poids d'un tensioactif. En outre, l'hydrofuge en poudre de la présente invention peut en outre contenir des particule de pyrobitume, la quantité de particules de pyrobitume ajoutées étant de préférence 0,5 à 1 % en poids pour la totalité de l'hydrofuge en poudre.
본 발명의 분말 구체방수제는 스테아린산 아연 100중량부, 실리카 퓸 10 내지 20중량부, 활성실리카 10 내지 15중량부, 규조토 30 내지 40중량부, 나트륨 라우릴 황산염 1 내지 2중량부, 소듐 벤조에이트 1 내지 2중량부, 하이드로겔 입자 1 내지 3중량부 및 계면활성제 1 내지 2중량부를 포함한다. 또한 본 발명의 분말 구체방수제는 피로역청 입자를 더 포함할 수 있는데, 피로역청 입자의 첨가량은 전체 분말 구체방수제 전체의 0.5 내지 1중량%인 것이 바람직하다.
POWDER WATERPROOFING ADMIXTURE, METHOD FOR PREPARING SAME, AND CONSTRUCTION METHOD USING SAME
A powder waterproofing admixture of the present invention contains 100 parts by weight of zinc stearate, 10-20 parts by weight of silica fume, 10-15 parts by weight of active silica, 30-40 parts by weight of diatomite, 1-2 parts by weight of sodium lauryl sulfate, 1-2 parts by weight of sodium benzoate, 1-3 parts by weight of hydrogel particles and 1-2 parts by weight of a surfactant. Further, the powder waterproofing admixture of the present invention may further contain pyrobitumen particles, wherein the amount of added pyrobitumen particles is preferably 0.5-1 wt% for the entire powder waterproofing admixture.
La présente invention concerne un hydrofuge en poudre contenant 100 parties en poids de stéarate de zinc, 10 à 20 parties en poids de fumées de silice, 10 à 15 parties en poids de silice active, 30 à 40 parties en poids de diatomite, 1 à 2 parties en poids de laurylsulfate de sodium, 1 à 2 parties en poids de benzoate de sodium, 1 à 3 parties en poids de particules d'hydrogel et 1 à 2 parties en poids d'un tensioactif. En outre, l'hydrofuge en poudre de la présente invention peut en outre contenir des particule de pyrobitume, la quantité de particules de pyrobitume ajoutées étant de préférence 0,5 à 1 % en poids pour la totalité de l'hydrofuge en poudre.
본 발명의 분말 구체방수제는 스테아린산 아연 100중량부, 실리카 퓸 10 내지 20중량부, 활성실리카 10 내지 15중량부, 규조토 30 내지 40중량부, 나트륨 라우릴 황산염 1 내지 2중량부, 소듐 벤조에이트 1 내지 2중량부, 하이드로겔 입자 1 내지 3중량부 및 계면활성제 1 내지 2중량부를 포함한다. 또한 본 발명의 분말 구체방수제는 피로역청 입자를 더 포함할 수 있는데, 피로역청 입자의 첨가량은 전체 분말 구체방수제 전체의 0.5 내지 1중량%인 것이 바람직하다.
POWDER WATERPROOFING ADMIXTURE, METHOD FOR PREPARING SAME, AND CONSTRUCTION METHOD USING SAME
HYDROGUGE EN POUDRE, PROCÉDÉ DE PRÉPARATION ASSOCIÉ ET PROCÉDÉ DE CONSTRUCTION L'UTILISANT
분말 구체방수제, 이의 제조방법 및 이를 이용한 시공방법
IM MYUNG SOO (author) / KIM MEONG JI (author)
2016-10-20
Patent
Electronic Resource
Korean
IPC:
C04B
Kalk
,
LIME
European Patent Office | 2016
|European Patent Office | 2015
|European Patent Office | 2015
|European Patent Office | 2022
|