SELF-LEVELING MATERIAL COMPOSITION
Provided is a gypsum-based self-leveling material as mentioned below, which has a stably retained pot life, and of which the variation in the light walking possible time, which has occurred under low-temperature conditions such as climate variability, can be reduced to a lower level and the operational efficiency can be improved significantly compared with the conventional products and therefore the practicality can become excellent. A gypsum-based self-leveling material composition comprising a base material containing hemihydrate gypsum as an essential component and also containing inorganic aggregates and cement as optional components and an additive contained in the base material, wherein: when the total amount of the base material components is defined as 100 parts in terms of a mass-based content, the content of hemihydrate gypsum is 55 to 100 parts; hemihydrate gypsum comprises α-form hemihydrate gypsum and β-form hemihydrate gypsum; when the total amount of α-form hemihydrate gypsum and β-form hemihydrate gypsum is defined as 100 parts, the content of α-form hemihydrate gypsum is 70 to 95 parts and the content of β-form hemihydrate gypsum is 5 to 30 parts; when the total amount of the base material components is defined as 100 parts, the content of β-form hemihydrate gypsum is 20 parts by mass or less; and the change in length prescribed in JASS 15M-103 is 0.05% or less.
L'invention fournit un matériau autonivelant à base de gypse qui possède une durée de conservation en pot stable, qui maintient les variations de la durée permettant une foulée légère sous des conditions de basse température, telles que des variations de température, ou similaire, à un niveau réduit, et qui se révèle excellent d'un point de vue pratique, l'efficacité d'exploitation étant clairement améliorée en comparaison avec l'art antérieur. Plus précisément, l'invention concerne une composition de matériau autonivelant à base de gypse de changement de longueur conformément à JASS 15M-103 inférieur ou égal à 0,5%, qui comprend un additif dans un substrat ayant un semi-hydrate de gypse pour composant essentiel et un agrégat organique ainsi qu'un ciment en tant que composant facultatif, et dont la teneur en semi-hydrate de gypse est comprise entre 55 et 100 parties dans le cas où le total des composants du substrat équivaut à 100 parties en termes de masse. Le semi-hydrate de gypse inclut un semi-hydrate de gypse type α et un semi-hydrate de gypse type β. Dans le cas où le total de semi-hydrate de gypse type α et semi-hydrate de gypse type β équivaut à 100 parties, la teneur en semi-hydrate de gypse type α est comprise entre 70 et 95 parties, et la teneur en semi-hydrate de gypse type β est comprise entre 5 et 30 parties. Dans le cas où le total des composants du substrat équivaut à 100 parties, la teneur en semi-hydrate de gypse type β est inférieure ou égale à 20 parties en masse.
可使時間を安定に保ち、気温変動等の低温条件下で生じていた軽歩行可能時間の変動を小さく抑えた、従来製品に比して顕著な作業効率の向上効果を実現した実用性に優れた下記のせっこう系のセルフレベリング材を提供する。 半水石膏を必須成分とし、無機骨材とセメントを任意成分とする基材に、添加剤を含有し、基材成分の合計を質量基準で100部とした場合、半水石膏の含有量が55~100部で、半水石膏は、α型半水石膏とβ型半水石膏とを含み、且つ、α型半水石膏とβ型半水石膏の合計を100部とした場合、α型半水石膏の含有量が70~95部、β型半水石膏の含有量が5~30部であり、さらに、基材成分の合計を100部とした場合、β型半水石膏の含有量は20質量部以下である、JASS 15M-103で規定する長さ変化が0.05%以下のせっこう系セルフレベリング材組成物である。
SELF-LEVELING MATERIAL COMPOSITION
Provided is a gypsum-based self-leveling material as mentioned below, which has a stably retained pot life, and of which the variation in the light walking possible time, which has occurred under low-temperature conditions such as climate variability, can be reduced to a lower level and the operational efficiency can be improved significantly compared with the conventional products and therefore the practicality can become excellent. A gypsum-based self-leveling material composition comprising a base material containing hemihydrate gypsum as an essential component and also containing inorganic aggregates and cement as optional components and an additive contained in the base material, wherein: when the total amount of the base material components is defined as 100 parts in terms of a mass-based content, the content of hemihydrate gypsum is 55 to 100 parts; hemihydrate gypsum comprises α-form hemihydrate gypsum and β-form hemihydrate gypsum; when the total amount of α-form hemihydrate gypsum and β-form hemihydrate gypsum is defined as 100 parts, the content of α-form hemihydrate gypsum is 70 to 95 parts and the content of β-form hemihydrate gypsum is 5 to 30 parts; when the total amount of the base material components is defined as 100 parts, the content of β-form hemihydrate gypsum is 20 parts by mass or less; and the change in length prescribed in JASS 15M-103 is 0.05% or less.
L'invention fournit un matériau autonivelant à base de gypse qui possède une durée de conservation en pot stable, qui maintient les variations de la durée permettant une foulée légère sous des conditions de basse température, telles que des variations de température, ou similaire, à un niveau réduit, et qui se révèle excellent d'un point de vue pratique, l'efficacité d'exploitation étant clairement améliorée en comparaison avec l'art antérieur. Plus précisément, l'invention concerne une composition de matériau autonivelant à base de gypse de changement de longueur conformément à JASS 15M-103 inférieur ou égal à 0,5%, qui comprend un additif dans un substrat ayant un semi-hydrate de gypse pour composant essentiel et un agrégat organique ainsi qu'un ciment en tant que composant facultatif, et dont la teneur en semi-hydrate de gypse est comprise entre 55 et 100 parties dans le cas où le total des composants du substrat équivaut à 100 parties en termes de masse. Le semi-hydrate de gypse inclut un semi-hydrate de gypse type α et un semi-hydrate de gypse type β. Dans le cas où le total de semi-hydrate de gypse type α et semi-hydrate de gypse type β équivaut à 100 parties, la teneur en semi-hydrate de gypse type α est comprise entre 70 et 95 parties, et la teneur en semi-hydrate de gypse type β est comprise entre 5 et 30 parties. Dans le cas où le total des composants du substrat équivaut à 100 parties, la teneur en semi-hydrate de gypse type β est inférieure ou égale à 20 parties en masse.
可使時間を安定に保ち、気温変動等の低温条件下で生じていた軽歩行可能時間の変動を小さく抑えた、従来製品に比して顕著な作業効率の向上効果を実現した実用性に優れた下記のせっこう系のセルフレベリング材を提供する。 半水石膏を必須成分とし、無機骨材とセメントを任意成分とする基材に、添加剤を含有し、基材成分の合計を質量基準で100部とした場合、半水石膏の含有量が55~100部で、半水石膏は、α型半水石膏とβ型半水石膏とを含み、且つ、α型半水石膏とβ型半水石膏の合計を100部とした場合、α型半水石膏の含有量が70~95部、β型半水石膏の含有量が5~30部であり、さらに、基材成分の合計を100部とした場合、β型半水石膏の含有量は20質量部以下である、JASS 15M-103で規定する長さ変化が0.05%以下のせっこう系セルフレベリング材組成物である。
SELF-LEVELING MATERIAL COMPOSITION
COMPOSITION DE MATÉRIAU AUTONIVELANT
セルフレベリング材組成物
WADA MASAHIRO (author) / KUBO HIROYUKI (author)
2021-04-22
Patent
Electronic Resource
Japanese
IPC:
C04B
Kalk
,
LIME