A platform for research: civil engineering, architecture and urbanism
This asphalt mix regeneration method comprises: an analysis step of analyzing an effective asphalt component content ratio in an asphalt mix waste material; a determination step of determining, on the basis of the effective asphalt content ratio obtained in the analysis step, the quantity of additive needed for regenerating the waste material; an introduction step of introducing into a container the waste material, and the additive in the quantity determined by the determination step; and a stir-heating step of decreasing to pebble-scale the sizes of the waste material and the additive that have been introduced into the container, while holding the internal temperature of the container in a temperature region of 170°C to 200°C through heating, and mixing together the waste material and the additive to produce a regenerated asphalt material.
Ce procédé de régénération de mélange d'asphalte comprend : une étape d'analyse consistant à analyser un rapport de teneur en composant d'asphalte efficace dans des déchets de mélange d'asphalte ; une étape de détermination consistant à déterminer, sur la base du rapport de teneur en asphalte efficace obtenu dans l'étape d'analyse, la quantité d'additif nécessaire pour régénérer les déchets ; une étape d'introduction consistant à introduire dans un conteneur les déchets, et l'additif dans la quantité déterminée par l'étape de détermination ; et une étape de chauffage par agitation consistant à réduire à l'échelle de boulets les tailles des déchets et de l'additif qui ont été introduits dans le conteneur tout en maintenant la température interne du conteneur dans une plage de températures de 170 °C à 200 °C par chauffage, et de mélange des déchets et de l'additif pour produire un matériau d'asphalte régénéré.
このアスファルト混合物の再生方法は、アスファルト混合物の廃材における有効アスファルト成分の含有率を分析する分析工程と、前記分析工程で得られた有効アスファルト含有率に基づいて前記廃材の再生に必要な添加剤の分量を決定する決定工程と、前記廃材と、前記決定工程で決定した分量の前記添加剤とを容器内に投入する投入工程と、前記容器内に投入された前記廃材及び前記添加剤を小石大に小径化すると共に、加熱により前記容器内の温度を170℃~200℃の温度域に保持し、前記廃材と前記添加剤とを混ぜ合わせて再生アスファルト材を作製する攪拌加熱工程とを有する。
This asphalt mix regeneration method comprises: an analysis step of analyzing an effective asphalt component content ratio in an asphalt mix waste material; a determination step of determining, on the basis of the effective asphalt content ratio obtained in the analysis step, the quantity of additive needed for regenerating the waste material; an introduction step of introducing into a container the waste material, and the additive in the quantity determined by the determination step; and a stir-heating step of decreasing to pebble-scale the sizes of the waste material and the additive that have been introduced into the container, while holding the internal temperature of the container in a temperature region of 170°C to 200°C through heating, and mixing together the waste material and the additive to produce a regenerated asphalt material.
Ce procédé de régénération de mélange d'asphalte comprend : une étape d'analyse consistant à analyser un rapport de teneur en composant d'asphalte efficace dans des déchets de mélange d'asphalte ; une étape de détermination consistant à déterminer, sur la base du rapport de teneur en asphalte efficace obtenu dans l'étape d'analyse, la quantité d'additif nécessaire pour régénérer les déchets ; une étape d'introduction consistant à introduire dans un conteneur les déchets, et l'additif dans la quantité déterminée par l'étape de détermination ; et une étape de chauffage par agitation consistant à réduire à l'échelle de boulets les tailles des déchets et de l'additif qui ont été introduits dans le conteneur tout en maintenant la température interne du conteneur dans une plage de températures de 170 °C à 200 °C par chauffage, et de mélange des déchets et de l'additif pour produire un matériau d'asphalte régénéré.
このアスファルト混合物の再生方法は、アスファルト混合物の廃材における有効アスファルト成分の含有率を分析する分析工程と、前記分析工程で得られた有効アスファルト含有率に基づいて前記廃材の再生に必要な添加剤の分量を決定する決定工程と、前記廃材と、前記決定工程で決定した分量の前記添加剤とを容器内に投入する投入工程と、前記容器内に投入された前記廃材及び前記添加剤を小石大に小径化すると共に、加熱により前記容器内の温度を170℃~200℃の温度域に保持し、前記廃材と前記添加剤とを混ぜ合わせて再生アスファルト材を作製する攪拌加熱工程とを有する。
ASPHALT MIX REGENERATION METHOD
PROCÉDÉ DE RÉGÉNÉRATION DE MÉLANGE D'ASPHALTE
アスファルト混合物の再生方法
SHINNAGA RYUICHI (author)
2021-10-07
Patent
Electronic Resource
Japanese
IPC:
E01C
Bau von Straßen, Sportplätzen oder dgl., Decken dafür
,
CONSTRUCTION OF, OR SURFACES FOR, ROADS, SPORTS GROUNDS, OR THE LIKE
Asphalt regeneration device and regeneration method thereof
European Patent Office | 2022
|