BLEND DESIGN METHOD FOR ASPHALT MIXTURE, METHOD FOR MANUFACTURING ASPHALT MIXTURE, AND ASPHALT MIXTURE
Provided is technology that makes it possible for an asphalt mixture to exhibit a suitable void ratio and saturation, even in a case where synthetic calcium carbonate is used. A blend design method for an asphalt mixture of the present disclosure comprises a determination step in which a ratio r1 (mass%) of a first filler and a ratio r2 (mass%) of a second filler are determined so that a converted specific surface area B0 (m2/g) is 5.00 (m2/g) or less, B0 being calculated on the basis of: a BET specific surface area B1 (m2/g) of the first filler that includes a synthetic calcium carbonate powder; a BET specific surface area B2 (m2/g) of the second filler that includes a calcium carbonate powder produced in a process that is at least different from that of the synthetic calcium carbonate powder; the ratio r1 (mass%) of the mass of the first filler to the sum of the mass of the first filler and the mass of the second filler; and the ratio r2 (mass%) of the mass of the second filler to the sum of the mass of the first filler and the mass of the second filler.
La présente invention concerne une technologie qui permet à un mélange d'asphalte de présenter un taux de vide et une saturation appropriés, même dans un cas où du carbonate de calcium synthétique est utilisé. Un procédé de conception de combinaison pour un mélange d'asphalte de la présente divulgation comprend une étape de détermination dans laquelle un rapport r1 (% de masse) d'une première charge et un rapport r2 (% de masse) d'une seconde charge sont déterminés de telle sorte qu'une surface spécifique convertie B0 (m2/g) soit inférieure ou égale à 5,00 (m2/g), B0 étant calculé sur la base : d'une surface spécifique BET B1 (m2/g) de la première charge qui comprend une poudre de carbonate de calcium synthétique ; d'une surface spécifique BET B2 (m2/g) de la seconde charge qui comprend une poudre de carbonate de calcium produite avec un procédé au moins différent de celui de la poudre de carbonate de calcium synthétique ; du rapport r1 (% de masse) de la masse de la première charge à la somme de la masse de la première charge et de la masse de la seconde charge ; et du rapport r2 (% de masse) de la masse de la seconde charge à la somme de la masse de la première charge et de la masse de la seconde charge.
合成炭酸カルシウムを用いた場合であっても、アスファルト混合物が適切な空隙率と飽和度を発現することを可能とする技術を提供する。 本開示のアスファルト混合物の配合設計方法は、合成炭酸カルシウム粉末を含む第1フィラーのBET比表面積B1(m2/g)とし、少なくとも上記合成炭酸カルシウム粉末とは生成過程の異なる炭酸カルシウム粉末を含む第2フィラーのBET比表面積B2(m2/g)とし、上記第1フィラーの質量と上記第2フィラーの質量との和に対する上記第1フィラーの質量の比率r1(質量%)とし、上記第1フィラーの質量と上記第2フィラーの質量との和に対する上記第2フィラーの質量の比率r2(質量%)とに基づいて算出される換算比表面積B0(m2/g)が5.00(m2/g)以下となるように、アスファルト組成物に混合する上記第1フィラーの比率r1(質量%)と、上記第2フィラーの比率r2(質量%)と、を決定する決定工程を備える。
BLEND DESIGN METHOD FOR ASPHALT MIXTURE, METHOD FOR MANUFACTURING ASPHALT MIXTURE, AND ASPHALT MIXTURE
Provided is technology that makes it possible for an asphalt mixture to exhibit a suitable void ratio and saturation, even in a case where synthetic calcium carbonate is used. A blend design method for an asphalt mixture of the present disclosure comprises a determination step in which a ratio r1 (mass%) of a first filler and a ratio r2 (mass%) of a second filler are determined so that a converted specific surface area B0 (m2/g) is 5.00 (m2/g) or less, B0 being calculated on the basis of: a BET specific surface area B1 (m2/g) of the first filler that includes a synthetic calcium carbonate powder; a BET specific surface area B2 (m2/g) of the second filler that includes a calcium carbonate powder produced in a process that is at least different from that of the synthetic calcium carbonate powder; the ratio r1 (mass%) of the mass of the first filler to the sum of the mass of the first filler and the mass of the second filler; and the ratio r2 (mass%) of the mass of the second filler to the sum of the mass of the first filler and the mass of the second filler.
La présente invention concerne une technologie qui permet à un mélange d'asphalte de présenter un taux de vide et une saturation appropriés, même dans un cas où du carbonate de calcium synthétique est utilisé. Un procédé de conception de combinaison pour un mélange d'asphalte de la présente divulgation comprend une étape de détermination dans laquelle un rapport r1 (% de masse) d'une première charge et un rapport r2 (% de masse) d'une seconde charge sont déterminés de telle sorte qu'une surface spécifique convertie B0 (m2/g) soit inférieure ou égale à 5,00 (m2/g), B0 étant calculé sur la base : d'une surface spécifique BET B1 (m2/g) de la première charge qui comprend une poudre de carbonate de calcium synthétique ; d'une surface spécifique BET B2 (m2/g) de la seconde charge qui comprend une poudre de carbonate de calcium produite avec un procédé au moins différent de celui de la poudre de carbonate de calcium synthétique ; du rapport r1 (% de masse) de la masse de la première charge à la somme de la masse de la première charge et de la masse de la seconde charge ; et du rapport r2 (% de masse) de la masse de la seconde charge à la somme de la masse de la première charge et de la masse de la seconde charge.
合成炭酸カルシウムを用いた場合であっても、アスファルト混合物が適切な空隙率と飽和度を発現することを可能とする技術を提供する。 本開示のアスファルト混合物の配合設計方法は、合成炭酸カルシウム粉末を含む第1フィラーのBET比表面積B1(m2/g)とし、少なくとも上記合成炭酸カルシウム粉末とは生成過程の異なる炭酸カルシウム粉末を含む第2フィラーのBET比表面積B2(m2/g)とし、上記第1フィラーの質量と上記第2フィラーの質量との和に対する上記第1フィラーの質量の比率r1(質量%)とし、上記第1フィラーの質量と上記第2フィラーの質量との和に対する上記第2フィラーの質量の比率r2(質量%)とに基づいて算出される換算比表面積B0(m2/g)が5.00(m2/g)以下となるように、アスファルト組成物に混合する上記第1フィラーの比率r1(質量%)と、上記第2フィラーの比率r2(質量%)と、を決定する決定工程を備える。
BLEND DESIGN METHOD FOR ASPHALT MIXTURE, METHOD FOR MANUFACTURING ASPHALT MIXTURE, AND ASPHALT MIXTURE
PROCÉDÉ DE CONCEPTION DE COMBINAISON POUR MÉLANGE D'ASPHALTE, PROCÉDÉ DE FABRICATION D'UN MÉLANGE D'ASPHALTE ET MÉLANGE D'ASPHALTE
アスファルト混合物の配合設計方法、アスファルト混合物の製造方法及びアスファルト混合物
WU YUEQIAO (author) / SEO AKIRA (author) / NOGUCHI KENTARO (author)
2022-04-07
Patent
Electronic Resource
Japanese
IPC:
C08L
COMPOSITIONS OF MACROMOLECULAR COMPOUNDS
,
Massen auf Basis makromolekularer Verbindungen
/
C04B
Kalk
,
LIME
/
C08K
Verwendung von anorganischen oder nichtmakromolekularen organischen Stoffen als Zusatzstoffe
,
USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES AS COMPOUNDING INGREDIENTS
COMPOSITION FOR MANUFACTURING ASPHALT MIXTURE, ASPHALT MIXTURE, AND ASPHALT PAVING METHOD
European Patent Office | 2015
|European Patent Office | 2019
|RECYCLED ASPHALT MIXTURE MANUFACTURING METHOD AND RECYCLED ASPHALT MIXTURE
European Patent Office | 2020
|European Patent Office | 2020
|ASPHALT MIXTURE, ASPHALT MIXTURE PRODUCTION SYSTEM AND METHOD
European Patent Office | 2024
|