SOLDER FOR CONNECTION AND PREPARATION METHOD THEREFOR AND METHOD FOR CONNECTING SILICON CARBIDE CLADDING
Disclosed are a solder for connection and a preparation method therefor and a method for connecting a silicon carbide cladding. The solder for connection comprises the following raw materials: a precursor, a glass powder and an organic solvent, wherein the mass ratio of the precursor to the glass powder is 90-98: 2-10. The solder for connection of the present invention is used for connecting a silicon carbide cladding. A glass additive phase formed by the glass powder has good wettability to silicon carbide and a high connection strength. The proportion of the glass powder is adjustable, so that the coefficient of thermal expansion of the glass additive phase is adjustable, and the stress of a joint after connection is controllable. A thick compact connection layer can be realized, facilitating engineering assembly and realizing better air tightness.
L'invention concerne une soudure pour raccordement et un procédé de préparation associé, ainsi qu'un procédé de raccordement d'une gaine en carbure de silicium. La soudure pour raccordement comprend les matières premières suivantes : un précurseur, une poudre de verre et un solvant organique, le rapport en masse du précurseur sur la poudre de verre étant de 90-98/2-10. La soudure pour raccordement de la présente invention est utilisée pour raccorder une gaine en carbure de silicium. Une phase d'additif de verre formée par la poudre de verre a une bonne mouillabilité vis-à-vis du carbure de silicium et une résistance de raccordement élevée. La proportion de la poudre de verre est ajustable, de telle sorte que le coefficient de dilatation thermique de la phase d'additif de verre est ajustable, et la contrainte d'un joint après le raccordement est régulable. Une couche de raccordement compacte épaisse peut être réalisée, facilitant l'assemblage d'ingénierie et réalisant une meilleure étanchéité à l'air.
本发明公开了一种连接钎料及其制备方法、碳化硅包壳连接方法,连接钎料包括原料如下:前驱体、玻璃粉体以及有机溶剂;所述前驱体和玻璃粉体的质量比为90~98:2~10。本发明的连接钎料,用于碳化硅包壳连接,其中的玻璃粉体形成的玻璃添加相与碳化硅的润湿性好,连接强度高;玻璃粉体比例可调,使得玻璃添加相的热膨胀系数可调,连接后接头的应力可控;能够实现较厚的致密连接层,有利于工程装配且气密性较好。
SOLDER FOR CONNECTION AND PREPARATION METHOD THEREFOR AND METHOD FOR CONNECTING SILICON CARBIDE CLADDING
Disclosed are a solder for connection and a preparation method therefor and a method for connecting a silicon carbide cladding. The solder for connection comprises the following raw materials: a precursor, a glass powder and an organic solvent, wherein the mass ratio of the precursor to the glass powder is 90-98: 2-10. The solder for connection of the present invention is used for connecting a silicon carbide cladding. A glass additive phase formed by the glass powder has good wettability to silicon carbide and a high connection strength. The proportion of the glass powder is adjustable, so that the coefficient of thermal expansion of the glass additive phase is adjustable, and the stress of a joint after connection is controllable. A thick compact connection layer can be realized, facilitating engineering assembly and realizing better air tightness.
L'invention concerne une soudure pour raccordement et un procédé de préparation associé, ainsi qu'un procédé de raccordement d'une gaine en carbure de silicium. La soudure pour raccordement comprend les matières premières suivantes : un précurseur, une poudre de verre et un solvant organique, le rapport en masse du précurseur sur la poudre de verre étant de 90-98/2-10. La soudure pour raccordement de la présente invention est utilisée pour raccorder une gaine en carbure de silicium. Une phase d'additif de verre formée par la poudre de verre a une bonne mouillabilité vis-à-vis du carbure de silicium et une résistance de raccordement élevée. La proportion de la poudre de verre est ajustable, de telle sorte que le coefficient de dilatation thermique de la phase d'additif de verre est ajustable, et la contrainte d'un joint après le raccordement est régulable. Une couche de raccordement compacte épaisse peut être réalisée, facilitant l'assemblage d'ingénierie et réalisant une meilleure étanchéité à l'air.
本发明公开了一种连接钎料及其制备方法、碳化硅包壳连接方法,连接钎料包括原料如下:前驱体、玻璃粉体以及有机溶剂;所述前驱体和玻璃粉体的质量比为90~98:2~10。本发明的连接钎料,用于碳化硅包壳连接,其中的玻璃粉体形成的玻璃添加相与碳化硅的润湿性好,连接强度高;玻璃粉体比例可调,使得玻璃添加相的热膨胀系数可调,连接后接头的应力可控;能够实现较厚的致密连接层,有利于工程装配且气密性较好。
SOLDER FOR CONNECTION AND PREPARATION METHOD THEREFOR AND METHOD FOR CONNECTING SILICON CARBIDE CLADDING
SOUDURE POUR RACCORDEMENT ET PROCÉDÉ DE PRÉPARATION ASSOCIÉ ET PROCÉDÉ DE RACCORDEMENT D'UNE GAINE EN CARBURE DE SILICIUM
连接钎料及其制备方法、碳化硅包壳连接方法
XUE JIAXIANG (author) / LIAO YEHONG (author) / REN QISEN (author) / LIU TONG (author) / ZHAI JIANHAN (author) / MA HAIBIN (author) / ZHANG XIANSHENG (author) / ZHANG YONGDONG (author) / LI RUI (author) / LIU YANG (author)
2022-05-19
Patent
Electronic Resource
Chinese
European Patent Office | 2024
|Silicon carbide cladding induction heating connection method and silicon carbide cladding
European Patent Office | 2021
|Silicon carbide ceramic connection method and silicon carbide cladding
European Patent Office | 2021
|European Patent Office | 2023
|European Patent Office | 2022
|